Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.013 - 0.019 cm/cm | 0.013 - 0.019 in/in | ASTM D955 |
PolyOne Dynaflex™ G7950-1 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7950-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Linear Mold Shrinkage, Flow | <= 0.013 cm/cm @Thickness 4.00 mm, Temperature 23.0 °C |
<= 0.013 in/in @Thickness 0.157 in, Temperature 73.4 °F |
Injection Molded, Bergmann Method; No Standard |
PolyOne Edgetek® QT-20MN/000 natural HI Syndiotactic Polystyrene (SPS) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.017 cm/cm | 0.013 - 0.017 in/in | ASTM D955 |
PolyOne Geon™ Vinyl Flexible A9000 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.017 cm/cm | 0.013 - 0.017 in/in | ASTM D955 |
PolyOne Geon™ Vinyl Flexible A90U2 Polyvinyl Chloride, Flexible (PVC, Flexible) GENERAL PURPOSE CLEAR PVC COMPOUND WITH LOW LEVEL OF U.V. INHIBITOR, to be used only in interior applications.Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.017 cm/cm | 0.013 - 0.017 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP FARADEX MX10014 PP (Europe-Africa-Middle East) LNP* Faradex* Mx10014 is a compound based on Polypropylene resin containing Stainless Steel Fiber. Added features of this material include: EMI/RFI Shielding. |
|||
Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | |
Polyplastic Armlen® PP MF 25-3-901 Polypropylene, 20% Mineral Filled Heat stabilized, black colorInformation provided by PolyPlastic Group. |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.021 cm/cm | 0.013 - 0.021 in/in | ASTM D955 |
PolyOne Dynaflex™ G7640-1 (Natural) Thermoplastic Elastomer (TPE) Dynaflex™ G7640-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhe.. |
|||
Linear Mold Shrinkage, Flow | 0.013 cm/cm @Thickness 2.00 mm |
0.013 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
DuPont Performance Polymers Zytel® 158L NC010 Nylon 612
(Unverified Data**) Zytel® 158L NC010 is an intermediate viscosity, lubricated polyamide 612 resin that is suitable for molding and extrusion applications.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.015 cm/cm @Thickness 3.20 mm |
0.013 - 0.015 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUPOL HM3102A PP+MF10%, High Impact Description: Injection Molding, PP+MF10%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsInformation provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.017 cm/cm | 0.013 - 0.017 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP RN001XXC PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RN001XXC is a compound based on Nylon 66 resin containing MOS2. |
|||
Linear Mold Shrinkage, Flow | 0.013 cm/cm @Thickness 3.17 mm |
0.013 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PA6/6 GB25 L BK 25% Glass Bead Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 25% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.016 cm/cm @Thickness 3.20 mm |
0.013 - 0.016 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX918W PPE+PS+PA High flow NORYL GTX resin for under-the-hood and electrical applications requiring retention of properties under thermal load |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.016 cm/cm @Thickness 3.20 mm |
0.013 - 0.016 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX974 PPE+PA (Europe-Africa-Middle East) NORYL GTX974 is a material especially designed for in- or on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity for electro-static paintin.. |
|||
Linear Mold Shrinkage, Flow | 0.013 cm/cm @Time 86400 sec |
0.013 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Thermocomp P1000P PA 6 LNP* Thermocomp* P1000P is a compound based on Nylon 6 resin. Added features of this material include: Exceptional Processing.This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Flow | 0.013 cm/cm @Time 86400 sec |
0.013 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Thermocomp PZ006 PA 6 LNP* Thermocomp* PZ006 is a compound based on Nylon 6 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.015 cm/cm @Thickness 3.20 mm |
0.013 - 0.015 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX678 PPE+PA (Europe-Africa-Middle East) Noryl GTX678 resin is a high performance blend of PPE/PA that exhibits an excellent balance on non-halogenated flame retardance, conductivity, ductility, and high-heat resistance. This grade can be.. |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.017 cm/cm | 0.013 - 0.017 in/in | DIS 294-4 |
Wellman Wellamid® MR409 22H-GY1 Nylon 66, 40% Mineral Reinforced All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® 2S 20 nat PA610 Product Description: Grilamid 2S 20 natural is an unmodified medium viscosity polyamide 610 (PA610), designed for injection molding as well as extrusion. It is characterized by the following product.. |
|||
Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® 100ST BK602 Acetal (POM)
(Unverified Data**) Super Toughened High Viscosity Acetal Homopolymer Delrin 100ST BK602 is a super tough high viscosity acetal homopolymer grade with superior impact resistance. It is designed for highly stressed part.. |
|||
Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® 100ST NC010 Acetal (POM)
(Unverified Data**) Super Toughened High Viscosity Acetal Homopolymer Delrin 100ST NC010 is a super tough high viscosity acetal homopolymer grade with superior impact resistance. It is designed for highly stressed part.. |
|||
Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Sorona® FG3301 NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**) Unreinforced Renewably Sourced Polytrimethylene Terephthalate Developed for Food Contact Applications Sorona FG3301 NC010 is an unreinforced polytrimethylene terephthalate resin containing 35% renew.. |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.015 cm/cm @Time 86400 sec |
0.013 - 0.015 in/in @Time 24.0 hour |
E2P method |
Eurostar Starflam MX05036 PP, Flame Retardant, Injection Molding Starflam MX05036 is an Unfilled, Halogen Free Flame Retardant, Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | Eurotec |
Eurotec® Tecomid® NA40 NL FA50 PA6.6, unfilled, flame retardant - halogen free, natural Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | Eurotec |
Eurotec® Tecomid® NB40 NL IX PA6, impact modified, natural Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | DAM; ISO 294-4 2577 |
DuPont Performance Polymers Zytel® 151 NC010 Nylon 612
(Unverified Data**) Unreinforced Polyamide 612Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | |
BASF Novolen® 1184 L Polypropylene Nucleated grade with high processing stability containing antistatic for thermoformed parts.Data was collected by ISO methods and provided by BASF. |
|||
Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | |
BASF Novolen® 2500 H Polypropylene Injection molded parts, blow moldings and thermoformed parts.Data was collected by ISO methods and provided by BASF. |
|||
Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | |
BASF Novolen® 2800 J Polypropylene Injection molded partsData was collected by ISO methods and provided by BASF. |
|||
Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | |
BASF Novolen® 3340 PC Polypropylene Nucleated grade for injection moldings with higher transparency.Data was collected by ISO methods and provided by BASF. |
|||
Linear Mold Shrinkage, Flow | 0.013 cm/cm @Thickness 3.17 mm |
0.013 in/in @Thickness 0.125 in |
1/8" Section |
Lucent Polymers TPO-10T Thermoplastic Polyolefin, 10% Mineral Filled Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |