Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.00400 - 0.0220 cm/cm
0.00400 - 0.0220 in/in
Average value: 0.0130 cm/cm Grade Count:44
Overview of materials for Polyester Thermoplastic Elastomer
This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values..
Linear Mold Shrinkage, Transverse 0.00400 - 0.00900 cm/cm
0.00400 - 0.00900 in/in
Average value: 0.00550 cm/cm Grade Count:7
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is ..
Linear Mold Shrinkage, Transverse 0.00400 - 0.00800 cm/cm
0.00400 - 0.00800 in/in
Average value: 0.00695 cm/cm Grade Count:5
Overview of materials for Polycarbonate, Stainless Steel Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Stainless Steel Fiber". Each property range of values reported is minimum and maximum val..
Linear Mold Shrinkage, Transverse 0.00400 - 0.00900 cm/cm
0.00400 - 0.00900 in/in
Average value: 0.00654 cm/cm Grade Count:13
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m..
Linear Mold Shrinkage, Transverse 0.00400 - 0.00750 cm/cm
0.00400 - 0.00750 in/in
Average value: 0.00593 cm/cm Grade Count:7
Overview of materials for Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled". Each property range of values reported is minimum..
Linear Mold Shrinkage, Transverse 0.00400 - 0.0189 cm/cm
0.00400 - 0.0189 in/in
Average value: 0.00895 cm/cm Grade Count:28
Overview of materials for Nylon 6, 30% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are includ..
Linear Mold Shrinkage, Transverse 0.00400 - 0.0180 cm/cm
0.00400 - 0.0180 in/in
Average value: 0.0120 cm/cm Grade Count:9
Overview of materials for Nylon 66, Stainless Steel Filled; EMI Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Stainless Steel Filled; EMI Grade". Each property range of values reported is minimum and maxi..
Linear Mold Shrinkage, Transverse 0.00400 - 0.0150 cm/cm
0.00400 - 0.0150 in/in
Average value: 0.00756 cm/cm Grade Count:16
Overview of materials for Polycarbonate, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, PTFE Filled". Each property range of values reported is minimum and maximum values of app..
Linear Mold Shrinkage, Transverse 0.00400 - 0.00800 cm/cm
0.00400 - 0.00800 in/in
Average value: 0.00550 cm/cm Grade Count:4
Overview of materials for Polyphenylene Ether, 30% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 30% Glass Filled". Specific grades with glass content between 25% and 34% are inclu..
Linear Mold Shrinkage, Transverse 0.00400 - 0.00800 cm/cm
0.00400 - 0.00800 in/in
Average value: 0.00583 cm/cm Grade Count:3
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Plating Grade
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Plating Grade". Each property range of values reported is minimum..
Linear Mold Shrinkage, Transverse 0.00400 - 0.0110 cm/cm
0.00400 - 0.0110 in/in
Average value: 0.00555 cm/cm Grade Count:47
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a..
Linear Mold Shrinkage, Transverse 0.00400 - 0.0206 cm/cm
0.00400 - 0.0206 in/in
Average value: 0.0109 cm/cm Grade Count:17
Overview of materials for Polypropylene with 20% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are i..