Techmer ES HiFill FR® PBT/ABS FR

Category Polymer , Thermoplastic , ABS Polymer , ABS/Polyester Alloy , Polyester, TP
Manufacturer Techmer ES
Trade Name HiFill FR®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Techmer ES HiFill FR® PBT/ABS FR.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Availability: North AmericaForms: PelletsFeatures: Flame RetardantProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.33 g/cc
0.0480 lb/in³
ASTM D792
Water Absorption 0.15 %

@Time 86400 sec
0.15 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0070 cm/cm

@Thickness 3.17 mm
0.0070 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 41.4 MPa
6000 psi
ASTM D638
Elongation at Yield 20 %
20 %
ASTM D638
Flexural Strength 62.1 MPa
9000 psi
ASTM D790
Flexural Modulus 0.238 GPa
34.5 ksi
ASTM D790
Izod Impact, Notched 0.374 J/cm

@Thickness 3.17 mm
0.700 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 101 µm/m-°C
56.0 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 90.6 °C
195 °F
Unannealed; ASTM D648
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
ASTM D257
Dielectric Strength 27.6 kV/mm
700 kV/in
Method A (Short-Time); ASTM D149