Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 25 g/10 min @Load 5.00 kg, Temperature 260 °C |
25 g/10 min @Load 11.0 lb, Temperature 500 °F |
ISO 1133 |
Polykemi AB POLYblend 65 M10 PC/ABS-blend, Reinforced Information provided by Polykemi AB |
|||
Melt Index of Compound | 25 g/10 min @Load 5.00 kg, Temperature 260 °C |
25 g/10 min @Load 11.0 lb, Temperature 500 °F |
ISO 1133 |
Polykemi AB POLYblend 65FS LB PC/ABS-Blend Information provided by Polykemi AB |
|||
Melt Index of Compound | 25 g/10 min @Load 5.00 kg, Temperature 260 °C |
25 g/10 min @Load 11.0 lb, Temperature 500 °F |
ISO 1133 |
Polykemi AB POLYblend 65V PC/ABS-Blend, Flame Retardant Information provided by Polykemi AB |
|||
Melt Index of Compound | 25 g/10 min @Load 5.00 kg, Temperature 260 °C |
25 g/10 min @Load 11.0 lb, Temperature 500 °F |
ISO 1133 |
Polykemi AB POLYblend 85VB PC/ABS-Blend, Flame Retardant Information provided by Polykemi AB |
|||
Melt Index of Compound | 25 g/10 min @Load 2.16 kg, Temperature 260 °C |
25 g/10 min @Load 4.76 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® CY6009 PC+ABS (Asia Pacific) CY6009 is a flame retardant (FR) PC+ABS blend with non-brominated and non-chlorinated FR systems. Its excellent flow together with balanced properties and thin wall 5VB capability at less than 2 mm.. |
|||
Melt Index of Compound | 25 g/10 min @Load 5.00 kg, Temperature 220 °C |
25 g/10 min @Load 11.0 lb, Temperature 428 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics LNP COLORCOMP EX12304C PEI (Asia Pacific) LNP* Colorcomp* EX12304C is an unfilled polyetherimide clean compound with extremely high level of cleanliness for the most demanding application. This compound is manufactured using LNP CCS technol.. |
|||
Melt Index of Compound | 25 g/10 min @Load 2.16 kg, Temperature 230 °C |
25 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPC T25020 UV Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Index of Compound | 25 g/10 min @Load 2.16 kg, Temperature 230 °C |
25 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPH GF35040 D PP, Glass Fiber-Reinforced, Chemically Coupled, Detergent Resistant Information provided by Polykemi AB |
|||
Melt Index of Compound | 25 g/10 min @Load 5.00 kg, Temperature 372 °C |
25 g/10 min @Load 11.0 lb, Temperature 702 °F |
ASTM D1238 |
3M Dyneon™ PFA 6525N Perfluoroalkoxy Fluorothermoplastic
(discontinued **) The excellent chemical temperature resistance of Dyneon™ 6500N PFA is available across a range of melt flow indices, for optimal processability. Dyneon™ PFA 6502N, the highest molecular weight gra.. |
|||
Melt Index of Compound | 25 g/10 min @Load 21.6 kg, Temperature 190 °C |
25 g/10 min @Load 47.6 lb, Temperature 374 °F |
MVR, [cm<sup>3</sup>/10 min] |
Huntsman IROGRAN® A 78 E 4506 TPU-Polyester Introduction: IROGRAN A 78 E 4506 is a thermoplastic polyester- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are excellent mechanical prop.. |
|||
Melt Index of Compound | 25 g/10 min @Load 21.6 kg, Temperature 190 °C |
25 g/10 min @Load 47.6 lb, Temperature 374 °F |
|
Huntsman IROGRAN® PS442-202 TPU-Polyester Introduction: IROGRAN PS440-202 is a high performance polyester based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN PS440-202 is part of the HUNTSMAN .. |
|||
Melt Index of Compound | 25 g/10 min @Load 2.16 kg, Temperature 190 °C |
25 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ICO Polymers ICOTEXâ„¢ 520-5004 1000 Micron EVA Powder Description: ICOTEX 520-5004 is an EVA powder that has been developed to meet the special requirements of the textile coating industry. Key Characteristics: good melt flow and flexibility and a viny.. |
|||
Melt Index of Compound | 25 g/10 min @Load 1.20 kg, Temperature 280 °C |
25 g/10 min @Load 2.65 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL V081 PPE+HIPS (Europe-Africa-Middle East) NORYL V081 is a high flow, UV stabilized PPO/PS blend for TV backplate applications. |
|||
Melt Index of Compound | 25 g/10 min @Load 5.00 kg, Temperature 360 °C |
25 g/10 min @Load 11.0 lb, Temperature 680 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM 1010K PEI Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming. |
|||
Melt Index of Compound | 25 g/10 min @Load 5.00 kg, Temperature 360 °C |
25 g/10 min @Load 11.0 lb, Temperature 680 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM HU1010 PEI Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI),.. |
|||
Melt Index of Compound | 25 g/10 min @Load 5.00 kg, Temperature 265 °C |
25 g/10 min @Load 11.0 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Xenoy® X5300WX PBT+PC (Europe-Africa-Middle East) Unreinforced, opaque PBT+PC alloy. Chemical resistance and good mechanical performance. UV-stabilized. Excellent weatherability. |
|||
Melt Index of Compound | 25 g/10 min | 25 g/10 min | |
Sibur PL-1GS Polyvinyl Chloride (PVC) For the production of boot tops and soles of autumn-spring purpose and for production of boots by molding method under pressure. |
|||
Melt Index of Compound | 25 g/10 min @Load 5.00 kg, Temperature 360 °C |
25 g/10 min @Load 11.0 lb, Temperature 680 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM AUT200 PEI Transparent high flow Polyetherimide (Tg 217C). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperat.. |
|||
Melt Index of Compound | 25 g/10 min @Load 2.16 kg, Temperature 250 °C |
25 g/10 min @Load 4.76 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® SHF4910 PBT (Europe-Africa-Middle East) 6.5% glass reinforced, Super High Flow, flame retardant PBT. |
|||
Melt Index of Compound | 25 - 31 g/10 min @Load 2.16 kg, Temperature 250 °C |
25 - 31 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
Shinkong Synthetic Fibers Shinite® D201K006 PBT, Medium Viscosity Information from Shinkong Synthetic Fibers Corp. |
|||
Melt Index of Compound | 25 g/10 min @Load 2.16 kg, Temperature 280 °C |
25 g/10 min @Load 4.76 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL EXNL1117 PPE+HIPS high gloss Noryl |
|||
Melt Index of Compound | 25 g/10 min @Load 2.16 kg, Temperature 280 °C |
25 g/10 min @Load 4.76 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL FXN4020H PPE+HIPS (Europe-Africa-Middle East) high gloss Noryl |
|||
Melt Index of Compound | 25 g/10 min @Load 2.16 kg, Temperature 230 °C |
25 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman POLYFORT™ FTP 3130H-01/FTP 3130HU-Colors DescriptionPolyfort® FTP 3130H-01 (non-UV stabilized) and FTP 3130HU-Colors (UV-stabilized) are high flow injection molding polyolefin alloys which exhibit an exceptional stiffness-impact balance a.. |
|||
Melt Index of Compound | 25 g/10 min @Load 2.16 kg, Temperature 190 °C |
25 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
DuPont Nucrel® 925 Ethylene-Methacrylic Acid Copolymer Resin Nucrel® 925 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for .. |
|||
Melt Index of Compound | 25 g/10 min @Load 2.16 kg, Temperature 230 °C |
25 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman POLYFORT™ FTP 3130H-01/FTP 3130HU-Colors DescriptionPolyfort® FTP 3130H-01 (non-UV stabilized) and FTP 3130HU-Colors (UV-stabilized) are high flow injection molding polyolefin alloys which exhibit an exceptional stiffness-impact balance a.. |
|||
Melt Index of Compound | 25 g/10 min @Load 2.16 kg, Temperature 230 °C |
25 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman POLYFORT™ FTP 3130H-01/FTP 3130HU-Colors DescriptionPolyfort® FTP 3130H-01 (non-UV stabilized) and FTP 3130HU-Colors (UV-stabilized) are high flow injection molding polyolefin alloys which exhibit an exceptional stiffness-impact balance a.. |
|||
Melt Index of Compound | 25 g/10 min @Load 5.00 kg, Temperature 265 °C |
25 g/10 min @Load 11.0 lb, Temperature 509 °F |
ASTM D1238 |
3M Dyneon™ THVP 2030GZ Fluorothermoplastic Granules THVP 2030GZ is a very flexible, transparent fluoroplastic composed of fluorinated monomers. It is ideal for applications that require the good temperature, chemical and flame resistance of a fluorop.. |
|||
Melt Index of Compound | 25 - 35 g/10 min @Load 2.16 kg, Temperature 190 °C |
25 - 35 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Petroquimica Triunfo Trithene® JX 7300 LDPE - Injection Molding The Trithene® JX 7300 resin is a low-density polyethylene (LDPE) with outstanding flow ability and flexibility. Those attributes are especially important to meet the requirements for fast injection.. |
|||
Melt Index of Compound | 25 g/10 min @Load 5.00 kg, Temperature 360 °C |
25 g/10 min @Load 11.0 lb, Temperature 680 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM AUT200 PEI (Europe-Africa-Middle East) Transparent high flow Polyetherimide (Tg 217C). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperatu.. |
|||
Melt Index of Compound | 25 g/10 min | 25 g/10 min | ASTM D1238 |
DuPont Elvax® 250 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |