| Category | Polymer , Thermoplastic , Fluoropolymer , PTFE |
| Manufacturer | Adamas |
| Trade Name | Adalon® |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Adamas Adalon® 451 PTFE, organic filler.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.76 - 1.80 g/cc | 1.76 - 1.80 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 62 - 65 | 62 - 65 | ASTM D2240 |
| Ball Indentation Hardness | 128 - 132 MPa | 18600 - 19100 psi | ISO 2032 |
| Tensile Strength at Break | >= 12.0 MPa | >= 1740 psi | ASTM D4745-97 |
| Elongation at Break | >= 115 % | >= 115 % | ASTM D4745-97 |
| Coefficient of Friction, Dynamic | 0.030 - 0.15 | 0.030 - 0.15 | ASTM D1894 |
| Coefficient of Friction, Static | 0.12 - 0.22 | 0.12 - 0.22 | ASTM D1894 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Thermal Conductivity | 0.190 W/m-K | 1.32 BTU-in/hr-ft²-°F | ASTM C 177 |
| Melting Point | 327 °C | 621 °F | DSC |
| Maximum Service Temperature, Air | 230 °C | 446 °F | DSC |
| Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | DSC |
| Flammability, UL94 | V-0 | V-0 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+18 ohm-cm | 1.00e+18 ohm-cm | ASTM D257 |
| Surface Resistance | 1.00e+16 ohm | 1.00e+16 ohm | ASTM D257 |
| Dielectric Constant | 2.1 @Frequency 60.0 - 2.00e+6 Hz |
2.1 @Frequency 60.0 - 2.00e+6 Hz |
ASTM D150 |
| Dielectric Strength | 20.0 - 70.0 kV/mm | 508 - 1780 kV/in | ASTM D149 |