Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0090 - 0.012 cm/cm | 0.0090 - 0.012 in/in | ISO 294-4 |
Polyplastic Armlen® PP MF 40-3M Polypropylene Copolymer, 40% Calcium Carbonate Injection moldingInformation provided by PolyPlastic Group. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | ISO Data |
BASF Capron® HPN 9333G HS Impact Modified, 33% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron HPN 9333G HS is a heat stabilized, 33% glass reinforced, impact modified polyamide 6 injection molding compound combining exceptional strength, stiffness and high temperature performance with.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm @Thickness 2.00 mm |
0.0090 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
DuPont Performance Polymers Minlon® 10B40HS1 BK061 Nylon 66
(Unverified Data**) Minlon® 10B40HS1 BK061 is a 40% mineral reinforced, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | DAM; ISO 294-4 |
DSM Akulon® K-FHGM35 (Cond.) 40% Glass/Mineral Reinforced, Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | ISO 294-4 |
DSM Akulon® Ultraflow™ K-FG0 Nylon 6-50% Glass Reinforced (European and Asian Grade) (Dry)
(discontinued **)& The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | ISO 294-4, 2577 |
Lanxess Pocan® DP CF 2200 000000 PBT+PC PBT+PC, non-reinforced, injection molding, flame retardant, impact modified, low tendency to warp |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm @Thickness 2.00 mm |
0.0090 in/in @Thickness 0.0787 in |
ASTM D955 |
Lavergne VYPET VNT 245 PET - PBT 45% Glass Reinforced Polyester Vypet VNT 245 is a 45% fiberglass reinforced modified PBT / PET polyester injection molding compound designed for electrical and automotive applications requiring low warp and improved surface finis.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.012 cm/cm | 0.0090 - 0.012 in/in | |
LATI Latilub 66-20T G/20-V1 PA66, 20% Glass Fiber Reinforced, PTFE Filled, Flame Retardant Self-lubricating product based on Polyamide 66 (PA66). PTFE. Glass fibers. UL94 V-1 classified, with brominated flame retardants, PBB/PBDE free.Availability: Africa & Middle East; Asia Pacific; Euro.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.018 cm/cm | 0.0090 - 0.018 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.020 cm/cm @Time 86400 sec |
0.0090 - 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP RC004SXS PA 66 LNP* THERMOCOMP* RC004SXS is a compound based on Nylon 66 containing 20% Carbon Fiber. Added feature of this grade includes: Heat Stabilized, Electrically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.020 cm/cm @Time 86400 sec |
0.0090 - 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP RFB66 PA 66 LNP* THERMOCOMP* RFB66 is a compound based on Nylon 66 resin containing 30% Glass Fiber, 30% Glass Bead. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.010 cm/cm | 0.0090 - 0.010 in/in | mold temp=60°C; SABIC Method |
SABIC Innovative Plastics LNP STAT-KON KD000 Acetal Copolymer LNP* STAT-KON* KD000 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.018 cm/cm | 0.0090 - 0.018 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Valox® IQ357U PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.020 cm/cm @Time 86400 sec |
0.0090 - 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOTUF VF006U Super Tough Nylon LNP* Thermotuf* VF006U is a compound based on Super Tough Nylon containing Glass Fiber. Characteristics of this grade are High Impact. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.013 cm/cm | 0.0090 - 0.013 in/in | ISO DIS 294-4 |
Wellman Wellamid® GF33-66/6 XE-BK167A 33% Glass Filled, Color Matched Ebony Nylon 66/6 Description: Glass Filled, Color Matched Ebony Nylon 66/6Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.011 cm/cm | 0.0090 - 0.011 in/in | ISO DIS 294-4 |
Wellman Wellamid® GFT1628-BK 17% Glass Fiber Reinforced, Impact Modified Nylon 66 Description: Glass Fiber Reinforced, Impact Modified Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | |
Toyobo TS401 PPS, 40% Glass Fiber Reinforced Key Feature: General Purpose Grade - balanced characteristics suitable for a broad range of uses.High performance injection-molding resin created from crystalline polyphenylene sulfide, using a spec.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | |
Toyobo Vylopet® EMC130-01 Glass Reinforced Polyester, Standard Grade Key Feature: Flame retardant V-0 UL-94 classApplications: General and high rigidity componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric stren.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm @Thickness 4.00 mm |
0.0090 in/in @Thickness 0.157 in |
|
CP-Polymer-Technik Wellamid® 6600 CF10 HWCP 10% Carbon Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® XE 4101 black 9225 PA*-GF40 Product description: Grivory XE 4101 is a 40% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partia.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | DAM; ISO 294-4 2577 |
DuPont Performance Polymers Minlon® 11C40 BKB086 Nylon 66
(Unverified Data**) 40% Mineral Reinforced Polyamide 66 Minlon 11C40 BKB086 is a 40% mineral reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | DAM; ISO 294-4 2577 |
DuPont Performance Polymers Zytel® FR70M30V0 BK010 Nylon 66
(Unverified Data**) 30% Mineral Reinforced Flame Retardant Polyamide 66 Zytel FR70M30V0 BK010 is a 30% mineral reinforced flame retardant black polyamide 66 resin for injection molding.Information provided by DuPont Pe.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | Eurotec |
Eurotec® Tecopet® PT70 GR30 NL100 XA20 PET, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | ISO 294-4 |
Azoty Tarnow™ Tarnamid® T-27 CF10 Polyamide 6 10% Carbon Fiber - Antistatic and Electroconductive Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Electroconductive grade based on carbon fiber reinforcement, very high stiffn.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm @Diameter 2.00 mm |
0.0090 in/in @Diameter 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® R530H BK02 Nylon 66, 30% Glass Reinforced, Conditioned Vydyne® R530H BK02 is high-flow, 30% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm @Thickness 2.00 mm |
0.0090 in/in @Thickness 0.0787 in |
ISO 294-4 |
Ascend Performance Materials VYDYNE® R533H Nylon, 33% Glass Reinforced, Conditioned Vydyne® R533H is 33% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties when exposed to anti-free.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm @Diameter 2.00 mm |
0.0090 in/in @Diameter 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® R543H NT Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H NT is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. .. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm @Diameter 2.00 mm |
0.0090 in/in @Diameter 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® R550 Nylon 66, 50% Glass Reinforced, Conditioned Vydyne® R550 is general-purpose, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is also lubricated for improved flow and offers superior surface appearance. G.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | |
Eurotec® Tecodur® PB70 GR45 NL PBT 45% glass fiber reinforced Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 cm/cm @Diameter 2.00 mm |
0.0090 in/in @Diameter 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® R530H Black Nylon 66, 30% Glass Reinforced, Conditioned Vydyne® R530H Black is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. It is specifically designed to maximize the retention of physical properties wh.. |