Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.85 - 1.90 g/cc | 1.85 - 1.90 g/cc | |
Premix Premi-Glas® 2207-20 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2207-20 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f.. |
|||
Specific Gravity | 1.85 - 1.90 g/cc | 1.85 - 1.90 g/cc | |
Premix Premi-Glas® 2207-22 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2207-22 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f.. |
|||
Specific Gravity | 1.80 - 1.90 g/cc | 1.80 - 1.90 g/cc | ISO 1183 |
Raschig Group MELOPAS® 156 MF Melamine Glass fiber reinforced Melamine molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 200.. |
|||
Specific Gravity | 1.70 - 1.90 g/cc | 1.70 - 1.90 g/cc | ISO 1183 |
Raschig Group RALUPOL® 2200 UP Polyester Organically filled polyester molding compound. Low post-shrinkage, good electrical values and mechanical properties, high surface quality and good color stability (non-yellowing). This product meets.. |
|||
Specific Gravity | 1.70 - 1.90 g/cc | 1.70 - 1.90 g/cc | ASTM D792 |
Mar-Bal MB1000-25 Thermoset Polyester Composite Molding Compound A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro.. |
|||
Specific Gravity | 1.80 - 1.90 g/cc | 1.80 - 1.90 g/cc | ASTM D792 |
Mar-Bal MB2000-10 Thermoset Polyester Composite Molding Compound An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can.. |
|||
Specific Gravity | 1.70 - 1.90 g/cc | 1.70 - 1.90 g/cc | ASTM D792 |
Mar-Bal MB4000 Thermoset Polyester Composite Molding Compound The high track resistant material. A flame retardant polyester molding compound with moderate strength and excellent electrical properties and exceptional arc and track resistance. Suitable for repl.. |
|||
Specific Gravity | 1.80 - 1.90 g/cc @Thickness 1.57 mm |
1.80 - 1.90 g/cc @Thickness 0.0620 in |
ASTM D792 |
Industrial Laminates/Norplex NP509 Glass Fabric Description: Woven glass fabric, melamine resin laminate. Very hard, flame resistant, machining grade with excellent electrical properties in high humidity conditions. High physical strength and exc.. |
|||
Specific Gravity | 1.80 - 1.90 g/cc @Thickness 1.57 mm |
1.80 - 1.90 g/cc @Thickness 0.0620 in |
ASTM D792 |
Industrial Laminates/Norplex NP510A Glass Fabric Description: Woven glass fabric epoxy laminate. Engineered to provide NEMA grade FR-4 properties. This material contains bromine on the epoxy resin backbone. Certifiable to MIL-I-24768/27, Type GEE-.. |
|||
Specific Gravity | 1.80 - 1.90 g/cc @Thickness 1.57 mm |
1.80 - 1.90 g/cc @Thickness 0.0620 in |
ASTM D792 |
Industrial Laminates/Norplex NP511 Glass Fabric Description: Woven glass fabric with high temperature epoxy resin. Excellent mechanical strength and electrical properties at elevated temperatures. Continuous operating temperature is 165°C. Mat.. |
|||
Specific Gravity | 1.70 - 1.90 g/cc | 1.70 - 1.90 g/cc | IEC 1212-2 8.1 |
Hippe EP GC 201 Woven Glass Cloth Reinforced Epoxy Resin - Sheet Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity.Information.. |
|||
Specific Gravity | 1.70 - 1.90 g/cc | 1.70 - 1.90 g/cc | IEC 1212-2 8.1 |
Hippe EP GC 202 Woven Glass Cloth Reinforced Epoxy Resin - Sheet Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. Flame ret.. |
|||
Specific Gravity | 1.70 - 1.90 g/cc | 1.70 - 1.90 g/cc | IEC 1212-2 8.1 |
Hippe EP GC 205 Woven Glass Cloth Reinforced Epoxy Resin - Sheet Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. High mech.. |
|||
Specific Gravity | 1.70 - 1.90 g/cc | 1.70 - 1.90 g/cc | IEC 1212-2 7.2 |
Hippe EP GC 22 Woven Glass Cloth Reinforced Epoxy Resin - Round, Rolled Tube Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperatures. High mechanical strength at elevated temperatures. Very good stability of .. |
|||
Specific Gravity | 1.70 - 1.90 g/cc | 1.70 - 1.90 g/cc | IEC 1212-2 8.1 |
Hippe EP GM 202 Glass Mat Reinforced Epoxy Resin - Sheet |
|||
Specific Gravity | 1.70 - 1.90 g/cc | 1.70 - 1.90 g/cc | IEC 1212-2 7.2 |
Hippe MF GC 21 Woven Glass Cloth Reinforced Melamine Resin - Round, Rolled Tube Used in mechanical and electrical applications. High mechanical strength. Good arc and tracking resistance. Information provided by Hippe. |
|||
Specific Gravity | 1.60 - 1.90 g/cc | 1.60 - 1.90 g/cc | IEC 1212-2 8.1 |
Hippe SI GC 201 Woven Glass Cloth Reinforced Silicone Resin - Sheet Used in electrical and electronic applications. Extremely good electrical properties under dry conditions; good properties under humid conditions.Information provided by Hippe. |
|||
Specific Gravity | 1.60 - 1.90 g/cc | 1.60 - 1.90 g/cc | IEC 1212-2 8.1 |
Hippe SI GC 202 Woven Glass Cloth Reinforced Silicone Resin - Sheet Used in mechanical and electrical applications at elevated temperature. Good heat resistance.Information provided by Hippe. |
|||
Specific Gravity | 1.50 - 1.90 g/cc | 1.50 - 1.90 g/cc | IEC 1212-2 8.1 |
Hippe UP GM 202 Woven Glass Mat Reinforced Polyester (unsaturated) Resin - Sheet Used in mechanical and electrical applications. Good stability of electrical properties under high humidity. Good mechanical properties at moderate temperature. Flame retardant.Information provid.. |
|||
Specific Gravity | 1.50 - 1.90 g/cc | 1.50 - 1.90 g/cc | IEC 1212-2 8.1 |
Hippe UP GM 204 Woven Glass Mat Reinforced Polyester (unsaturated) Resin - Sheet Used in mechanical and electrical applications. Very high mechanical properties at ambient temperatures. Good mechanical properties at elevated temperatures.Information provided by Hippe. |
|||
Specific Gravity | 1.70 - 1.90 g/cc | 1.70 - 1.90 g/cc | IEC 1212-2 8.1 |
Hippe EP GM 203 Glass Mat Reinforced Epoxy Resin - Sheet |
|||
Specific Gravity | 1.80 - 1.90 g/cc | 1.80 - 1.90 g/cc | ASTM D792-66 |
BCC Products Kwik Kast BC 8645 Urethane Casting BCC Kwik Kast/Gray is a two component, fast setting polyurethane reproduction plastic. BC8645 has been reformulated to enhance filler suspension and avoid hard packing @ 77ºF. Uses include; tracing.. |
|||
Specific Gravity | 1.80 - 1.90 g/cc | 1.80 - 1.90 g/cc | ASTM D792-66 |
BCC Products SLO-KAST BC 8009 Urethane Casting Slo-Kast is a low viscosity, medium setting, easy to use casting material. This polyurethane system features extremely low shrinkage when properly cured. Unlike Kwik-Kast, BC 8009 offers the user lo.. |
|||
Specific Gravity | 1.80 - 1.90 g/cc | 1.80 - 1.90 g/cc | |
Bulk Molding Compounds BMC 404 Thermoset Polyester, Low Shrink, High Strength, Electrical Grade BMC 404 is a high strength, low shrink, glass reinforced polyester molding compound that meets Ford Specification ESF-M3D121-A. BMC 404 has excellent electrical properties and creep resistance. It c.. |
|||
Specific Gravity | 1.75 - 1.90 g/cc | 1.75 - 1.90 g/cc | |
Bulk Molding Compounds BMC 850 Corrosion Resistant, Flame Retardant Molding Compound BMC 850 is a high strength, corrosion resistant and flame retardant molding compound. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk form.Typical applications a.. |
|||
Specific Gravity | 1.75 - 1.90 g/cc | 1.75 - 1.90 g/cc | |
Bulk Molding Compounds BMC 880 Medium Strength Molding Compound BMC 880 is a medium strength, low shrink molding compound designed for outdoor applications. This material is UL Listed 94-V0/5V and is UL approved for outdoor use. It can be supplied in bulk or ext.. |
|||
Specific Gravity | 1.80 - 1.90 g/cc | 1.80 - 1.90 g/cc | |
BCC Products Kwik Kast BC 8001 Urethane Casting BC8001 is an advanced fast cast polyurethane tooling system. It features low viscosity, low exotherm and minimal shrinkage. It cures hard, yet more durable resulting in less brittle parts. Designed.. |
|||
Specific Gravity | 1.75 - 1.90 g/cc | 1.75 - 1.90 g/cc | |
Bulk Molding Compounds BMC 851 Corrosion Resistant, Flame Retardant Molding Compound BMC 851is a high strength, corrosion resistant and flame retardant molding compound. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk form.Typical applications ar.. |
|||
Specific Gravity | 1.75 - 1.90 g/cc | 1.75 - 1.90 g/cc | |
Bulk Molding Compounds BMC 900 Thermoset Polyester, Soft Flow Encapsulation Grade BMC 900 is an encapsulation grade, soft flow material. As with all other BMCI compounds, this series can be supplied in logs, slugs or bulk.Typical applications are electrical coil encapsulations an.. |
|||
Specific Gravity | 1.50 - 1.90 g/cc | 1.50 - 1.90 g/cc | IEC 1212-2 8.1 |
Hippe UP GM 203 Woven Glass Mat Reinforced Polyester (unsaturated) Resin - Sheet Used in mechanical and electrical applications. Good stability of electrical properties under high humidity. Good mechanical properties at moderate temperature. Flame retardant. With improved re.. |