Ascend Performance Materials Vydyne® 67B Nylon 66, General Purpose, very high viscosity, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Ascend Performance Materials (formerly Solutia)
Trade Name VYDYNE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ascend Performance Materials Vydyne® 67B Nylon 66, General Purpose, very high viscosity, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Vydyne® 67B is a very-high-viscosity PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 67B resin offers high strength, rigidity and toughness over a broad range of demanding applications and good fluid resistance to a wide variety of chemicals, solvents and oils. Typical Applications/End Uses: Typical uses include packaging films, monofilaments, bristles, rods, tubing, sheet and extruded profiles.Availability:Asia PacificEuropeNorth America Features:Gasoline ResistanceGeneral PurposeGood Chemical ResistanceGood ToughnessHigh Melt StabilityHigh RigidityHigh StrengthHigh Viscosity Oil Resistant
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ISO 1183
Water Absorption 8.5 %
8.5 %
24 hrs; ISO 62
Moisture Absorption at Equilibrium 2.5 %
2.5 %
Equilibrium at 50%rh; ISO 62
Linear Mold Shrinkage 0.022 cm/cm

@Thickness 2.00 mm
0.022 in/in

@Thickness 0.0787 in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.020 cm/cm

@Thickness 2.00 mm
0.020 in/in

@Thickness 0.0787 in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 70.0 MPa
10200 psi
ISO 527
Tensile Strength, Yield 55.0 MPa
7980 psi
ISO 527
Elongation at Break 250 %
250 %
ISO 527
Elongation at Yield 20 %
20 %
ISO 527
Tensile Modulus 1.90 GPa
276 ksi
ISO 527
Flexural Strength 20.0 MPa
2900 psi
ISO 178
Flexural Modulus 0.750 GPa
109 ksi
ISO 178
Izod Impact, Notched (ISO) 30.0 kJ/m²
14.3 ft-lb/in²
ISO 180
6.00 kJ/m²

@Temperature -30.0 °C
2.86 ft-lb/in²

@Temperature -22.0 °F
ISO 180
Charpy Impact Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
ISO 179
Charpy Impact, Notched 0.600 J/cm²

@Temperature -30.0 °C
2.86 ft-lb/in²

@Temperature -22.0 °F
ISO 179
3.00 J/cm²

@Temperature 23.0 °C
14.3 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Descriptive Properties Value Comments
Blown Film Bath Temperature 20-80°C
Chill Roll Temperature (Cast Film) 20-80°C