Wellman Wellamid® GF33-66/6 XE-BK167A 33% Glass Filled, Color Matched Ebony Nylon 66/6

Category Polymer , Thermoplastic , Nylon , Nylon 6/66 , Nylon 66/6, 30% Glass Fiber Reinforced
Manufacturer Wellman Engineering Resins
Trade Name Wellamid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wellman Wellamid® GF33-66/6 XE-BK167A 33% Glass Filled, Color Matched Ebony Nylon 66/6.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Glass Filled, Color Matched Ebony Nylon 66/6Information provided by Wellman.
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
ISO 1183-87
Filler Content 33 %
33 %
Linear Mold Shrinkage, Flow 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
ISO DIS 294-4
Linear Mold Shrinkage, Transverse 0.0090 - 0.013 cm/cm
0.0090 - 0.013 in/in
ISO DIS 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 145 MPa
21000 psi
ISO 527-93
Elongation at Break 2.0 %
2.0 %
ISO 527-93
Flexural Strength 200 MPa
29000 psi
ISO 178-93
Flexural Modulus 9.40 GPa
1360 ksi
ISO 178-93
Izod Impact, Notched (ISO) 6.20 kJ/m²
2.95 ft-lb/in²
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 230 °C
446 °F
ISO 75-93