Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0070 - 0.013 cm/cm | 0.0070 - 0.013 in/in | ASTM D955 |
PolyOne Versollan™ OM 1255NX-1 Thermoplastic Elastomer (TPE) Versollan™ OM 1255NX-1 is a high performance TPU alloy designed for thin-wall overmolding onto polycarbonate (PC), ABS, PC/ABS and copolyester substrates. - Improved Grip with Matte, Rubbery Finish.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0070 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® 4501 PPC High heat resistant polyphthlate carbonate, provides DTUL of 290F at 264 psi. |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm | 0.0070 in/in | ASTM D955 |
Solvay Specialty Polymers Udel® P-1710 Polysulfone (PSU)
(Unverified Data**) Udel P-1710 polysulfone (PSU) is a tough, rigid, high-strength thermoplastic that is suitable for continuous use up to 300°F (149°C). The resin is resistant to oxidation and hydrolysis and withsta.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.012 cm/cm @Thickness 3.20 mm |
0.0070 - 0.012 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUMID GP2130A(W) PA6+GF13%, General Purpose Feature: Injection Molding, PA6+GF13%, General PurposeApplication: Automotive PartsCAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm | 0.0070 in/in | |
Ineos ABS Triax® 1120 ABS + Polyamide Blend (DAM) Key Features:UnfilledPlatableHigh impact or high impact modifiedSuitable processing methods:Injection moldingFilm extrusionBlow molding |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.0090 cm/cm @Time 86400 sec |
0.0070 - 0.0090 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP GL003 PSU (Asia Pacific) LNP* Lubricomp* GL003 is a compound based on Polysulfone resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.010 cm/cm @Time 86400 sec |
0.0070 - 0.010 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP LX00430 PEEK LNP* LUBRICOMP* LX00430 is a compound based on Pelyetheretherketone containing Proprietary Fillers. Added feature of this grade is: Wear Resistant. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.0090 cm/cm @Time 86400 sec |
0.0070 - 0.0090 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP WFL33 PBT LNP* LUBRICOMP* WFL33 is a compound based on PBT containing 15% Glass Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant. |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm @Thickness 3.18 mm |
0.0070 in/in @Thickness 0.125 in |
|
Solvay Specialty Polymers Radel® R-5000 Polyphenylsulfone (PPSU) Radel® R-5000 is a transparent polyphenylsulfone (PPSU) which offers exceptional hydrolytic stability, and toughness superior to other commercially-available, high-temperature engineering resins... |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm @Thickness 3.18 mm |
0.0070 in/in @Thickness 0.125 in |
|
Solvay Specialty Polymers Radel® R-5800 Polyphenylsulfone (PPSU) Radel® R-5800 is a high melt flow grade of Radel® polyphenylsulfone (PPSU). It is especially well-suited for parts requiring long flow length with thin walls. Radel® resins offer exceptiona.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm @Thickness 3.17 mm |
0.0070 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill FR® PBT/ABS FR Availability: North AmericaForms: PelletsFeatures: Flame RetardantProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm | 0.0070 in/in | |
Solvay Specialty Polymers Udel® P-3500 LCD Polysulfone (PSU) Udel® P-3500 LCD is a very high molecular weight grade of polysulfone, and therefore offers the greatest toughness and chemical resistance of the available grades. It is well-suited for extrusion.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.0090 cm/cm @Thickness 3.20 mm |
0.0070 - 0.0090 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® K4530 PBT (Europe-Africa-Middle East) 15% glass reinforced PBT, Hydrolytically stable, High flow, Automotive connectors. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.011 cm/cm @Thickness 3.20 mm |
0.0070 - 0.011 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Xenoy® CL101 PBT+PC Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm @Thickness 3.17 mm |
0.0070 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Plastiblend® PC/PBT IM 5720 A BK Availability: North AmericaForms: PelletsAdditive: Impact Modifier and UV StabilizerFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.0090 cm/cm @Thickness 3.20 mm |
0.0070 - 0.0090 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL HNA033 PPE+HIPS (Asia Pacific) Noryl* HNA033 resin is an unfilled modified polyphenylene ether resin designed to withstand several cycles in an autoclave. This resin is suitable for multiple conversion routes and is available in.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.0090 cm/cm @Time 86400 sec |
0.0070 - 0.0090 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP EP003 PEI LNP* Lubricomp EP003 is a Polyetherimide containing 15% PTFE/Silicone. Added features include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.0090 cm/cm @Thickness 3.20 mm |
0.0070 - 0.0090 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Xenoy® X4850 PBT+PC (Asia Pacific) Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional .. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.0090 cm/cm | 0.0070 - 0.0090 in/in | ISO DIS 294-4 |
Wellman Wellamid® GFT1525-BK 15% Glass Fiber Reinforced, Impact Modified Nylon 6 Description: Glass Fiber Reinforced, Impact Modified Nylon 6Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm @Thickness 2.00 mm |
0.0070 in/in @Thickness 0.0787 in |
60x60x2 mm; 500 bar; ISO 294-4 |
Covestro Makrolon® 2665 MAS071 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Med.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm | 0.0070 in/in | ISO 294-4,2577 |
Covestro Makrolon® LTG3123 Polycarbonate PreprocessingMax. Water content |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm | 0.0070 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® TSM-30/2 PA666-MD30 Product description: Grilon TSM-30/2 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% mineral filler. Grilon TSM-30/2 has the following important properties: Excell.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm | 0.0070 in/in | DAM; ISO 294-4 2577 |
DuPont Performance Polymers Minlon® 22C NC010 Nylon 66
(Unverified Data**) 38% Mineral/Glass Reinforced Polyamide 66 Minlon 22C NC010 is a 38% mineral/glass reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polym.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.0090 cm/cm | 0.0070 - 0.0090 in/in | b.o. ISO 2577 |
Covestro Makroblend® UT5205 PC/PBT Blend Main characteristics:• High toughness even at low temperatures• Good chemical resistance• Good paintability• Good flowability• Low moisture intakeGrade characteristics:• Impact modified•.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm @Thickness 2.00 mm |
0.0070 in/in @Thickness 0.0787 in |
60x60x2 mm; 500 bar; ISO 294-4 |
Covestro Makrolon® ET2613 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• Medium vi.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm | 0.0070 in/in | ISO 294-4,2577 |
Covestro Makrolon® LQ2687 Polycarbonate ISO 7391-PC,MLR,(,,)-18-9MVR (300 °C/1.2 kg) 12.5 cm3/10 minOptical lensMedium viscosityUV stabilizedUV 400 cut offEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in clear t.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.0090 cm/cm @Thickness 3.20 mm |
0.0070 - 0.0090 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® K4530 PBT 15% glass reinforced PBT, Hydrolytically stable, High flow, Automotive connectors. |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm @Thickness 3.17 mm |
0.0070 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill FR® PBT FR-C Availability: North AmericaForms: PelletsFeatures: Flame RetardantUL File Number: E157318Processing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm @Time 86400 sec |
0.0070 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Lubricomp GZL34E PSU LNP LUBRICOMP* GZL34E is a compound based on Polysulfone resin containing Glass Fiber, Milled Glass, PTFE. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP f.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.0090 cm/cm | 0.0070 - 0.0090 in/in | ASTM D955 |
PolyOne Edgetek® XT XT-100-CX00 PC+PBT
(discontinued **) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |