Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Samsung Cheil Industries Starex® WR-9120 ASA, Unreinforced

Category Polymer , Thermoplastic , ASA Polymer , Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded
Manufacturer Samsung, Cheil Industries
Trade Name Starex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Starex® WR-9120 ASA, Unreinforced.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0040 - 0.0070 in/in

@Thickness 0.126 in
ASTM D955
Melt Flow 17.6 g/10 min

@Load 10.0 kg,
Temperature 220 °C
17.6 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 108
108
ASTM D785
Tensile Strength, Yield 47.1 MPa
6830 psi
5 mm/min; ASTM D638
Elongation at Break 50 %
50 %
5 mm/min; ASTM D638
Flexural Strength 66.7 MPa
9670 psi
2.8 mm/min; ASTM D638
Flexural Modulus 2.16 GPa
313 ksi
2.8 mm/min; ASTM D638
Izod Impact, Notched 1.96 J/cm

@Thickness 3.17 mm
3.67 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 83.0 °C

@Thickness 6.40 mm
181 °F

@Thickness 0.252 in
ASTM D648
Vicat Softening Point 96.0 °C
205 °F
B/50; ISO R306
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in