Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.00100 - 0.0100 cm/cm | 0.00100 - 0.0100 in/in | Average value: 0.00566 cm/cm Grade Count:33 |
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi.. |
|||
Linear Mold Shrinkage, Transverse | 0.00300 - 0.0100 cm/cm | 0.00300 - 0.0100 in/in | Average value: 0.00804 cm/cm Grade Count:5 |
Overview of materials for Polyphthalamide (PPA), Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber". Each property range of values reported is minimum and maximum values of .. |
|||
Linear Mold Shrinkage, Transverse | 0.000900 - 0.0100 cm/cm | 0.000900 - 0.0100 in/in | Average value: 0.00647 cm/cm Grade Count:3 |
Overview of materials for Polystyrene + Polyphenylene Ether, Glass + Mineral Filler This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass + Mineral Filler". Each property range of values reported is mi.. |
|||
Linear Mold Shrinkage, Transverse | 0.00550 - 0.0100 cm/cm | 0.00550 - 0.0100 in/in | Average value: 0.00700 cm/cm Grade Count:5 |
Overview of materials for Polyphenylene Ether, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Molded". Each property range of values reported is minimum and maximum values of ap.. |
|||
Linear Mold Shrinkage, Transverse | 0.00300 - 0.0100 cm/cm | 0.00300 - 0.0100 in/in | Average value: 0.00668 cm/cm Grade Count:19 |
Overview of materials for Polycarbonate, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of.. |
|||
Linear Mold Shrinkage, Transverse | 0.00500 - 0.0100 cm/cm | 0.00500 - 0.0100 in/in | Average value: 0.00727 cm/cm Grade Count:22 |
Overview of materials for Polycarbonate, UV Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, UV Stabilized". Each property range of values reported is minimum and maximum values of a.. |
|||
Linear Mold Shrinkage, Transverse | 0.00300 - 0.0100 cm/cm | 0.00300 - 0.0100 in/in | Average value: 0.00600 cm/cm Grade Count:47 |
Overview of materials for Polycarbonate/PET Polyester Blend This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values.. |
|||
Linear Mold Shrinkage, Transverse | 0.00200 - 0.0100 cm/cm | 0.00200 - 0.0100 in/in | Average value: 0.00740 cm/cm Grade Count:20 |
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum .. |
|||
Linear Mold Shrinkage, Transverse | 0.00400 - 0.0100 cm/cm | 0.00400 - 0.0100 in/in | Average value: 0.00650 cm/cm Grade Count:4 |
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler". Specific grades with glass content between 15%.. |
|||
Linear Mold Shrinkage, Transverse | 0.00150 - 0.0100 cm/cm | 0.00150 - 0.0100 in/in | Average value: 0.00438 cm/cm Grade Count:41 |
Overview of materials for Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled". Each property range of values reported is mini.. |
|||
Linear Mold Shrinkage, Transverse | 0.00750 - 0.0100 cm/cm | 0.00750 - 0.0100 in/in | Average value: 0.00860 cm/cm Grade Count:4 |
Overview of materials for Nylon 6, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are includ.. |
|||
Linear Mold Shrinkage, Transverse | 0.00190 - 0.0100 cm/cm | 0.00190 - 0.0100 in/in | Average value: 0.00715 cm/cm Grade Count:10 |
Overview of materials for Nylon 66/6, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are incl.. |
|||
Linear Mold Shrinkage, Transverse | 0.00100 - 0.0100 cm/cm | 0.00100 - 0.0100 in/in | Average value: 0.00425 cm/cm Grade Count:19 |
Overview of materials for Nylon 12, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. .. |
|||
Linear Mold Shrinkage, Transverse | 0.00100 - 0.0100 cm/cm @Temperature 150 - 150 °C |
0.00100 - 0.0100 in/in @Temperature 302 - 302 °F |
Average value: 0.00500 cm/cm Grade Count:17 |
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m.. |
|||
Linear Mold Shrinkage, Transverse | 0.00100 - 0.0100 cm/cm @Time 900 - 900 sec |
0.00100 - 0.0100 in/in @Time 0.250 - 0.250 hour |
Average value: 0.00500 cm/cm Grade Count:17 |
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m.. |
|||
Linear Mold Shrinkage, Transverse | 0.00500 - 0.0100 cm/cm | 0.00500 - 0.0100 in/in | Average value: 0.00768 cm/cm Grade Count:11 |
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 50% Glass Reinforced". Specific grades with glass content between 45% .. |
|||
Linear Mold Shrinkage, Transverse | 0.00530 - 0.0100 cm/cm | 0.00530 - 0.0100 in/in | Average value: 0.00804 cm/cm Grade Count:19 |
Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass/Mineral Reinforced". Each property range of values reported is m.. |
|||
Linear Mold Shrinkage, Transverse | 0.00800 - 0.0100 cm/cm @Temperature 80.0 - 80.0 °C |
0.00800 - 0.0100 in/in @Temperature 176 - 176 °F |
Average value: 0.00867 cm/cm Grade Count:3 |
Overview of materials for Nylon 6, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Glass Fiber Filled".Specific grades with glass content between 15% and 24% are included. Ea.. |