Material Notes:
BorSafe™ HE3494-LS-H is a bimodal polyethylene compound produced by the advanced Borstar® technology. It includes a combination of pigments and stabilizers to ensure excellent long-term thermal stability and UV resistance. BorSafe™ HE3494-LS-H is classified as an MRS 10.0 material (PE100). Applications: BorSafe™ HE3494-LS-H is recommended for drinking water. It is especially designed for the production of larger diameter, thick wall pipe, but can be processed for the whole range of diameters.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 0.948 g/cc
0.0342 lb/in³
ISO 1872-2/ISO 1183
0.959 g/cc
0.0346 lb/in³
ISO 1872-2/ISO 1183
Environmental Stress Crack Resistance >= 5.0 hour

@Pressure 0.920 MPa,
Temperature 80.0 °C
>= 5.0 hour

@Pressure 133 psi,
Temperature 176 °F
ISO 13479
Oxidative Induction Time (OIT) >= 20 min

@Temperature 200 °C
>= 20 min

@Temperature 392 °F
EN 728
Melt Flow 0.25 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.25 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.0 MPa
3480 psi
50mm/min; ISO 527-2
Elongation at Break >= 600 %
>= 600 %
ISO 527-2
Tensile Modulus 1.00 GPa
145 ksi
1mm/min; ISO 527-3
Processing Properties Metric English Comments
Middle Barrel Temperature 190 - 210 °C
374 - 410 °F
cylinder
Die Temperature 200 - 210 °C
392 - 410 °F
Melt Temperature 200 - 220 °C
392 - 428 °F
Head Temperature 200 - 210 °C
392 - 410 °F
Descriptive Properties Value Comments
Resistance To Rapid Crack Propagation (bar) 10
S4 test, Pc at 0°C, test pipe 250mm, SDR11, ISO 13477