Polymer Property : Linear Mold Shrinkage, Transverse = 0.00500 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.00500 - 0.0150 cm/cm
0.00500 - 0.0150 in/in
Average value: 0.00940 cm/cm Grade Count:10
Overview of materials for Polyaryletherketone (PAEK), Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Glass Fiber Filled". Each property range of values reported is minimum and m..
Linear Mold Shrinkage, Transverse 0.00500 - 0.00800 cm/cm
0.00500 - 0.00800 in/in
Average value: 0.00641 cm/cm Grade Count:22
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max..
Linear Mold Shrinkage, Transverse 0.00500 - 0.0100 cm/cm
0.00500 - 0.0100 in/in
Average value: 0.00727 cm/cm Grade Count:22
Overview of materials for Polycarbonate, UV Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, UV Stabilized". Each property range of values reported is minimum and maximum values of a..
Linear Mold Shrinkage, Transverse 0.00500 - 0.00600 cm/cm
0.00500 - 0.00600 in/in
Average value: 0.00550 cm/cm Grade Count:4
Overview of materials for Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced". Each property range of values repor..
Linear Mold Shrinkage, Transverse 0.00500 - 0.00950 cm/cm
0.00500 - 0.00950 in/in
Average value: 0.00752 cm/cm Grade Count:11
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler". Specific grades with glass content between 25%..
Linear Mold Shrinkage, Transverse 0.00500 - 0.0130 cm/cm
0.00500 - 0.0130 in/in
Average value: 0.00821 cm/cm Grade Count:37
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl..
Linear Mold Shrinkage, Transverse 0.00500 - 0.0240 cm/cm
0.00500 - 0.0240 in/in
Average value: 0.0171 cm/cm Grade Count:8
Overview of materials for Nylon 66, Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of ..
Linear Mold Shrinkage, Transverse 0.00500 - 0.100 cm/cm
0.00500 - 0.100 in/in
Average value: 0.0118 cm/cm Grade Count:62
Overview of materials for Nylon 6, Heat Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro..
Linear Mold Shrinkage, Transverse 0.00500 - 0.0105 cm/cm
0.00500 - 0.0105 in/in
Average value: 0.00819 cm/cm Grade Count:12
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% ..
Linear Mold Shrinkage, Transverse 0.00500 - 0.0165 cm/cm
0.00500 - 0.0165 in/in
Average value: 0.00972 cm/cm Grade Count:9
Overview of materials for Polypropylene with 40% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are i..
Linear Mold Shrinkage, Transverse 0.00500 - 0.0250 cm/cm
0.00500 - 0.0250 in/in
Average value: 0.0145 cm/cm Grade Count:34
Overview of materials for Polypropylene Copolymer
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Copolymer". Each property range of values reported is minimum and maximum values of approp..
Linear Mold Shrinkage, Transverse 0.00500 - 0.0220 cm/cm
0.00500 - 0.0220 in/in
Average value: 0.00916 cm/cm Grade Count:9
Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified". Each property range of values reported..
Linear Mold Shrinkage, Transverse 0.00500 - 0.0170 cm/cm
0.00500 - 0.0170 in/in
Average value: 0.0113 cm/cm Grade Count:11
Overview of materials for Polytrimethylene Terephthalate (PTT)
This property data is a summary of similar materials in the MatWeb database for the category "Polytrimethylene Terephthalate (PTT)". Each property range of values reported is minimum and maximum val..