Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.70 - 1.80 g/cc | 1.70 - 1.80 g/cc | |
Premix Premi-Glas® 2143-24 CR-SX Fiberglass Reinforced Thick Molding Compound Premi-Glas® 2143-24 CR-SX is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves.. |
|||
Specific Gravity | 1.70 - 1.80 g/cc | 1.70 - 1.80 g/cc | |
Premix Premi-Glas® 2143-24 CR-SX-HT Fiberglass Reinforced Thick Molding Compound Premi-Glas® 2143-24 CR-SX is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves.. |
|||
Specific Gravity | 1.30 - 1.80 g/cc | 1.30 - 1.80 g/cc | ASTM D792 |
Parker Chomerics CHO-SEAL® 2557 Non-Conductive Extruded Elastomer Specifications Description: Chomerics manufactures a dual performance extruded gasket in one simple design. By a seam vulcanization process, CHO-SEAL or CHO-SIL conductive elastomers are extruded in parallel with .. |
|||
Specific Gravity | 1.70 - 1.80 g/cc | 1.70 - 1.80 g/cc | ISO 1183 |
Raschig Group DECAL® 572R Phenolic Glass-fiber reinforced phenolic molding compound. Exceptional heat resistance with regard to maintaining surface finish and mechanical properties, outstanding mechanical properties, excellent rotati.. |
|||
Specific Gravity | 1.75 - 1.80 g/cc | 1.75 - 1.80 g/cc | ASTM D792 |
Solvay Specialty Polymers Solef® 1015 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 1015 PVDF homopolymer has very high viscosity, suitable for membrane manufacturing. It is available exclusively as powder.Information provided by Solvay Specialty Polymers. |
|||
Specific Gravity | 1.75 - 1.80 g/cc | 1.75 - 1.80 g/cc | ASTM D792 |
Solvay Specialty Polymers Solef® 6008 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 6008 PVDF homopolymer is a low-viscosity PVDF resin and is typically processed by injection molding.Information provided by Solvay Specialty Polymers. |
|||
Specific Gravity | 1.75 - 1.80 g/cc | 1.75 - 1.80 g/cc | ASTM D792 |
Solvay Specialty Polymers Solef® 6010 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 6010 PVDF homopolymer has medium viscosity and is typically processed by extrusion.Information provided by Solvay Specialty Polymers. |
|||
Specific Gravity | 1.75 - 1.80 g/cc | 1.75 - 1.80 g/cc | ASTM D792 |
Solvay Specialty Polymers Solef® 6012 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 6012 PVDF homopolymer is a high-viscosity PVDF resin and is typically processed by extrusion or compression molding.Information provided by Solvay Specialty Polymers. |
|||
Specific Gravity | 1.75 - 1.80 g/cc | 1.75 - 1.80 g/cc | ASTM D792 |
Mar-Bal MB2000-20 Thermoset Polyester Composite Molding Compound An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can.. |
|||
Specific Gravity | 1.75 - 1.80 g/cc | 1.75 - 1.80 g/cc | ASTM D792 |
Mar-Bal MB5500 Thermoset Polyester Composite Molding Compound A superior heat resistant material. U.L. RTI rating of 160°C-170°C.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc. |
|||
Specific Gravity | 1.74 - 1.80 g/cc | 1.74 - 1.80 g/cc | ASTM D 792 |
Karina 18/97-RG-GE (CS) Gray Color Concentrate for PVC Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. .. |
|||
Specific Gravity | 1.60 - 1.80 g/cc | 1.60 - 1.80 g/cc | IEC 1212-2 7.2 |
Hippe SI GC 41 Woven Glass Cloth Reinforced Silicone Resin - Round, Molded Tube and Rod Used in mechanical, electrical and electronic applications. Good stability of electrical properties at elevated temperatures.Information provided by Hippe. |
|||
Specific Gravity | 1.50 - 1.80 g/cc | 1.50 - 1.80 g/cc | IEC 1212-2 7.2 |
Hippe EP MP 21 Mica Paper Reinforced Epoxy Resin - Round, Rolled Tube Used in mechanical, electrical and electronic applications. Good stability of electrical properties when exposed to high relative humidity. Good heat resistance.Information provided by Hippe. |
|||
Specific Gravity | 1.76 - 1.80 g/cc | 1.76 - 1.80 g/cc | ASTM D792 |
Arkema Group KYNAR FLEX® 2800-00 Polyvinylidene Fluoride Copolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low.. |
|||
Specific Gravity | 1.77 - 1.80 g/cc | 1.77 - 1.80 g/cc | ASTM D792 |
Arkema Group KYNAR FLEX® 2850 Black Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating, pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness .. |
|||
Specific Gravity | 1.77 - 1.80 g/cc | 1.77 - 1.80 g/cc | ASTM D792 |
Arkema Group KYNAR FLEX® 2850-02 Polyvinylidene Fluoride Copolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |
|||
Specific Gravity | 1.77 - 1.80 g/cc | 1.77 - 1.80 g/cc | ASTM D792 |
Arkema Group KYNAR FLEX® 2850-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |
|||
Specific Gravity | 1.76 - 1.80 g/cc | 1.76 - 1.80 g/cc | ASTM D792 |
Arkema Group KYNAR FLEX® 2900-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness.. |
|||
Specific Gravity | 1.78 - 1.80 g/cc | 1.78 - 1.80 g/cc | ASTM D792 |
Arkema Group KYNAR FLEX® 2950-05 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toug.. |
|||
Specific Gravity | 1.75 - 1.80 g/cc | 1.75 - 1.80 g/cc | |
Bulk Molding Compounds BMC 1608 Very High Strength, Corrosion Resistant BMC 1608 is a very high strength, general purpose, corrosion resistant material. Recommended for compression molding only. UL® recognized. Meets FDA requirements for food contact. This material was.. |
|||
Specific Gravity | 1.76 - 1.80 g/cc | 1.76 - 1.80 g/cc | ASTM D792 |
Adamas Adalon® 451 PTFE, organic filler Information provided by Adamas, HPM |
|||
Specific Gravity | 1.75 - 1.80 g/cc | 1.75 - 1.80 g/cc | ASTM D792 |
Solvay Specialty Polymers Solef® 11010 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 11010 PVDF is a medium-viscosity flexible PVDF copolymer resin and is typically processed by extrusion.Information provided by Solvay Specialty Polymers. |
|||
Specific Gravity | 1.75 - 1.80 g/cc | 1.75 - 1.80 g/cc | ASTM D792 |
Solvay Specialty Polymers Solef® 21510 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 21510 PVDF copolymer has low viscosity and is suitable for solution processing in lithium batteries applications.Information provided by Solvay Specialty Polymers. |
|||
Specific Gravity | 1.75 - 1.80 g/cc | 1.75 - 1.80 g/cc | ASTM D792 |
Solvay Specialty Polymers Solef® 31508 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 31508 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Information provided by Solvay Specialty Polymers. |
|||
Specific Gravity | 1.60 - 1.80 g/cc | 1.60 - 1.80 g/cc | IEC 1212-2 8.1 |
Hippe PF GC 201 Woven Glass Cloth Reinforced Phenolic Resin - Sheet Used in mechanical and electrical applications. High mechanical strength and good electrical properties under normal humidity. Heat resistant. Information provided by Hippe. |
|||
Specific Gravity | 1.50 - 1.80 g/cc | 1.50 - 1.80 g/cc | IEC 1212-2 7.2 |
Hippe PF GC 21 Woven Glass Cloth Reinforced Phenolic Resin - Round, Rolled Tube Used in mechanical, electrical and electronic applications. Very high mechanical strength at moderate temperatures.Information provided by Hippe. |
|||
Specific Gravity | 1.78 - 1.80 g/cc | 1.78 - 1.80 g/cc | ASTM D792 |
Arkema Group KYNAR FLEX® 2750-01 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |
|||
Specific Gravity | 1.76 - 1.80 g/cc | 1.76 - 1.80 g/cc | ASTM D792 |
Arkema Group KYNAR FLEX® 2800-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low.. |
|||
Specific Gravity | 1.77 - 1.80 g/cc | 1.77 - 1.80 g/cc | ASTM D792 |
Arkema Group KYNAR FLEX® 2850-00 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |
|||
Specific Gravity | 1.77 - 1.80 g/cc | 1.77 - 1.80 g/cc | ASTM D792 |
Arkema Group KYNAR FLEX® 2850-07 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |