Category | Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) |
Manufacturer | SABIC Innovative Plastics (GE Plastics) |
Trade Name | Valox® |
Port | Shanghai port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | SABIC Innovative Plastics Valox® K4530 PBT.pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.41 g/cc | 1.41 g/cc | ASTM D792 |
Linear Mold Shrinkage, Flow | 0.0070 - 0.0090 cm/cm @Thickness 3.20 mm |
0.0070 - 0.0090 in/in @Thickness 0.126 in |
SABIC Method |
Linear Mold Shrinkage, Transverse | 0.010 - 0.012 cm/cm @Thickness 3.20 mm |
0.010 - 0.012 in/in @Thickness 0.126 in |
SABIC Method |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 82.0 MPa | 11900 psi | Type I, 5 mm/min; ASTM D638 |
89.0 MPa | 12900 psi | Type I, 5 mm/min; ASTM D638 | |
98.0 MPa | 14200 psi | Type I, 5 mm/min; ASTM D638 | |
103 MPa | 14900 psi | Type I, 5 mm/min; ASTM D638 | |
Tensile Strength, Yield | 103 MPa | 14900 psi | Type I, 5 mm/min; ASTM D638 |
Elongation at Break | 2.3 % | 2.3 % | Type I, 5 mm/min; ASTM D638 |
2.5 % | 2.5 % | Type I, 5 mm/min; ASTM D638 | |
3.8 % | 3.8 % | Flexural Strain, 1.3 mm/min, 50 mm span; ASTM D790 | |
4.0 % | 4.0 % | Type I, 5 mm/min; ASTM D638 | |
4.0 % | 4.0 % | Type I, 5 mm/min; ASTM D638 | |
6.0 % | 6.0 % | Flexural Strain, 1.3 mm/min, 50 mm span; ASTM D790 | |
7.0 % | 7.0 % | Flexural Strain, 1.3 mm/min, 50 mm span; ASTM D790 | |
9.7 % | 9.7 % | Flexural Strain, 1.3 mm/min, 50 mm span; ASTM D790 | |
Elongation at Yield | 4.0 % | 4.0 % | Type I, 5 mm/min; ASTM D638 |
Tensile Modulus | 3.55 GPa | 515 ksi | 5 mm/min; ASTM D638 |
Flexural Strength | 150 MPa | 21800 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
Flexural Modulus | 4.52 GPa | 656 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
4.64 GPa | 673 ksi | 1.3 mm/min, 50 mm span; ASTM D790 | |
4.82 GPa | 699 ksi | 1.3 mm/min, 50 mm span; ASTM D790 | |
5.10 GPa | 740 ksi | 1.3 mm/min, 50 mm span; ASTM D790 | |
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
Izod Impact, Unnotched | 4.00 J/cm | 7.49 ft-lb/in | ASTM D4812 |
Dart Drop, Total Energy | 4.00 J | 2.95 ft-lb | ASTM D3763 |
5.00 J | 3.69 ft-lb | ASTM D3763 | |
6.00 J | 4.43 ft-lb | ASTM D3763 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 218 °C @Thickness 3.20 mm |
424 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
Deflection Temperature at 1.8 MPa (264 psi) | 193 °C @Thickness 3.20 mm |
379 °F @Thickness 0.126 in |
unannealed; ASTM D648 |