Material Notes:
Heat stabilized, black colorInformation provided by PolyPlastic Group.
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.013 cm/cm
0.013 in/in
Linear Mold Shrinkage, Transverse 0.013 cm/cm
0.013 in/in
Melt Flow 13 g/10 min

@Load 2.16 kg,
Temperature 230 °C
13 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 33.0 MPa
4790 psi
ISO 527-2
Tensile Modulus 2.70 GPa
392 ksi
ISO 527-2
Izod Impact, Notched (ISO) 4.00 kJ/m²
1.90 ft-lb/in²
ISO 180/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 125 °C
257 °F
ISO 75A
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
ISO 75A
Processing Properties Metric English Comments
Melt Temperature 235 °C
455 °F
Mold Temperature 60.0 °C
140 °F