Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.020 cm/cm @Thickness 2.00 mm |
0.020 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Hytrel® HTR8441 BK316 TPC-ET
(Unverified Data**) Hytrel® HTR8441 is a 55 nom. Shore D thermoplastic polyester elastomer for blow molding. It provides good mechanical properties at high temperature.Information provided by DuPont Performance Polyme.. |
|||
Linear Mold Shrinkage, Transverse | 0.020 cm/cm | 0.020 in/in | LATI |
LATI LATAN 13 Medium Viscosity Polyoxymethylene Copolymer (POM)
(Unverified Data**) Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea.. |
|||
Linear Mold Shrinkage, Transverse | 0.020 cm/cm | 0.020 in/in | LATI |
LATI LATILUB 73/13-01M Polyoxymethylene Base (POM), 1% Molybdenum Disulfide Self Lubricating Plastic
(Unv Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri.. |
|||
Linear Mold Shrinkage, Transverse | 0.020 cm/cm | 0.020 in/in | ISO 294-4 |
Aardvark Polymers AARTEL® 100 D/S Rotational Molding Resin Aartel 100SD is a new conductive grade developed to dissipate electricity in fuel handling systems. Aartel 100SD maintains all o the excellent properties of our general purpose acetal, has a volume .. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.0225 cm/cm | 0.020 - 0.0225 in/in | |
LATI Latan 23UV POM Polyoxymethylene (POM). UV stabilized. Low viscosity. Very good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by .. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.040 cm/cm @Time 86400 sec |
0.020 - 0.040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP KL004L Acetal Copoly (Asia Pacific) LNP* Lubricomp* KL004L is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.021 cm/cm @Time 86400 sec |
0.020 - 0.021 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP RAL23 PA 66 LNP LUBRICOMP* RAL23 is a compound based on Nylon 66 resin containing 15% PTFE, 10% Aramid Fiber. Added features of this material include: Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.050 cm/cm @Time 86400 sec |
0.020 - 0.050 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP VN001 Super Tough Nylon LNP* LUBRICOMP* VN001 is a compound based on Super Tough Nylon containing 2% MOS2. Added feature of th is grade is: Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.040 cm/cm @Time 86400 sec |
0.020 - 0.040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP WL002 PBT LNP* LUBRICOMP WL002 is a compound based on PBT resin containing 10% PTFE. Added feature of this grade is: Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.022 cm/cm @Thickness 3.20 mm |
0.020 - 0.022 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® 309 PBT PBT, For compounding only. Not intended for Injection Molding. Melt viscosity: 250C at 21.6 kgf is 3500-4500. Available in Natural (1001) only. |
|||
Linear Mold Shrinkage, Transverse | 0.020 cm/cm @Time 86400 sec |
0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP KF004A Acetal Homopolymer LNP THERMOCOMP* KF004A is a compound based on Acetal Homopolymer resin containing 20% Glass Fiber. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.040 cm/cm @Time 86400 sec |
0.020 - 0.040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP KAL22M Acetal Copolymer LNP LUBRICOMP* KAL22M is a compound based on Acetal Copolymer resin containing 10% PTFE, 10% Aramid. Added features of this material include: Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.040 cm/cm @Time 86400 sec |
0.020 - 0.040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON RD000I PA 66 LNP* STAT-KON* RD000I is a compound based on Nylon 66 resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Linear Mold Shrinkage, Transverse | 0.020 cm/cm | 0.020 in/in | Sim. To ISO 294-4 |
DSM Stanyl® TW341-J PA46 Heat Stabilized, Lubricated |
|||
Linear Mold Shrinkage, Transverse | 0.020 cm/cm | 0.020 in/in | ISO 294-4 |
DSM Stanyl® TW441 Nylon 46 (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing unmatched performance and value across an amazingly broad range of automotive and electronic applications. Stanyl offers:Highest mechanical propertie.. |
|||
Linear Mold Shrinkage, Transverse | 0.020 cm/cm @Thickness 2.00 mm |
0.020 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
DuPont Performance Polymers Zytel® ST801AW BK195 Nylon 66
(Unverified Data**) Zytel® ST801AW BK195 is a Super Tough, weatherable, easy flow and processing friendly, black polyamide 66 resin for injection molding. It offers the best resistance to outdoor exposure.Information.. |
|||
Linear Mold Shrinkage, Transverse | 0.020 cm/cm | 0.020 in/in | ISO 294-4 |
Barlog Plastics KEBAFORM C 130 LS white POM Copolymer unreinforced, laser markable POMInformation provided by BARLOG plastics GmbH. |
|||
Linear Mold Shrinkage, Transverse | 0.020 cm/cm | 0.020 in/in | ISO 294-4 |
Barlog Plastics KEBAFORM C 270.0 POM Copolymer unreinforced POMInformation provided by BARLOG plastics GmbH. |
|||
Linear Mold Shrinkage, Transverse | 0.020 cm/cm | 0.020 in/in | ISO 294-4 |
Barlog Plastics KEBAFORM C 90.0 POM Copolymer unreinforced POMInformation provided by BARLOG plastics GmbH. |
|||
Linear Mold Shrinkage, Transverse | 0.020 cm/cm | 0.020 in/in | ISO 294-4 |
Barlog Plastics KEBAFORM C 901 SO POM Copolymer unreinforced, improved wear and friction POMInformation provided by BARLOG plastics GmbH. |
|||
Linear Mold Shrinkage, Transverse | 0.020 cm/cm @Thickness 2.00 mm |
0.020 in/in @Thickness 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 21SPF Nylon 66, General Purpose, High Productivity, DAM Vydyne® 21SPF is general-purpose PA66 resin. Available in natural, it is designed principally for injection-molding fabrication. This grade offers a well-balanced combination of engineering propert.. |
|||
Linear Mold Shrinkage, Transverse | 0.020 cm/cm @Diameter 2.00 mm |
0.020 in/in @Diameter 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 21SPF BLK Nylon 66, DAM Vydyne® 21SPF BLK is a, general-purpose PA66 resin used for extrusion-compounding. Available in black, it is designed principally for injection-molding fabrication. This grade offers a well-balance.. |
|||
Linear Mold Shrinkage, Transverse | 0.020 cm/cm @Thickness 2.00 mm |
0.020 in/in @Thickness 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 66R Nylon 66, General Purpose, high viscosity, Conditioned Vydyne® 66R is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66R resin offers high strength, .. |
|||
Linear Mold Shrinkage, Transverse | 0.020 cm/cm @Thickness 2.00 mm |
0.020 in/in @Thickness 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 67B Nylon 66, General Purpose, very high viscosity, Conditioned Vydyne® 67B is a very-high-viscosity PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 67B resin offers high strength, rigidity and.. |
|||
Linear Mold Shrinkage, Transverse | 0.020 cm/cm @Thickness 2.00 mm |
0.020 in/in @Thickness 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 67B Nylon 66, General Purpose, very high viscosity, DAM Vydyne® 67B is a very-high-viscosity PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 67B resin offers high strength, rigidity and.. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.040 cm/cm @Time 86400 sec |
0.020 - 0.040 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Thermocomp TX88477 PU LNP* Thermocomp* TX88447 is a compound based on Polyurethane resin containing proprietary fillers.This data was supplied by SABIC-IP for the Americas region. |