Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Cresset Powers Cress-Alon™ A2350 2.35 r.v. Injection Molding Grade Nylon 6, Dry As Molded

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Cresset Powers, Ltd
Trade Name Cress-Alon™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cresset Powers Cress-Alon™ A2350 2.35 r.v. Injection Molding Grade Nylon 6, Dry As Molded.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Neat resin, for injection molding.Information provided by Cresset Powers Ltd.
Physical Properties Metric English Comments
Density 1.12 - 1.14 g/cc
0.0405 - 0.0412 lb/in³
ASTM D792
Apparent Bulk Density 0.650 g/cc
0.0235 lb/in³
circa
Viscosity Measurement 2.3 - 2.4
2.3 - 2.4
Relative Viscosity
Melt Flow 79 g/10 min

@Load 2.16 kg,
Temperature 230 °C
79 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 80.0 MPa
11600 psi
ASTM D638
Tensile Strength, Yield 84.0 MPa
12200 psi
ASTM D638
Elongation at Break 55 %
55 %
ASTM D638
Elongation at Yield 3.6 %
3.6 %
ASTM D638
Flexural Yield Strength 111 MPa
16100 psi
ASTM D790
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ASTM DSC
Deflection Temperature at 0.46 MPa (66 psi) 185 °C
365 °F
Processing Properties Metric English Comments
Moisture Content <= 0.10 %
<= 0.10 %
Descriptive Properties Value Comments
Extractables, wt% <0.5