Borealis FT3200 Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Film Grade
Manufacturer Borealis
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis FT3200 Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
FT3200 is a Low Density Polyethylene for Film Extrusion. Applications heavy-duty bags, shrink film, construction films, and agricultural films. FT3200 contains no additives.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ISO 1183
Melt Flow 0.25 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.25 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 400 %
400 %
ISO 527-3
Film Elongation at Break, TD 600 %
600 %
ISO 527-3
Tensile Modulus 0.160 GPa
23.2 ksi
MD/TD; ASTM D882-A
Puncture Energy 7.00 J
5.16 ft-lb
170N; ASTM D5748
Coefficient of Friction 0.70
0.70
Dynamic; ISO 8295
Elmendorf Tear Strength, MD 3.26 g/micron
82.8 g/mil
ISO 6383/2
Elmendorf Tear Strength, TD 5.71 g/micron
145 g/mil
ISO 6383/2
Dart Drop Test 500 g
1.10 lb
ISO 7765-1
Film Tensile Strength at Break, MD 25.0 MPa
3630 psi
ISO 527-3
Film Tensile Strength at Break, TD 26.0 MPa
3770 psi
ISO 527-3
Thermal Properties Metric English Comments
Melting Point 110 °C
230 °F
ISO 11357-3
Vicat Softening Point 92.0 °C
198 °F
ISO 306