Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 11 g/10 min | 11 g/10 min | (Condition L) ASTM D-1238-94a |
Multibase Multi-Pro® 1010 T Black 10% Talc Content Polypropylene PPH talc filled compound suitable for containers and wash-tubs requiring elevated stiffness and improved cycle times.Data provided by Multibase. |
|||
Melt Flow | 11 g/10 min @Load 2.16 kg, Temperature 230 °C |
11 g/10 min @Load 4.76 lb, Temperature 446 °F |
Procedure A; ASTM D1238 |
PolyOne Maxxam™ PPH-40T Nat Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Melt Flow | 11 g/10 min @Load 5.00 kg, Temperature 260 °C |
11 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® CY100FC PC+ABS (Asia Pacific) High impact PC+ABS material designed for local Pacific Automotive applications |
|||
Melt Flow | 11 g/10 min @Load 5.00 kg, Temperature 200 °C |
11 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
PolyOne Dynaflex™ G7960-1 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7960-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Melt Flow | 11 g/10 min | 11 g/10 min | I<sub>21</sub>; ASTM D238 |
Petromont 5001 High Density Polyethylene Resin Petromont HDPE 5001 is a high-density polyethylene copolymer resin produced using the UNIPOL®
Process. This resin is intended for use in prime sheet and thermoforming applications such as arena boa.. |
|||
Melt Flow | 11 g/10 min @Load 1.20 kg, Temperature 250 °C |
11 g/10 min @Load 2.65 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® OQ1022 PC Standard Flow OQ Resin |
|||
Melt Flow | 11 g/10 min | 11 g/10 min | ASTM D1238 |
LyondellBasell Microthene® G MU76300 Ethylene Vinyl Acetate Copolymer General DescriptionMicrothene G polyolefin powders are ground, irregularly-shaped particles designed for use in a broad range of specialty applications. Microthene G powders combine the unique prop.. |
|||
Melt Flow | 11 g/10 min | 11 g/10 min | ASTM D1238 |
Hyosung Topilene J700 PP J700 Injection General HomopolymerApplications: General injectionCharacteristics:ProcessabilityStiffnessInformation provided by Hyosung Corporation |
|||
Melt Flow | 11 g/10 min @Load 5.00 kg, Temperature 200 °C |
11 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
LG Chemical HIPS 403AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Electric Parts Requiring Flame RetardancyCAS: 9003-55-8, 21850-44-2 and 1309-64-4Information provided by LG Chemical |
|||
Melt Flow | 11 g/10 min @Load 2.16 kg, Temperature 230 °C |
11 g/10 min @Load 4.76 lb, Temperature 446 °F |
L; ASTM D1238 |
Global PP-1100-NK Polypropylene Homopolymer Description-transparency, high stiffness, high heat resistantApplications-general purpose, household goods, closures, food applicationsInformation provided by Global Polymers Corporation. |
|||
Melt Flow | 11 g/10 min @Load 2.16 kg, Temperature 230 °C |
11 g/10 min @Load 4.76 lb, Temperature 446 °F |
L; ASTM D1238 |
Global PP-1126-NK Polypropylene Homopolymer Description-transparency, high stiffness, high heat resistantApplications- food applicationsInformation provided by Global Polymers Corporation. |
|||
Melt Flow | 11 g/10 min | 11 g/10 min | Condition G |
Ineos Nova 3100 General Purpose Crystal Polystyrene Good balance of flow and set-up properties, Good crack resistanceApplications: Single service cutlery, Single service drinkware, Consumer electronic packagingExposure to gamma radiation in the 2.02-.. |
|||
Melt Flow | 11 g/10 min @Load 2.16 kg, Temperature 230 °C |
11 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
IRPC Polimaxx Polene N700P Polypropylene Homopolymer APPLICATION: BASE COMPONENT FOR COLORING RESIN |
|||
Melt Flow | 11 g/10 min @Load 10.0 kg, Temperature 250 °C |
11 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL WCD795 PPE-TPE (Asia Pacific) Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as cable jacket of UL 62 SVE and NISPE confiations. Flame retardant performance capable of m.. |
|||
Melt Flow | 11 g/10 min @Load 6.60 kg, Temperature 337 °C |
11 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM CRS5011 PEI (Asia Pacific) Transparent, Enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 listing. |
|||
Melt Flow | 11 g/10 min @Load 5.00 kg, Temperature 250 °C |
11 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics Xenoy® HX5600HP PBT+PC (Europe-Africa-Middle East) Xenoy HX5600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Melt Flow | 11 g/10 min @Load 5.00 kg, Temperature 250 °C |
11 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics Xenoy® HX6600HP PBT+PC (Europe-Africa-Middle East) Xenoy HX6600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Melt Flow | 11 g/10 min @Load 10.0 kg, Temperature 250 °C |
11 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® HN-3203G PC, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 11 g/10 min @Load 10.0 kg, Temperature 220 °C |
11 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® SD-0150UF ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 11 g/10 min @Load 1.20 kg, Temperature 300 °C |
11 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Styron EMERGEâ„¢ 4410-11 MFR Polycarbonate EMERGEâ„¢ PC 4410-11 advanced resin is a high impact polycarbonate resin designed for Information Technology Equipment and Injection Molding Applications.Information provided by DowThis product l.. |
|||
Melt Flow | 11 g/10 min @Load 2.16 kg, Temperature 230 °C |
11 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238; ISO 1133 |
Styron INSPIREâ„¢ TF1302 Thermoplastic Polyolefin Information provided by DowThe Inspire brand was spun off from Dow Chemical to Styron in 2010 |
|||
Melt Flow | 11 g/10 min @Load 6.60 kg, Temperature 337 °C |
11 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM AUT210 PEI (Asia Pacific) Transparent Polyetherimide (Tg 227 degC). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature o.. |
|||
Melt Flow | 11 g/10 min @Load 1.20 kg, Temperature 300 °C |
11 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM Data |
Styron CALIBRE™ IM 401 11 Polycarbonate, Impact Modified CALIBRE® IM401 series resins are impact modified, UL listed polycarbonate resins which contain mold release. CALIBRE IM401 polycarbonate resins exhibit an excellent balance of impact strength and.. |
|||
Melt Flow | 11 g/10 min @Load 2.16 kg, Temperature 190 °C |
11 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Unipetrol PE HD LITEN® MB/ML 73 HDPE Made for injection molding applications.Information provided by Unipetrol RPA |
|||
Melt Flow | 11 g/10 min | 11 g/10 min | ASTM D1238 |
Washington Penn Polypropylene Copolymer 20% Glass Reinforced, 11 MFI Fiberglass & mineral-reinforced polypropylene compounds provide excellent tensile and impact properties. Mold shrinkage is similar to ABS and polystyrene. Compounds also have dimensional stability. .. |
|||
Melt Flow | 11 g/10 min @Load 2.16 kg, Temperature 230 °C |
11 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Total PPH 7059 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 7059 is homopolymer.ApplicationATOFINA Polypropylene PPH 7059 is intended for extrusion of staple fibers for non-woven applications. It exhibits excellent spinning propert.. |
|||
Melt Flow | 11 g/10 min | 11 g/10 min | Condition 190/21.6, HLMI; ASTM D1238 |
Chevron Phillips Marlex® 9398 HDPE Pipe and Corrugated Extrusion Resin Resin Type: Hexene CopolymerCharacteristics: Good melt strengthExcellent ESCRApplications: ConduitDuctInformation provided by Chevron Phillips. |
|||
Melt Flow | 11 g/10 min | 11 g/10 min | ASTM D1238 |
Aclo Accutech Polypropylene Copolymer CP0436M20L Mica Reinforced |
|||
Melt Flow | 11 g/10 min @Load 2.16 kg, Temperature 190 °C |
11 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Ineos J50-1000-181 HDPE A high density polyethylene copolymer. It has a narrow molecular weight distribution and is intended for the injection molding of screw caps dedicated to the packaging of still water. This resin c.. |
|||
Melt Flow | 11 g/10 min @Load 1.20 kg, Temperature 300 °C |
11 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Covestro Makrolon® LQ-2847 Polycarbonate, Lens Quality Optical, Mold Release, UV Stabilized
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |