Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Elvax® 240 Ethylene Vinyl Acetate  (discontinued **)

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Elvax® 240 Ethylene Vinyl Acetate  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
DuPont™ Elvax® 240 is an ethylene-vinyl acetate copolymer resin for use in industrial applications. Applications:Elvax® 240 resins can be used for the following applications: adhesives, sealants, and wax blends; wires and cables. Information provided by DuPont™
Physical Properties Metric English Comments
Density 0.951 g/cc
0.0344 lb/in³
ASTM D792-ISO 1183, ASTM D1505
Vinyl Acetate Content 28 %
28 %
Melt Flow 43 g/10 min

@Load 2.16 kg,
Temperature 190 °C
43 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238, ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore A 78
78
ASTM D2240-ISO 868
Hardness, Shore D 26
26
ASTM D2240-ISO 868
Thermal Properties Metric English Comments
Melting Point 74.0 °C
165 °F
DSC; ASTM D3417- ISO 3146
Vicat Softening Point 40.0 °C
104 °F
ASTM D1525, ISO 306
Brittleness Temperature -100 °C
-148 °F
ASTM D746
Ring & Ball Softening Point 110 °C
230 °F
ASTM E28
Descriptive Properties Value Comments
Cloud Point in Paraffin Wax, °C 66
10% Elvax® in fully refined paraffin wax, 146 AMP. Incompatible at temperatures up to 177°C.