DuPont Elvax® 3185 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade
Manufacturer DuPont Packaging and Industrial Polymers
Trade Name Elvax®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Elvax® 3185 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
33 wt% Vinyl Acetate.Elvax® 3185 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.Additives: Antioxidant.Applications: Elvax® 3185 is designed to provide a low temperature heat seal to itself or many other materials commonly used in flexible packaging applications. The melt properties of this resin allow it to be processed on blown or cast coextrusion film equipment over a wide range of line speeds and film thicknesses. It can be coextruded with a variety of other polymers. Elvax®3185 is typically used as a low temperature seal layer in coextruded film. Information provided by DuPont Packaging Polymers.
Physical Properties Metric English Comments
Density 0.960 g/cc
0.0347 lb/in³
ASTM D792
Melt Flow 43 g/10 min
43 g/10 min
Condition not noted.; ASTM D1238
Thermal Properties Metric English Comments
Melting Point 37.0 °C
98.6 °F
Freezing Point via DSC/ASTM D3418
61.0 °C
142 °F
Upon Melting via DSC/ASTM D3418
Vicat Softening Point 40.0 °C
104 °F
ASTM D1525