Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Petroquimica Triunfo Trithene® JX 7300 LDPE - Injection Molding

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer Petroquimica Triunfo
Trade Name Trithene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Petroquimica Triunfo Trithene® JX 7300 LDPE - Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The Trithene® JX 7300 resin is a low-density polyethylene (LDPE) with outstanding flow ability and flexibility. Those attributes are especially important to meet the requirements for fast injection cycles and thin wall parts. This product complies with ASTM standard D1248-IA1.Applications: Lids, covers and caps for frozen food storage. Housewares. Toys and decorative items. Production of Master Batch for dyeing and concentrate of additives such as slip agent, anti-block, anti-static, etc.Resin Properties: Compressed molded plate. Method ASTM D-1928, procedure C.Information provided by Dax Resinas
Physical Properties Metric English Comments
Density 0.915 - 0.919 g/cc
0.0331 - 0.0332 lb/in³
ASTM D1505
Melt Index of Compound 25 - 35 g/10 min

@Load 2.16 kg,
Temperature 190 °C
25 - 35 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 7.00 MPa
1020 psi
ASTM D638
Tensile Strength, Yield 9.00 MPa
1310 psi
ASTM D638
Elongation at Break 120 %
120 %
ASTM D638
Thermal Properties Metric English Comments
Melting Point 108 °C
226 °F
ASTM D3418
Vicat Softening Point 78.0 °C
172 °F
ASTM D1525
Processing Properties Metric English Comments
Feed Temperature 170 - 210 °C
338 - 410 °F
Die Cooling Temperature 25.0 - 45.0 °C
77.0 - 113 °F
Copyright © lookpolymers.com All Rights Reserved