Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Escorene™ LD 783.CD Ethylene Vinyl Acetate Copolymer

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer Exxon Chemical
Trade Name Escorene™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene™ LD 783.CD Ethylene Vinyl Acetate Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: Escorene Ultra LD 783.CD is a 31.4% VA copolymer that is suitable for making a variety of specialty molding and extrusion compounds. It has high clarity and very low modulus. LD 783.CD contains an additive package to improve pellet flowabiltiy and handling.Availability: North America and South America Additive: Antiblock: NoSlip: NoThermal Stabilizer: YesApplications:Crosslinkable CompoundsExtrusion CompoundsMolding CompoundsWire and Cable CompoundsInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.955 g/cc
0.0345 lb/in³
ExxonMobil method
Vinyl Acetate Content 31.4 %
31.4 %
ExxonMobil method
Melt Flow 43 g/10 min

@Load 2.16 kg,
Temperature 190 °C
43 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 55

@Time 15.0 sec
55

@Time 0.00417 hour
ASTM D2240
Tensile Strength at Break 3.03 MPa
440 psi
ASTM D638
Elongation at Break >= 800 %
>= 800 %
ASTM D638
Flexural Modulus, 1% Secant 12.4 MPa
1800 psi
ASTM D790
Dart Drop, Total Energy 10.8 J

@Temperature 22.8 °C
8.00 ft-lb

@Temperature 73.0 °F
ASTM D3763
29.8 J

@Temperature -40.0 °C
22.0 ft-lb

@Temperature -40.0 °F
ASTM D3763
Thermal Properties Metric English Comments
Melting Point <= 136 °C
<= 277 °F
Peak Melting Point; ExxonMobil method
Users viewing this material also viewed the following: