Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0050 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0050 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® BFL2015 PC Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0050 cm/cm @Thickness 3.18 mm |
0.0020 - 0.0050 in/in @Thickness 0.125 in |
ASTM D955 |
PolyOne Edgetek® PC-30GF/000 BLACK Polycarbonate (PC) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0050 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0050 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® 3262R PC (Asia Pacific) Lexan* 3262R Polycarbonate (PC) resin is a 20% glass fiber filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant GF-PC has an UL-94 V2@1.5mm rating and is available .. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0050 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0050 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® 3412ECR PC (Europe-Africa-Middle East) Lexan* 3412ECR Polycarbonate (PC) resin is a 20% glass fiber filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant GF-PC has an UL-94 V0 rating and is available in v.. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 cm/cm | 0.0020 in/in | LATI |
LATI LASTANE 50 G/40 40% Glass Fiber Reinforced Polyurethane (PUR)
(discontinued **) Description: Lastane thermoplastics are polyurethane (PUR) products. They exhibit good wear and impact resistance, even at low temperatures, noise inertness and excellent mould release. These proper.. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0040 cm/cm | 0.0020 - 0.0040 in/in | |
Idemitsu Kosan Xarec® WA 214LG SPS, 40% Glass Filled Crystalline Polymer, Glass Filled |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0035 cm/cm | 0.0020 - 0.0035 in/in | |
LATI Lastil G/25-V0 SAN, 25% Glass Fiber Reinforced, Flame Retardant Styrene-Acrylonitrile copolymer (SAN) based compound. Glass fibers. UL94 V-0 classified, with brominated flame retardants. Very high dimensional stability.Availability: Africa & Middle East; Asia Pa.. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0040 cm/cm | 0.0020 - 0.0040 in/in | 60x60x2; 290°C / MT 80°C; 600 bar; ISO 294-4 |
Lanxess Durethan® ECO BV 35 H2 900500 Nylon 6, 35% Glass Fiber PA 6, 35% glass fibers, injection molding, heat-ageing stabilized, contains 30% pre-consumer recycled materialInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 cm/cm | 0.0020 in/in | Post-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4 |
Lanxess Durethan® TP 142-011 900116 Nylon 6 PA 6, non-reinforced, extrusion, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0060 cm/cm | 0.0020 - 0.0060 in/in | |
LATI Latigea B01 I8 Bio-Polymer Bio-Polymer (PLA, PHB, ...). Unfilled. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p... |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics ULTEM 2300 PEI 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. NSF 51 listing, WRAS certification, KTW certification in recognized colors. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Ultem 2412EPR PEI 40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Am.. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Ultem 2412EPR PEI (Asia Pacific) 40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the As.. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0040 cm/cm @Time 86400 sec |
0.0020 - 0.0040 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Stat-kon TE002 LNP* Stat-kon* TE002 is a compound based on Polyurethane resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the A.. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0050 cm/cm @Time 86400 sec |
0.0020 - 0.0050 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP CX05470 PS LNP* THERMOCOMP* CX05470 is a compound based on Polystyrene resin containing 20% Glass Fiber. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0040 cm/cm @Time 86400 sec |
0.0020 - 0.0040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP DC006 PC (Asia Pacific) LNP THERMOCOMP* DC006 is a compound based on Polycarbonate resin containing Carbon Fiber.This product is also known as Thermocomp* DC-1006. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0050 cm/cm @Time 86400 sec |
0.0020 - 0.0050 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Thermocomp OC008A PPS - Branched LNP* Thermocomp* OC008A is a compound based on Branched Polyphenylene Sulfide containing Carbon Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0050 cm/cm | 0.0020 - 0.0050 in/in | ISO 294-4 |
Styron CALIBREâ„¢ 7101-15 Polycarbonate CALIBREâ„¢ 7101-15 glass-reinforced resin offers increased modulus and improved heat distortion resistance, with minimal shrinkage. It also offers outstanding UL-94 flammability ratings. CALIBR.. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0050 cm/cm | 0.0020 - 0.0050 in/in | ISO 294-4 |
Styron CALIBREâ„¢ 7102-15 Polycarbonate CALIBREâ„¢ 7102-15 glass-reinforced resin offers increased modulus and improved heat distortion resistance, with minimal shrinkage. It also offers outstanding UL-94 flammability ratings. CALIBR.. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0050 cm/cm | 0.0020 - 0.0050 in/in | ISO 294-4 |
Styron CALIBREâ„¢ 7102-8 Polycarbonate CALIBREâ„¢ 7102-8 glass-reinforced resin offers increased modulus and improved heat distortion resistance, with minimal shrinkage. It also offers outstanding UL-94 flammability ratings. CALIBRE.. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0050 cm/cm | 0.0020 - 0.0050 in/in | ISO 294-4 |
Styron CALIBREâ„¢ 7103-15 Polycarbonate CALIBREâ„¢ 7103-15 glass-reinforced resin offers increased modulus and improved heat distortion resistance, with minimal shrinkage. It also offers outstanding UL-94 flammability ratings. CALIBR.. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0050 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0050 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GFN1630V PPE+HIPS (Asia Pacific) Noryl* GFN1630V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en.. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL EM7430 PPE+PS 30% glass reinforced, high flow PPO. Automotive. Energy management material. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0050 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0050 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GFN1630V PPE+HIPS (Europe-Africa-Middle East) Noryl* GFN1630V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en.. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 cm/cm | 0.0020 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® GVX-6 H black 9915 PA*-GF60 Product description: Grivory GVX-6H black 9915 is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyam.. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 cm/cm | 0.0020 in/in | |
E-Polymers SEPAZ® LA60 PA66 LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 cm/cm | 0.0020 in/in | LATI |
LATI LASTIROL TR G/10-V1 ES 10% Glass Fiber Polystyrene (PS) Structural Foam Resin (UL94 V-1)
(discontinued * Description: Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass f.. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0050 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0050 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® 3412ECR PC (Asia Pacific) Lexan* 3412ECR Polycarbonate (PC) resin is a 20% glass fiber filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant GF-PC has an UL-94 V0 rating and is available in v.. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 cm/cm @Time 86400 sec |
0.0020 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP VERTON UX06451 BK8-312 PPA (Asia Pacific) LNP* Verton* UX06451 BK8-312 is a compound based on Polyphthalamide resin containing Long Glass Fiber. |