Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.650 - 0.850 g/cc | 0.0235 - 0.0307 lb/in³ | ISO 60 |
Raschig Group SURAPLAST UPA 63 UP Glass fiber reinforced polyester molding compound. Minimal mold shrinkage and post-shrinkage, very good arc resistance, very good mechanical strength. This product meets the allowed upper limits for.. |
|||
Apparent Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | ISO 60 |
Hexion Bakelite™ PF 13 Phenolic Formaldehyde Resin, UL Listed
(discontinued **) Phenolic molding compound, inorganically mica filled, heat resistance, good electrical properties, UL listed molding compound 0.75 mm/V-1 (NC), 3 mm/V-0, standardized molding compound.Application ar.. |
|||
Apparent Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | ISO 60 |
Hexion Bakelite™ PF 2400 Phenolic Formaldehyde Resin, High Surface Quality, Dishwasher Proof, UL Listed
(disc Phenolic molding compound, inorganically/organically filled, average heat resistance, increased dimensional stability, dish washer proof, UL listed molding compound 1.5 mm/V-0 (ALL).Application area.. |
|||
Apparent Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | ISO 60 |
Hexion Bakelite™ PF 12404 Phenolic Formaldehyde Resin, High Surface Quality, Low Shrinkage
(discontinued **)& Phenolic molding compound, inorganically/organically filled, good dimensional stability, low shrinkage.Application areas: Housing parts for gas meter.Information provided by Bak AGBak AG became a pa.. |
|||
Apparent Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | ISO 60 |
Hexion Bakelite™ PF 38110 Phenolic Formaldehyde Resin, High Surface Quality
(discontinued **) Phenolic molding compound, mainly organically filled.Application areas: Devices for the electrical installation, pan handles, knobs, mainly for compression molding.Information provided by Bak AGBak .. |
|||
Apparent Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | ASTM D1895 |
Plenco 5303 Black Electrical Grade Mineral/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok 5303 is a two-stage, mineral and flock-filled phenolic molding compound designed for use in appliance, automotive and electrical applications. It can be molded by compression, transfer or i.. |
|||
Apparent Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | ASTM D1895 |
Solvay Specialty Polymers Catalyst PS/2 Black Polyolefin Catalyst PS/2 is a PE based black catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water.. |
|||
Apparent Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | ISO 60 |
Styron MAGNUMâ„¢ 3416 SLG Acrylonitrile Butadiene Styrene (ABS) Resin Overview: The mass (continuous process) ABS technology of Styron ensures an ABS resin that combines excellent processability with a stable light base color providing an ideal resin for self coloring.. |
|||
Apparent Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | ISO 60 |
Styron MAGNUMâ„¢ 3904 Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ 3904 is a resin with super-high impact. It is used in a wide range of technical applications. It can be processed by injection molding, extrusion or thermoforming. The mass (c.. |
|||
Apparent Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | ISO 60 |
Styron MAGNUMâ„¢ 3904 Smooth Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ 3904 is an extrusion/thermoforming resin developed for high impact and other technical applications. The mass (continuous process) ABS technology of Styron ensures an ABS tech.. |
|||
Apparent Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | ISO 60 |
Styron MAGNUMâ„¢ 8391 Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ 8391 ABS combines an excellent glossy appearance with high flow and medium impact performance. The mass continuous process) ABS technology of Styron ensures an ABS resin that .. |
|||
Apparent Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | ISO 60 |
Styron Magnumâ„¢ 8391 MED Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ MED ABS combines an excellent glossy appearance with high flow and medium impact performance. The mass (continuous process) ABS technology of Styron ensures an ABS resin that .. |
|||
Apparent Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | ASTM D1895 |
Sumitomo Bakelite Durez® 156 Phenolic, Compression Grade Durez 156 Black Phenolic is a two-stage, asbestos-free, heat resistant/electrical molding material. It exhibits excellent dimensional stability, high heat resistance, good molded appearance, and UL.. |
|||
Apparent Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | ASTM D1895 |
Sumitomo Bakelite Durez® 156 Phenolic, Injection Grade Durez 156 Black Phenolic is a two-stage, asbestos-free, heat resistant/electrical molding material. It exhibits excellent dimensional stability, high heat resistance, good molded appearance, and UL.. |
|||
Apparent Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | circa |
Cresset Powers Cress-Alon™ A2350 2.35 r.v. Injection Molding Grade Nylon 6, 50% RH Neat resin, for injection molding.Information provided by Cresset Powers Ltd. |
|||
Apparent Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | circa |
Cresset Powers Cress-Alon™ A2350 2.35 r.v. Injection Molding Grade Nylon 6, Dry As Molded Neat resin, for injection molding.Information provided by Cresset Powers Ltd. |
|||
Apparent Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | circa |
Cresset Powers Cress-Alon™ A3000 3.0 r.v. Film or Extrusion Grade Nylon 6, 50% RH Neat resin, for film or extrusion.Information provided by Cresset Powers Ltd. |
|||
Apparent Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | circa |
Cresset Powers Cress-Alon™ A3000 3.0 r.v. Film or Extrusion Grade Nylon 6, Dry As Molded Neat resin, for film or extrusion.Information provided by Cresset Powers Ltd. |
|||
Apparent Bulk Density | 0.650 - 0.720 g/cc | 0.0235 - 0.0260 lb/in³ | IS 867-1963 |
Amity Thermosets ATS 155 Phenolic Molding Inorganic and glass fiber Filler, Compression Molded Characteristics:Shock resistantElectrical low lossHigh mechanical strengthHeat stableHigh electrical insulationDimensional stabilityGood mechanical tension bearing strengthGood copper adhesion Color.. |
|||
Apparent Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | ASTM D1895 |
Teknor Apex Sinvicomp DFR 5806 Polyvinyl Chloride, Rigid Availability: Asia Pacific Features: Good Impact Resistance Uses: Profiles Forms: Powder Processing Method: ExtrusionInformation Provided by Teknor Apex |
|||
Apparent Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | ASTM D4894 |
Solvay Specialty Polymers Algoflon® A.15 PTFE (Polytetrafluoroethylene)
(discontinued **) Data provided by the manufacturer.Type IV.G.1 Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent dielectric p.. |
|||
Apparent Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | ASTM D1895 |
Ashley Polymers Ashlene® R6043 Nylon 6 Medium viscosity extrusion grade Nylon 6 resin with excellent melt stability, good melt strength: suitable for extrusion coating and film co-extrusion applications. Excellent grease resistance, tou.. |
|||
Apparent Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | ISO 60 |
Hexion Bakelite™ PF 4041 Phenolic Formaldehyde Resin, Resistant to High Temperatures
(discontinued **) Phenolic molding compound, glass fiber reinforced and inorganically filled, elasticized. Very good heat resistance, very good mechanical properties, reduced mold shrinkage and post-shrinkage, good .. |
|||
Apparent Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | ASTM D1895 |
Plaslok 5303 Black Electrical Grade Mineral/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 5303 is a two-stage, mineral and floc.. |