Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 43 g/10 min | 43 g/10 min | Exxon Method |
ExxonMobil Escorene® LD-783 EVA Copolymer for Specialty Applications
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 33% vinyl acetate copolymerApplications: Soft, injection molded parts; Low modulus applications. |
|||
Melt Flow | 43 g/10 min | 43 g/10 min | Exxon Method |
ExxonMobil Escorene® UL-7740 EVA Copolymer, Adhesive and Sealant Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 28% vinyl acetate copolymerApplications: Hot melt adhesives; Wax blends; Industrial sealants. |
|||
Melt Flow | 43 g/10 min @Load 10.0 kg, Temperature 220 °C |
43 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
LG Chemical HF380NS ABS, High Flow, General Anti-Static Feature: Injection Molding, High Flow, General Anti-StaticApplication: Electric & Electronic Products, Miscellaneous goods)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Melt Flow | 43 g/10 min @Load 10.0 kg, Temperature 220 °C |
43 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
LG Chemical HF380U ABS, High Flow Feature: Injection Molding, High Flow, Good WeatherabilityApplication: Electric & Electronic Products, Miscellaneous Goods)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Melt Flow | 43 g/10 min @Load 10.0 kg, Temperature 220 °C |
43 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
LG Chemical HG193S ABS, High Flow, Chemical Resistance Feature: Injection Molding, High Flow, Chemical ResistanceApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Melt Flow | 43 g/10 min @Load 5.00 kg, Temperature 260 °C |
43 g/10 min @Load 11.0 lb, Temperature 500 °F |
Estimated using room temperature density; ISO 1133 |
Lanxess Pocan® B 4235 Z 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding, flame retardant, impact modified |
|||
Melt Flow | 43 g/10 min @Load 5.00 kg, Temperature 190 °C |
43 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Multibase Multibatch® ME 50043 Anti-blocking Masterbatch LLDPE. 50% CaCO3, 30%TiO2FilledWhiteInformation provided by Multibase |
|||
Melt Flow | 43 g/10 min @Load 6.60 kg, Temperature 337 °C |
43 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM DT1810EV PEI Blend Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming, UL94 V0 listed. |
|||
Melt Flow | 43 g/10 min @Load 6.60 kg, Temperature 337 °C |
43 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM DT1810EV PEI Blend (Asia Pacific) Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming, UL94 V0 listed. |
|||
Melt Flow | 43 g/10 min @Load 6.60 kg, Temperature 337 °C |
43 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM EXUM0169 PEI Blend Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming. |
|||
Melt Flow | 43 g/10 min @Load 6.60 kg, Temperature 337 °C |
43 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM EXUM0169 PEI Blend (Asia Pacific) Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming. |
|||
Melt Flow | 43 g/10 min @Load 2.16 kg, Temperature 265 °C |
43 g/10 min @Load 4.76 lb, Temperature 509 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® IQ8280SF PBT+PET Valox iQ8280SF resin is an environmentally responsible, low carbon footprint, and sustainable resin. Valox iQ8280SF resin offer Super High Flow characteristics combined with high modulus and excell.. |
|||
Melt Flow | 43 g/10 min @Load 2.16 kg, Temperature 265 °C |
43 g/10 min @Load 4.76 lb, Temperature 509 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® IQ8280SF PBT+PET (Europe-Africa-Middle East) Valox iQ8280SF resin is an environmentally responsible, low carbon footprint, and sustainable resin. Valox iQ8280SF resin offer Super High Flow characteristics combined with high modulus and excell.. |
|||
Melt Flow | 43 g/10 min @Load 2.16 kg, Temperature 230 °C |
43 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
SCG Chemicals EL-Proâ„¢ P840J Polypropylene Injection Molding Key Characteristics:Excellent flowabilityExcellent processabilityHigh stiffnessSuitable for complex parts and large partsRecommended Applications:Automotive, motorcycle and electrical appliance part.. |
|||
Melt Flow | 43 g/10 min @Load 2.16 kg, Temperature 190 °C |
43 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238, ISO 1133 |
DuPont Elvax® 150W Ethylene Vinyl Acetate DuPont™ Elvax® 150W is an ethylene-vinyl acetate copolymer resin containing an anti-blocking additive for use in industrial applications. This resin is supplied in pellet form and to prevent the p.. |
|||
Melt Flow | 43 g/10 min @Load 2.16 kg, Temperature 190 °C |
43 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238, ISO 1133 |
DuPont Elvax® 240W Ethylene Vinyl Acetate DuPont™ Elvax® 240W is an ethylene-vinyl acetate copolymer resin for use in industrial applications. Addition: antiblock Applications:Elvax® 240W resins can be used for the following applications.. |
|||
Melt Flow | 43 g/10 min | 43 g/10 min | Condition not noted.; ASTM D1238 |
DuPont Elvax® 3185 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion 33 wt% Vinyl Acetate.Elvax® 3185 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.. |
|||
Melt Flow | 43 g/10 min @Load 2.16 kg, Temperature 190 °C |
43 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Escorene™ LD 783.CD Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra LD 783.CD is a 31.4% VA copolymer that is suitable for making a variety of specialty molding and extrusion compounds. It has high clarity and very low modulus. L.. |
|||
Melt Flow | 43 g/10 min @Load 2.16 kg, Temperature 190 °C |
43 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Escorene™ UL 04331EL Ethylene Vinyl Acetate Copolymer Product Description: UL 04331EL is a HEVA grade, especially designed for photovoltaic cells and encapsulation applications, requiring a good balance of adhesion and COF. It offers excellent light tr.. |
|||
Melt Flow | 43 g/10 min @Load 2.16 kg, Temperature 190 °C |
43 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Escorene™ UL 7741 Ethylene Vinyl Acetate Copolymer Availability: Latin America, North America and South America Additive: Antiblock: NoSlip: NoThermal Stabilizer: Yes Applications:Adhesives and SealantsIndustrial SealantsHot Melt AdhesivesWax Blends.. |
|||
Melt Flow | 43 g/10 min @Load 10.0 kg, Temperature 220 °C |
43 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D-1238 |
Bhansali Engineering Abstron MIF-45 ABS Injection Molding Grade High Impact, Medium, High Flow, General PurposeInformation provided by Bhansali |
|||
Melt Flow | 43 g/10 min @Load 2.16 kg, Temperature 190 °C |
43 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 2514 MDPE Injection Molding Resin
(discontinued **) Features: Excellent processability for applications requiring moderate stiffness and toughness, good cold temperature impact properties.Applications: Roll-out cart lids, housewares, deep skirt lids,.. |
|||
Melt Flow | 43 g/10 min @Load 2.16 kg, Temperature 190 °C |
43 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238, ISO 1133 |
DuPont Elvax® 240 Ethylene Vinyl Acetate
(discontinued **) DuPont™ Elvax® 240 is an ethylene-vinyl acetate copolymer resin for use in industrial applications. Applications:Elvax® 240 resins can be used for the following applications: adhesives, sealants,.. |
|||
Melt Flow | 43 g/10 min | 43 g/10 min | ASTM D1238 |
ExxonMobil Escorene® LD 783.ND Molding, extrusion and compounding resin
(discontinued **) Escorene Ultra LD 783.ND is a 33% vinyl acetate copolymer suitable for making a variety of specialty molding and extrusion compounds. It has high clarity and a very low modulus.Information provided .. |
|||
Melt Flow | 43 g/10 min | 43 g/10 min | Exxon Method |
ExxonMobil Escorene® UL-7840C EVA Copolymer, Adhesive and Sealant Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 33% vinyl acetate copolymerApplications: Hot melt adhesives; Wax blends; Industrial sealants. |
|||
Melt Flow | 43 g/10 min @Load 10.0 kg, Temperature 220 °C |
43 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D-1238 |
Bhansali Engineering Abstron MIF-45 ABS Injection Molding Grade High Impact, Medium, High Flow, General PurposeInformation provided by Bhansali |