Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 3.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
STN EN ISO 1133 |
Plastcom SLOVAMID 6 GF 15 LS Polyamide 6, 15% Glass Fiber, UV Stabilization FeaturesPA 6 for injection moulding, chemically reinforced with 15% glass fiber, stabilized against UV-radiation. Used for the grips of electric tools, hobby tools, gears, covers of electric tools... |
|||
Melt Flow | 3.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
Procedure A; ASTM D1238 |
PolyOne Maxxam™ MN-818.S001-8000 Polypropylene, Unspecified (PP, Unspecified) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Melt Flow | 3.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
3.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 4504 PPC (Asia Pacific) High heat resistant polycarbonate copolymer, provides DTUL of 290F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported wit.. |
|||
Melt Flow | 3.0 - 9.0 g/10 min @Load 2.16 kg, Temperature 250 °C |
3.0 - 9.0 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
Polymer Resources TP-FR-IM Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low Flow Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa.. |
|||
Melt Flow | 3.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
Condition L; ASTM D1238 |
PolyMirae Moplen HP420J BDDP Film Grade Polypropylene Moplen HP420J is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP420J is a homopolymer particularly suitable for BOPP (Tender) fi.. |
|||
Melt Flow | 3.0 g/10 min @Load 1.00 kg, Temperature 235 °C |
3.0 g/10 min @Load 2.20 lb, Temperature 455 °F |
ASTM D1238 |
Honeywell Aegis™ HCA95QP Nylon 6/6,6 Extrusion Grade Copolymer
(discontinued **) Description: Aegis HCA95QP is a lubricated medium viscosity, nylon 6/6,6 extrusion grade copolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500.. |
|||
Melt Flow | 3.0 g/10 min | 3.0 g/10 min | ASTM D1238 |
LyondellBasell Petrothene® NA324009 Low Density Polyethylene (Film Grade) ApplicationsPETROTHENE NA 324 is a series of homopolymer resins specifically designed for overwrap packaging. NA 324 provides excellent optical properties and good stiffness for improved machineabi.. |
|||
Melt Flow | 3.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1183 |
Metabolix M-vera™ B5010 Film Grade Compostable Bioplastic For use in tough, certified compostable film and bag applications. Mvera B5010 offers a wide range of attractive traits—excellent tear and puncture toughness, excellent seal strength, good prin.. |
|||
Melt Flow | 3.0 g/10 min @Load 12.5 kg, Temperature 200 °C |
3.0 g/10 min @Load 27.6 lb, Temperature 392 °F |
2 mm x 8 mm |
Ineos Barex® 210 E Acrylonitrile-Methyl Acrylate Copolymer Extrusion Grade. Barex® Resins are available in either natural or blue tint. Barex® 210E is most commonly used for thermoformed sheet applications. |
|||
Melt Flow | 3.0 - 4.0 g/10 min | 3.0 - 4.0 g/10 min | ASTM D1238 |
Micropol Microlin ML20 Linear Polyethylene Rotational Molding Powder Information provided by Micropol Limited |
|||
Melt Flow | 3.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Multibase Multi-Flex® G 7940 TPE Styrene Ethylene Butylene Styrene Block Copolymer Features: Chemical Resistance, Good General PurposeOzone Resistant Thermal Stability, Good Forms:PelletsProcessing Method:Injection MoldingBlow MoldingExtrusion Uses: Automotive ApplicationsInfor.. |
|||
Melt Flow | 3.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
Condition L; ASTM D1238 |
LyondellBasell Hostacomâ„¢ BR712GC Polypropylene Copolymer Description: Hostacomâ„¢ BR712GC conventional melt flow, 1,300 MPa flexural modulus, UV-stabilized, mineral-filled polypropylene copolymer has an excellent balance of stiffness, impact and weathe.. |
|||
Melt Flow | 3.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D 1238 |
Styrolution PS 6220 HIPS Excellent toughnessHigh glossDesigned for deep draw thermoformingInformation provided by Styrolution |
|||
Melt Flow | 3.0 g/10 min | 3.0 g/10 min | ISO 1133 |
Borealis Borclear™ RC707MO Polypropylene Borclear™ RC707MO is intended for blow molding. This grade provides high gloss, high transparency and excellent impact properties. This grade also features high heat distortion temperature. Applic.. |
|||
Melt Flow | 3.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis Borpact™ BC914TF Polypropylene Copolymer Borpact™ BC914TF is a high crystalline heterophasic copolymer film resin, based on special Borstar® nucleating technology. This grade is especially developed for the manufacturing of unoriented f.. |
|||
Melt Flow | 3.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman PAPERMATCH® H-3818 Specialty Masterbatch DescriptionPAPERMATCH® H-3818 is a specialty masterbatch formulated to impart paper-like properties to polyethylene films. PAPERMATCH® H-3818 is a natural color, low opacity grade designed to pro.. |
|||
Melt Flow | 3.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Total PPH 4042 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 4042 is a nucleated homopolymer.ApplicationATOFINA Polypropylene PPH 4042 has been developed for extrusion-thermoforming, providing improved rigidity and impact resistance .. |
|||
Melt Flow | 3.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Total PSI 825EX Polystyrene Polystyrene 825EX is a high impact polystyrene designed for high stiffness in extrusion/thermoforming applications. The balance of high stiffness and impact properties allow for light weighting of t.. |
|||
Melt Flow | 3.0 g/10 min @Load 5.00 kg, Temperature 190 °C |
3.0 g/10 min @Load 11.0 lb, Temperature 374 °F |
ASTM D1238 |
ELASTO UK Dryflex® 650900 TPE, Improved Compression Set and High Temperature Resistance, 90A Hardness The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. This grade is designed with improved compressi.. |
|||
Melt Flow | 3.0 - 10 g/10 min @Load 5.00 kg, Temperature 230 °C |
3.0 - 10 g/10 min @Load 11.0 lb, Temperature 446 °F |
ISO 1133 |
Eurostar Starpylen MFB44S PP, Glass Bead/Glass Fiber Filled Starpylen MFB44S is a Glass Beads, Glass Fiber Reinforced, Polypropylene Injection Molding Resin heat stabilized (also known as Starpylen WS 2020VK S37.7)Information provided by Eurostar. |
|||
Melt Flow | 3.0 g/10 min | 3.0 g/10 min | ASTM D1238 |
Aclo Accucomp ABS ABS811L Medium Impact Grade |
|||
Melt Flow | 3.0 g/10 min | 3.0 g/10 min | ASTM D1238 |
Aclo Accucomp ABS ABS881L Clear Grade |
|||
Melt Flow | 3.0 g/10 min | 3.0 g/10 min | ASTM D1238 |
Aclo Accuguard Polypropylene CP0467V0CSL Copolymer Flame Retardant Copper Stabilized |
|||
Melt Flow | 3.0 g/10 min | 3.0 g/10 min | ASTM D1238 |
Aclo Accutech Nylon 6 NY0730G40L Glass Reinforced |
|||
Melt Flow | 3.0 g/10 min | 3.0 g/10 min | ASTM D1238 |
Aclo Accutech Polypropylene Homopolymer HP0336G10M20CL Glass/Mineral Reinforced Coupled |
|||
Melt Flow | 3.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Carmel Olefins CAPILENE® G 65 F Polypropylene Homopolymer Description: CAPILENE® G 65 F is a polypropylene homopolymer designed for the production of biaxially oriented polypropylene films (BOPP). It exhibits good processability, easy film stretchabilit.. |
|||
Melt Flow | 3.0 - 8.0 g/10 min @Load 12.5 kg, Temperature 232 °C |
3.0 - 8.0 g/10 min @Load 27.6 lb, Temperature 450 °F |
ASTM D1238 |
Arkema Group KYNAR FLEX® 2800-01 Polyvinylidene Fluoride Copolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical s.. |
|||
Melt Flow | 3.0 - 7.0 g/10 min | 3.0 - 7.0 g/10 min | |
Asahi Glass Fluon® P-65P PFA Perfluoropolymer Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character.. |
|||
Melt Flow | 3.0 - 7.0 g/10 min | 3.0 - 7.0 g/10 min | |
Asahi Glass Fluon® P-805UP PFA Perfluoropolymer Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character.. |
|||
Melt Flow | 3.0 - 8.0 g/10 min @Load 12.5 kg, Temperature 232 °C |
3.0 - 8.0 g/10 min @Load 27.6 lb, Temperature 450 °F |
ASTM D1238 |
Arkema Group KYNAR FLEX® 2850-00 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |