Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.021 cm/cm | 0.021 in/in | Annealed; ISO 294-4 |
DuPont Performance Polymers Crastin® 6130 NC010 PBT
(Unverified Data**) Crastin® 6130 NC010 is an unreinforced, medium high viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Transverse | 0.021 cm/cm | 0.021 in/in | Annealed; ISO 294-4 |
DuPont Performance Polymers Crastin® S600F20 NC010 PBT
(Unverified Data**) Crastin® S600F20 NC010 is an unreinforced, lubricated, medium viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Transverse | 0.021 cm/cm | 0.021 in/in | STN 64 0808 |
Plastcom SLOVALEN PH 49 GF 10 Polypropylene Homopolymer, 10% Glass Fiber FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 10% glass fiber, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP.. |
|||
Linear Mold Shrinkage, Transverse | 0.021 - 0.022 cm/cm | 0.021 - 0.022 in/in | ASTM D955 |
PolyOne Stat-Tech™ NN-20SS/000 Black Polyamide 66 (Nylon 66) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Linear Mold Shrinkage, Transverse | 0.021 cm/cm | 0.021 in/in | ASTM D955 |
Shell Carilon® DP P1000 Polyketone
(discontinued **) Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON® Thermoplastic Polymer DP P1000 is the first in a family of developmental engineering polyketone resins fr.. |
|||
Linear Mold Shrinkage, Transverse | 0.021 cm/cm | 0.021 in/in | ASTM D955 |
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and better .. |
|||
Linear Mold Shrinkage, Transverse | 0.021 cm/cm | 0.021 in/in | ASTM D955 |
LG Chemical Lupox® HV-1010 General Purpose PBT, Unreinforced, High Viscosity LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Linear Mold Shrinkage, Transverse | 0.021 cm/cm | 0.021 in/in | ASTM D955 |
LG Chemical Lupox® SV-1080 General Purpose PBT, Unreinforced, High Molecular Weight, Extrusion LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Linear Mold Shrinkage, Transverse | 0.021 - 0.024 cm/cm @Time 86400 sec |
0.021 - 0.024 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Lubricomp KX99792 Acetal Copoly (Asia Pacific) LNP* Lubricomp* KX99792 is a compound based on Acetal Copolymer resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the .. |
|||
Linear Mold Shrinkage, Transverse | 0.021 - 0.031 cm/cm @Time 86400 sec |
0.021 - 0.031 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRILOY R2000 PA 66 LNP* LUBRILOY* R2000 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.021 cm/cm | 0.021 in/in | Dry; ASTM D955 |
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA) Amodel® AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and bet.. |
|||
Linear Mold Shrinkage, Transverse | 0.021 cm/cm | 0.021 in/in | ASTM D955 |
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA) Amodel® AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and bet.. |
|||
Linear Mold Shrinkage, Transverse | 0.021 - 0.027 cm/cm @Thickness 3.20 mm |
0.021 - 0.027 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® IQ3001 PBT (Europe-Africa-Middle East) Valox IQ3001 is an unfilled environmentally responsible iQ-PBT resin modified with elastomer. Targeted for flexible hinge applications. |
|||
Linear Mold Shrinkage, Transverse | 0.021 - 0.027 cm/cm @Thickness 3.20 mm |
0.021 - 0.027 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® V3004 PBT (Asia Pacific) Unfilled PBT modified with elastomer. Targeted for flexible hinge, automotive connectors, film applications. |
|||
Linear Mold Shrinkage, Transverse | 0.021 - 0.025 cm/cm | 0.021 - 0.025 in/in | ISO DIS 294-4 |
Wellman Wellamid® 22LH-NBK4 Unfilled Nylon 66 Description: Unfilled Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.021 cm/cm | 0.021 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Hytrel® HTR8730 BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 63 Shore D High Viscosity Polyester Elastomer with Excellent Mechanical Properties at Elevated Temperatures Developed for Blow MoldingInformation provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Transverse | 0.021 cm/cm | 0.021 in/in | ISO Data |
BASF Ultraform H 2320 006 Q600 POM Ultraform H2320 006 is a high-molecular-weight grade of POM for injection molding. It conforms to FDA requirements of 21 CFR 177.2470. |
|||
Linear Mold Shrinkage, Transverse | 0.021 cm/cm | 0.021 in/in | ISO Data |
BASF Ultraform N 2320 U03 UNC Q600 POM Ultraform N2320 U03 UNC Q600 is a rapidly freezing UV stabilized general-purpose injection molding grade. |
|||
Linear Mold Shrinkage, Transverse | 0.021 cm/cm | 0.021 in/in | ISO 2577 |
BASF Ultraform® N2520 L POM Description: Is a POM, product having reduced electric surface resistance.Information provided by BASF |
|||
Linear Mold Shrinkage, Transverse | 0.021 cm/cm | 0.021 in/in | ISO 2577 |
BASF Ultraform® N2770 K POM Description: Is a POM, injection-molding grade with improved wear characteristics for sliding elements.Information provided by BASF |
|||
Linear Mold Shrinkage, Transverse | 0.021 cm/cm | 0.021 in/in | ISO 2527 |
BASF Ultraform® W2320 003 PRO POM Description: Is a POM, is a very easy flowing grade for thin-walled components with long flow paths.Information provided by BASF |
|||
Linear Mold Shrinkage, Transverse | 0.021 cm/cm | 0.021 in/in | ISO 2577 |
BASF Ultraform® Z2320 003 POM Description: Is a POM, rapidly solidifying grade for applications with exceptional demands on flowability.Information provided by BASF |
|||
Linear Mold Shrinkage, Transverse | 0.021 cm/cm | 0.021 in/in | ISO 294-4 |
Azoty Tarnow™ Tarnamid® T-27 MCS HI Polyamide 6 - Impact Modified Very high impact resistance, cold impact grade (to -40°C). Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has t.. |
|||
Linear Mold Shrinkage, Transverse | 0.021 cm/cm | 0.021 in/in | ISO 2577 |
BASF Ultraform® S2320 003 POM Description: Easy flowing and rapidly freezing grade for injection molding difficult, thin-walled part.Information provided by BASF |
|||
Linear Mold Shrinkage, Transverse | 0.021 cm/cm | 0.021 in/in | ISO 2577 |
BASF Ultraform® S2320 003 PRO POM Description: Is a POM, is a standard flowing and rapidly freezing grade suitable for standard functional applications.Information provided by BASF |
|||
Linear Mold Shrinkage, Transverse | 0.021 cm/cm | 0.021 in/in | |
Plastcom SLOVALEN PH 91 GF 10 PP, 10% glass fibre FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 10% glass fibre. Increased strength in comparison with unfilled PP. Applied in all industry branches. Increased str.. |
|||
Linear Mold Shrinkage, Transverse | 0.021 cm/cm @Diameter 2.00 mm |
0.021 in/in @Diameter 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 66Z Nylon 66, Conditioned Vydyne® 66Z is a high-viscosity PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66Z resin offers high strength, rigidity and toug.. |
|||
Linear Mold Shrinkage, Transverse | 0.021 cm/cm @Diameter 2.00 mm |
0.021 in/in @Diameter 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 66Z Nylon 66, DAM Vydyne® 66Z is a high-viscosity PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66Z resin offers high strength, rigidity and toug.. |