Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eurostar Starflam RF0023K PA66/6, Glass Fiber Filled, Flame Retardant, Injection Molded

Category Polymer , Thermoplastic , Nylon , Nylon 6/66
Manufacturer Eurostar Engineering Plastics
Trade Name Starflam
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurostar Starflam RF0023K PA66/6, Glass Fiber Filled, Flame Retardant, Injection Molded.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Starflam RF0023K is a Flame Retardant, Halogen Free, Red Phosphorous Free, Glass Reinforced Polyamide 66/6 Injection Molding, Crosslinkable under Beta or Gamma RadiationInformation provided by Eurostar.
Physical Properties Metric English Comments
Density 1.74 g/cc
0.0629 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0030 - 0.0060 cm/cm
0.0030 - 0.0060 in/in
on Tensile Bar; E2P method
Mechanical Properties Metric English Comments
Tensile Strength at Break 90.0 MPa
13100 psi
5 mm/min; ISO 527
Elongation at Break 1.0 - 2.0 %
1.0 - 2.0 %
5 mm/min; ISO 527
Flexural Strength 145 MPa
21000 psi
2 mm/min; ISO 178
Flexural Modulus 10.7 GPa
1550 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
80x10x4; ISO 179/1eA
Izod Impact, Unnotched (ISO) 15.0 kJ/m²
7.14 ft-lb/in²
80x10x4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 203 °C
397 °F
Flatw 80x10x4, sp=64 mm; ISO 75/Af
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
Glow Wire Test 960 °C

@Thickness 1.50 mm
1760 °F

@Thickness 0.0591 in
IEC 60695-2-12
Electrical Properties Metric English Comments
Comparative Tracking Index 600 V
600 V
IEC 60112
Processing Properties Metric English Comments
Zone 1 260 - 280 °C
500 - 536 °F
Zone 2 270 - 280 °C
518 - 536 °F
Zone 3 270 - 290 °C
518 - 554 °F
Melt Temperature 270 - 290 °C
518 - 554 °F
Mold Temperature 60.0 - 90.0 °C
140 - 194 °F