Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP Thermocomp P1000P PA 6

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Thermocomp P1000P PA 6.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LNP* Thermocomp* P1000P is a compound based on Nylon 6 resin. Added features of this material include: Exceptional Processing.This data was supplied by SABIC-IP for the Americas region.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D 792
Linear Mold Shrinkage, Flow 0.013 cm/cm

@Time 86400 sec
0.013 in/in

@Time 24.0 hour
ASTM D 955
Linear Mold Shrinkage, Transverse 0.014 cm/cm

@Time 86400 sec
0.014 in/in

@Time 24.0 hour
ASTM D 955
Mechanical Properties Metric English Comments
Tensile Strength at Break 84.0 MPa
12200 psi
ASTM D 638
Elongation at Break 14.7 %
14.7 %
ASTM D 638
Flexural Strength 110 MPa
16000 psi
ASTM D 790
Flexural Modulus 31.23 GPa
4530 ksi
ASTM D 790
Izod Impact, Notched 0.530 J/cm

@Temperature 23.0 °C
0.993 ft-lb/in

@Temperature 73.4 °F
ASTM D 256