Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Dyneon™ THV 220A Fluorothermoplastic  (discontinued **)

Category Polymer , Thermoplastic , Fluoropolymer
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Dyneon™ THV 220A Fluorothermoplastic  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
THV 220A is a flexible, transparent fluoroplastic composed of tetrafluoroethylene, hexafluoropropylene, and vinylidene fluoride in the form of agglomerate. It is soluble in ketones, esters, or ethers and can be used to prepare solutions to coat a range of substrates to provide surfaces with good weatherability and anti-soiling properties. This agglomerate form can also be used for compounding. The THV 200, 300, 400, 500 and 600 series process at relatively low temperatures compared to other fluoroplastic and may not require the same level of corrosion resistant equipment as that used with higher melting fluoroplastic.Information provided by Dyneon, A 3M Company
Physical Properties Metric English Comments
Specific Gravity 1.95 g/cc
1.95 g/cc
ASTM D792
Melt Index of Compound 20 g/10 min

@Load 5.00 kg,
Temperature 265 °C
20 g/10 min

@Load 11.0 lb,
Temperature 509 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 20.0 MPa
2900 psi
ASTM D638
Elongation at Break 600 %
600 %
ASTM D638
Flexural Modulus 0.0800 GPa
11.6 ksi
ASTM D790
Thermal Properties Metric English Comments
Melting Point 120 °C
248 °F
ASTM D4591
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Descriptive Properties Value Comments
Form Agglomerate