Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | STN EN ISO 294-4 |
Plastcom PLASTAMID® 66 BT B 27 TS PA66 heat stabilized Basic type PA66 for injection molding, heat stabilized, modified for general use, with excellent manufacturing properties. Use: automotive, engineering, electrical and consumer-goods industry - elec.. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm @Thickness 2.00 mm |
0.019 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Delrin® FG900P NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG900P is a low viscosity acetal homopolymer, with improved thermal stability. It has been developed for consideration into applications such as parts for the food industry.Information prov.. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm @Thickness 2.00 mm |
0.019 in/in @Thickness 0.0787 in |
|
Aardvark Polymers AARTEL® 2100UV Acetal Homopolymer Rotational Molding Resin Aartel 2100UV is a natural acetal homopolymer with UV stabilizers.Aartel 2100UV is a medium viscosity resin with excellent flow characteristics.Aartel 2100UV is available in natural white and may be.. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | 60x60x2 mm; ISO 294-4 |
Gromax BTE25-DN00N1 Nylon 6 (Dry) Information provided by Gromax Enterprises Corp. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | 60x60x2 mm; ISO 294-4 |
Gromax BTE35-DN00N1 Nylon 6 (Dry) Information provided by Gromax Enterprises Corp. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | 60x60x2 mm; ISO 294-4 |
Gromax BTE70-FN001N1 Nylon 6 (Dry) Information provided by Gromax Enterprises Corp. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | 60x60x2 mm; ISO 294-4 |
Gromax BTE45-DN00N1 Nylon 6 (Dry) Information provided by Gromax Enterprises Corp. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | RHODIA-EP |
Solvay Technyl® A 246M Nylon 66, Impact Grade, EH0 Unreinforced and modified polyamide 66, with improved impact resistance, heat stabilized, for injection molding.Technyl A 246m offers an excellent notched impact resistance at low temperatures makin.. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | |
Solvay TECHNYL® A 246M PA66, DRY Description: Unreinforced and modified polyamide 66, with very high impact resistance even at low temperature, for injection molding.Available in: Europe and North AmericaProduct Applications: TECHN.. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | |
Solvay TECHNYL® A 402H1 Natural PA66, DRY Description: TECHNYL® A 402H1 is an unreinforced polyamide 66, very high viscosity, heat stabilized, for extrusion and injection molding. This product is available in natural color.Benefits: The .. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | |
Solvay TECHNYL® A 216 PA66, DRY Description: Unreinforced polyamide 66, medium viscosity, for injection molding.Available in: Asia Pacific and Latin AmericaProduct Applications: TECHNYL ® A 216 offers all of the primary propert.. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm @Time 86400 sec |
0.019 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP WBL36L PBT (Asia Pacific) LNP* Lubricomp* WBL36L is a compound based on Polybutylene Terephalate resin containing Glass Bead, PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | |
Solvay TECHNYL® A 205F PA66, DRY Description: TECHNYL ® A 205F is an unreinforced polyamide 66 for injection molding. It is available in natural color.Benefits: The product offers two main advantages: excellent filling qualities.. |
|||
Linear Mold Shrinkage, Transverse | 0.019 - 0.023 cm/cm | 0.019 - 0.023 in/in | ISO DIS 294-4 |
Wellman Wellamid® XT1482-BK High Impact Nylon 66 Description: High Impact Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Crastin® CE2055 BK580 Polybutylene Terephthalate (PBT) Unreinforced Low Viscosity Polybutylene Terephthalate Crastin CE2055 is an unreinforced low viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performanc.. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® 127UV NC010 Acetal (POM)
(Unverified Data**) UV Stabilized High Viscosity Acetal HomopolymerDelrin 127UV is a high viscosity acetal homopolymer with UV stabilizers developed for automotive interior applications. It has improvements in UV aging.. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® 527UV NC010 Acetal (POM)
(Unverified Data**) UV Stabilized Medium Viscosity Acetal HomopolymerDelrin 527UV NC010 is a medium viscosity acetal homopolymer resin with UV stabilizers developed for automotive interior applications. It has improvem.. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® 527UVE NC010 Acetal (POM)
(Unverified Data**) UV Stabilized Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 527UVE NC010 (formerly DE20556) is a medium viscosity acetal homopolymer with UV stabilizers with very low VOC emissi.. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® FG900P NC010 Acetal (POM)
(Unverified Data**) Low Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG900P is a low viscosity acetal homopolymer with improved thermal stability. It has been developed for consideration .. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Hytrel® HTR4275 BK316 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Hytrel HTR4275 BK316 is designed for blow molding or processing techniques requiring high me.. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Hytrel® RS R4275 BK316 Polyester Elastomer TPC-ET 55 Shore D Renewably Sourced High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | ISO 294-4 |
Azoty Tarnow™ Tarnamid® T-27 MCS I Polyamide 6 - Impact Modified High impact resistance grade. Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:H.. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | 60x60x2mm; ISO 294 |
BASF Ultradur B 2550 PBT Ultradur B2550 is an unfilled, very free-flowing grade for coating paper and board with high heat resistance, for example for packaging of frozen goods and ready-prepared meals. Also suitable for in.. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | ISO 2577 |
BASF Ultradur® B 4520 High Speed PBT Description: Very easy flowing unreinforced injection molding grade with enhanced elongation for thin-walled parts (e.g. automotive connectors, switches, relay parts)Information provided by BASF |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | 60x60x2mm; ISO 294 |
BASF Ultradur B 4500 PBT Ultradur B4500 is a general-purpose injection molding grade for high-precision, high-toughness, and dimensionally stable engineering parts. It conforms to FDA requirements of 21 CFR 177.1660. |
|||
Linear Mold Shrinkage, Transverse | 0.019 - 0.021 cm/cm | 0.019 - 0.021 in/in | ASTM D955 |
Solvay Specialty Polymers Amodel® AT-1001L Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1001L is an unreinforced, impact modified polyphthalamide (PPA) resin that exhibits exceptional impact strength at temperatures ranging from room temperature to as low as -40°F (-40°C), .. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm @Thickness 2.00 mm |
0.019 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Crastin® CE2055 BK580 PBT
(Unverified Data**) Crastin® CE2055 is an unreinforced, low viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm | 0.019 in/in | Rhodia EP test |
Solvay Technyl® A 402 H1 Nylon 66 Unreinforced, very high viscosity, heat stabilized, for extrusion and injection molding. TECHNYL® A 402 H1 offers three main advantages: high impact resistance at low humidity levels, good rigidit.. |
|||
Linear Mold Shrinkage, Transverse | 0.019 - 0.023 cm/cm | 0.019 - 0.023 in/in | DIS 294-4 |
Wellman Wellamid® 22L-NBK1/WE-1434 Nylon 66, Engineering Grade All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Transverse | 0.019 cm/cm @Thickness 2.00 mm |
0.019 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Delrin® 527UVE NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 527UVE NC010 (formerly DE20556) is a medium viscosity acetal homopolymer with UV stabilizers having extremely low VOC emissions, developed for automotive interior applications.Information p.. |