Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.95 g/cc | 1.95 g/cc | |
Premix Premi-Glas® 1203-30 Fiberglass Reinforced SMC Description: Premi-Glas® 1203-30 is a fiberglass-reinforced, thermoset sheet molding compound designed for structural and semi-structural components where smooth flat surfaces, high strength and st.. |
|||
Specific Gravity | 1.95 g/cc | 1.95 g/cc | |
Pyrotek Hirolex HG Electrical Insulating Material Hirolex HG has superior mechanical properties. It is highly resistant to thermal shock, non-flammable and offers good arc resistance.Information provided by Pyrotek. |
|||
Specific Gravity | 1.95 - 2.45 g/cc | 1.95 - 2.45 g/cc | ASTM D792 |
Parker Chomerics CHO-BOND® 1016 Electrically Conductive Sealant Description: CHO-BOND 1016 sealant is an electrically conductive, one-component RTV silicone which provides both environmental sealing and EMI shielding. This seal, filled with nickel-plated graphit.. |
|||
Specific Gravity | 1.95 - 2.45 g/cc | 1.95 - 2.45 g/cc | ASTM D792 |
Parker Chomerics CHO-SEAL L6303 Conductive Elastomer Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact.Molded and ExtrudedRoHS CompliantInformation provid.. |
|||
Specific Gravity | 1.95 g/cc | 1.95 g/cc | ASTM D792 |
Quantum Composites QC-8816 66% Glass Fiber Reinforced Polyester Hybrid SMC QC-8816 is a polyester hybrid engineered structural composite molding compound reinforced with continuous, unidirectional (0°) glass fibers. It provides high strength, stiffness and fatigue resist.. |
|||
Specific Gravity | 1.95 - 2.05 g/cc | 1.95 - 2.05 g/cc | ISO 1183 |
Raschig Group 3536 Epoxy Glass-fiber reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. This product meets the allowed.. |
|||
Specific Gravity | 1.95 - 2.15 g/cc | 1.95 - 2.15 g/cc | ISO 1183 |
Raschig Group RALUPOL® 5000 UP Polyester Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, excellent heat resistance, good mechanical strength. This product meets the all.. |
|||
Specific Gravity | 1.95 g/cc | 1.95 g/cc | ASTM D792 |
3M Dyneon™ THV 220A Fluorothermoplastic
(discontinued **) THV 220A is a flexible, transparent fluoroplastic composed of tetrafluoroethylene, hexafluoropropylene, and vinylidene fluoride in the form of agglomerate. It is soluble in ketones, esters, or ether.. |
|||
Specific Gravity | 1.95 g/cc | 1.95 g/cc | ASTM D792 |
3M Dyneon™ THV 220G Fluorothermoplastic
(discontinued **) THV 220G is a flexible, transparent fluoroplastic composed of tetrafluoroethylene, hexafluoropropylene, and vinylidene fluoride in the form of pellets. IT proves a balance of low temperature process.. |
|||
Specific Gravity | 1.95 g/cc | 1.95 g/cc | ASTM D792 |
3M Dyneon™ THV 340C Fluorothermoplastic
(discontinued **) THV 340C is a flexible, transparent fluoroplastic composed of tetrafluoroethylene, hexafluoropropylene, and vinylidene fluoride in the form of concentrated water-based dispersion containing an ionic.. |
|||
Specific Gravity | 1.95 g/cc | 1.95 g/cc | ASTM D792 |
3M Dyneon™ THV 510ESD Fluorothermoplastic
(discontinued **) THV 510ESD is a flexible, fluoroplastic compound composed of tetrafluoroethylene, hexafluoropropylene, and vinylidene fluoride in the form of pellets. It provides a balance of low temperature proces.. |
|||
Specific Gravity | 1.95 g/cc | 1.95 g/cc | ASTM D792 |
LG Chemical LUCON PN9008 PPS+MF+GF Injection Molding Grade, PPS+MF+GF, High Thermal Conductivity, Chemical Resistance, High Heat ResistanceApplication: Electrical or Electronic Parts (Heat sink, LED etc.), Motor HousingsCAS No. 25212.. |
|||
Specific Gravity | 1.95 g/cc | 1.95 g/cc | ASTM D792 |
LG Chemical LUCON PN9009 PPS+MF Injection Molding Grade, PPS+MF, High Thermal Conductivity, Chemical Resistance, High Heat ResistanceApplication: Electrical or Electronic Parts (Heat sink, LED etc.) Motor HousingCAS No. 25212-74-2.. |
|||
Specific Gravity | 1.95 g/cc | 1.95 g/cc | ASTM D297 |
Greene Tweed CHEMRAZ® 504 Perfluoroelastomer Greene Tweeds Chemraz® 504, a 65 Shore A hardness perfluoroelastomer, provides an extremely broad range of chemical resistance and is perfect for services with low pressures and/or low temperatur.. |
|||
Specific Gravity | 1.95 - 2.01 g/cc | 1.95 - 2.01 g/cc | ASTM D 792 |
Karina 10/70-IE White Color Concentrate MBU EVA based color concentrate, with 70% of titanium dioxide, recommended for application in polyolefinic and PVC compounds for general purposes. Minimum recommended usage of 0.5%.Information provided.. |
|||
Specific Gravity | 1.95 - 2.05 g/cc | 1.95 - 2.05 g/cc | ASTM D792 |
Adamas Adalon® 433 PTFE, 10% Ekonol® Information provided by Adamas, HPM |
|||
Specific Gravity | 1.95 - 2.01 g/cc | 1.95 - 2.01 g/cc | |
Bulk Molding Compounds BMC 1603 Multi-purpose grade BMC 1603 is a multi-purpose, moderate strength, low cost material that is suitable for injection, compression and transfer molding. UL® recognized. This material was formerly known as Glastic® 160.. |
|||
Specific Gravity | 1.95 g/cc | 1.95 g/cc | |
Bulk Molding Compounds BMC 600LS Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 600LS molding compound is a low-shrink, Mineral filled, glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is a general purpose materia.. |
|||
Specific Gravity | 1.95 g/cc | 1.95 g/cc | |
Bulk Molding Compounds BMC 605L Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 605L molding compound is a low cost, mineral filled, glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is characterized by good molda.. |
|||
Specific Gravity | 1.95 - 2.01 g/cc | 1.95 - 2.01 g/cc | |
Bulk Molding Compounds BMC SLC 1000 Glass Reinforced Polyester BMC SLC 1000 is a medium strength, low-cost, glass reinforced polyester compound with adjustable shrinkage. It is V-0 flame arc and track resistant. UL® recognized. This material was formerly known.. |
|||
Specific Gravity | 1.95 g/cc | 1.95 g/cc | |
Aremco Aremco-Bond™ 2315 High Performance Epoxide High Temperature, Low Viscosity, Potting Compound for Electrical Applications. |
|||
Specific Gravity | 1.95 - 2.05 g/cc | 1.95 - 2.05 g/cc | |
Bulk Molding Compounds BMC 1050 Thermoset Polyester BMC 1050 is a cosmetic, appliance grade material with superior heat stability. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk.Typical applications are toaster e.. |