Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Escorene® LD-783 EVA Copolymer for Specialty Applications  (discontinued **)

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate; Molded/Extruded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene® LD-783 EVA Copolymer for Specialty Applications  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Data provided by the manufacturer, Exxon Chemical.A 33% vinyl acetate copolymerApplications: Soft, injection molded parts; Low modulus applications.
Physical Properties Metric English Comments
Density 0.956 g/cc
0.0345 lb/in³
Exxon Method
Apparent Bulk Density 0.577 g/cc
0.0208 lb/in³
ASTM D1895 (B)
Melt Flow 43 g/10 min
43 g/10 min
Exxon Method
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 3.00 MPa
435 psi
ASTM D638
Elongation at Break 1050 %
1050 %
ASTM D638
Thermal Properties Metric English Comments
Melting Point 61.0 °C
142 °F
Exxon Method
Vicat Softening Point 105 °C
221 °F
Softening Point, R&B; ASTM E-28
Users viewing this material also viewed the following: