Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.25 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.25 g/10 min @Load 4.76 lb, Temperature 374 °F |
Procedure A Condition E; ASTM D1238 |
Network Polymers NPP 50-0252 Description: High Density Polyethylene (HDPE) Blow Molding GradeInformation provided by Network Polymers Inc. |
|||
Melt Flow | 0.25 g/10 min | 0.25 g/10 min | ASTM D1238 |
ExxonMobil LD 051.LJ Molding, Extrusion and Compounding Resin
(discontinued **) LD 051.LJ resin is used in Blow molded, squeeze bottles, Pail lids, Closures, and Extruded profiles.Information provided by ExxonMobil Chemical |
|||
Melt Flow | 0.25 g/10 min | 0.25 g/10 min | ExxonMobil Method |
ExxonMobil LD 051.LT Shrink Film Resin
(discontinued **) LD 051 blown film resins are designed for demanding heavy duty film applications, and combine excellent strength properties with outstanding processability. Used in heavy duty shipping bags and shr.. |
|||
Melt Flow | 0.25 g/10 min | 0.25 g/10 min | ExxonMobil Method |
ExxonMobil LD 641.LN Molding, Extrusion and Compounding Resin
(discontinued **) LD 641.LN is a low density homopolymer specifically designed for high performance blow molding applications. This resin is suitable for applications requiring high melt strength, flexibility, good .. |
|||
Melt Flow | 0.25 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.25 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D 1238 |
Chevron Phillips HiD® 9638 HDPE Sheeting and Blown Film Resin
(discontinued **) Resin Type: Sheeting Resin for the Geomembrane Market; ASTM D 4976 Classification: PE 225, A 56507Applications:Cast Geomembrane Applications, Notion and Millinery Bags, Heavy Duty Shipping Sacks, In.. |
|||
Melt Flow | 0.25 g/10 min | 0.25 g/10 min | Condition 190/2.16; ASTM D1238 |
Chevron Phillips Marlex® HHM 5502-01 Polyethylene, Sheet/Thermoforming Grade, HDPE
(discontinued **) Meets FDA Regulation 177.1520.Data provided by the manufacturer |
|||
Melt Flow | 0.25 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.25 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Braskem PB 526 LDPE Blow Molding Polyethylene
(discontinued **) Applications: Heavy duty bags; tubes and hoses; shrink films for pallets; tarpaulins. Blown Film. Information provided by Braskem |
|||
Melt Flow | 0.25 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.25 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
LG Chemical LUTENE-H BE0350 HDPE Description: LUTENE-H BE0350 is an excellent material for blow-molded articles with high density and rigidity. It has good flow characteristics, high parison stability and impact resistance.Applicat.. |
|||
Melt Flow | 0.25 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.25 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
LG Chemical LUTENE-H BE0400 HDPE Description: LUTENE - H BE0400 is an excellent materials for blow-molded articles with high density and rigidity. It has good flow characteristics and impact resistance.Applications: Blow molded con.. |
|||
Melt Flow | 0.25 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.25 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
LG Chemical LUTENE-H PE0235 HDPE Description: LUTENE-H PE0235 is a materials with high toughness and rigidity suitable for cable protection It has very high resistance to stress cracking and long-term internal pressure creep proper.. |
|||
Melt Flow | 0.25 g/10 min | 0.25 g/10 min | ASTM D1238 |
LyondellBasell Petrothene® NA480145 Low Density Polyethylene ApplicationsPETROTHENE NA 480 is a series of low density/EVA copolymer resins designed for specialty films. NA 480 produces film with superior puncture resistance, Heat sealability, clarity and low.. |
|||
Melt Flow | 0.25 g/10 min | 0.25 g/10 min | ASTM D1238 |
LyondellBasell Petrothene® NA480178 Low Density Polyethylene ApplicationsPETROTHENE NA 480 is a series of low density/EVA copolymer resins designed for specialty films. NA 480 produces film with superior puncture resistance, Heat sealability, clarity and low.. |
|||
Melt Flow | 0.25 g/10 min | 0.25 g/10 min | ASTM D1238 |
LyondellBasell Petrothene® NA940000 Low Density Polyethylene (Blow Molding) ApplicationsPETROTHENE NA 940-000 is a low density homopolymer resin intended for use in blow molding applications. Excellent toughness, good clarity and processability make NA 940-000 an ideal cho.. |
|||
Melt Flow | 0.25 g/10 min | 0.25 g/10 min | ASTM D1238 |
LyondellBasell Petrothene® NA940085 Low Density Polyethylene (Film Grade) ApplicationsPETROTHENE NA 940 is a series of resins designed for heavy duty film applications. Superior puncture resistance combined with excellent impact properties make NA 940 an ideal choice for.. |
|||
Melt Flow | 0.25 g/10 min | 0.25 g/10 min | ASTM D1238 |
LyondellBasell Petrothene® NA940094 Low Density Polyethylene (Film Grade) ApplicationsPETROTHENE NA 940 is a series of resins designed for heavy duty film applications. Superior puncture resistance combined with excellent impact properties make NA 940 an ideal choice for.. |
|||
Melt Flow | 0.25 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.25 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Lucobit Lucofin® 1400HN Powder Ethylene Butyl Acrylate Lucofin 1400HN Powder is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin 1400HN Powder is softer and more flexible than ethy.. |
|||
Melt Flow | 0.25 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.25 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
SCG Chemicals EL-Leneâ„¢ H1000PC High Density Polyethylene Pipe Resin Key Characteristics: Good processing, high thermal stability, low sagging, good balance of MRS, SCG, and RCPRecommended Applications: Water pressure and gas pipesCertification: Certified by EXOVA.. |
|||
Melt Flow | 0.25 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.25 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Borealis BorSafe™ HE3494-LS-H HDPE Compound for Pressure Pipes BorSafe™ HE3494-LS-H is a bimodal polyethylene compound produced by the advanced Borstar® technology. It includes a combination of pigments and stabilizers to ensure excellent long-term thermal s.. |
|||
Melt Flow | 0.25 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.25 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Borealis Casico™ FR6082 Reduced Fire Hazard Jacketing Compound Casico™ FR6082 is a thermoplastic, reduced fire hazard, zero halogen black jacketing compound combined with high mechanical strength, toughness and excellent extrusion properties. It is based on th.. |
|||
Melt Flow | 0.25 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.25 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Borealis FT3200 Low Density Polyethylene FT3200 is a Low Density Polyethylene for Film Extrusion. Applications heavy-duty bags, shrink film, construction films, and agricultural films. FT3200 contains no additives.Information provided by.. |
|||
Melt Flow | 0.25 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.25 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis RA130E-1498 Polypropylene Random Copolymer RA130E-1498 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is white colored. Applications: RA130E-1498 is recommended for the production of PP-R p.. |
|||
Melt Flow | 0.25 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.25 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
Formosa Plastics Formolene® HB5502S1 Sheet and Thermoforming HDPE High Density Polyethylene Hexene CopolymerApplications: Molded or formed industrial housings and parts, tanks, shrouds.Formolene HB5502S1 HDPE resin is designed for applications requiring excellent .. |
|||
Melt Flow | 0.25 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.25 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Borealis BorSafe™ HE3490-LS-H HDPE Compound for Pressure Pipes BorSafe™ HE3490-LS-H is a bimodal polyethylene compound produced by the advanced Borstar® technology. It includes a combination of pigments and stabilizers to ensure excellent long-term thermal s.. |
|||
Melt Flow | 0.25 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.25 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis RA130E-8427 Polypropylene Random Copolymer RA130E-8427 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is grey colored. Applications: domestic water, heating, relining, plumbing, and industr.. |
|||
Melt Flow | 0.25 g/10 min | 0.25 g/10 min | ExxonMobil Method |
ExxonMobil LD 317.09 Film Resin LD 317 Series offer excellent impact strength, tensile properties, and heat sealability. Applications include ice bags, frozen food packaging, and other food packaging.Information provided by Exxon.. |
|||
Melt Flow | 0.25 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.25 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LDPE LD 051.LQ Low Density Polyethylene Resin Product Description: LD 051.LQ blown film resin is a fractional melt index grade designed for demanding heavy duty film applications, and combines excellent strength properties with outstanding proc.. |
|||
Melt Flow | 0.25 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.25 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Paxon™ AA53-003 Pipe Extrusion Resin Product Description: AA53-003 is a pipe extrusion grade high density polyethylene copolymer offering an excellent combination of stiffness and stress crack resistance. This material meets or exceeds.. |
|||
Melt Flow | 0.25 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.25 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Bapolene® 105F Low Density Polyethylene Film Resin Description: Bapolene LD105F is an unmodified low density polyethylene which extrudes into a low gloss high impact film. It contains antiblock additives and no slip additives. This product meets th.. |
|||
Melt Flow | 0.25 g/10 min @Load 2.16 kg |
0.25 g/10 min @Load 4.76 lb |
ASTM D 1238 |
Total Finathene® RS 528 HDPE blow molding
(discontinued **) Applications: Bleach and detergents, industrial chemicals, industrial parts, cosmetic bottles, food packaging.Information provided provided by Total Petrochemicals.Total Petrochemicals includes form.. |
|||
Melt Flow | 0.25 g/10 min | 0.25 g/10 min | Condition 190/2.16; ASTM D1238 |
Chevron Phillips Marlex® HHM 5502-01 ST High Density Ethylene Hexene Copolymer High Density Ethylene Hexene CopolymerSag Upper Limit: 18 cm, Lower Limit: 13 cm; 2 ft. X 4ft. X 125 mil thick blank heated to forming temperature.Data provided by Chevron Phillips Chemical Company.. |