Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0080 - 0.011 cm/cm | 0.0080 - 0.011 in/in | ASTM D955 |
PolyOne Gravi-Tech™ GRV-NY-027-SS-BLK-F Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.011 cm/cm | 0.0050 - 0.011 in/in | ASTM D955 |
PolyOne Gravi-Tech™ GRV-NY-085-W-NAT Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.011 cm/cm | 0.0070 - 0.011 in/in | ASTM D955 |
PolyOne Maxxam™ STFPP.1220 BK-L Polypropylene, Unspecified (PP, Unspecified) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.011 cm/cm | 0.0090 - 0.011 in/in | on tensile bar; SABIC Method |
SABIC Innovative Plastics Lexan® FL3000 PC (Europe-Africa-Middle East) FL3000 is an FR product with excellent low temperature impact, bromine and chlorine free, good retention of properties upon weathering.This data was supplied by SABIC-IP for the Europe-Africa-Middle.. |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.011 cm/cm | 0.0050 - 0.011 in/in | ASTM D955 |
PolyOne Dynaflex™ G2701-1000-02 Thermoplastic Elastomer (TPE) Dynaflex™ G2701-1000-02 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Adhesion to Polypropylene - Excellent Colorability - Good .. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.011 cm/cm | 0.0060 - 0.011 in/in | ASTM D955 |
PolyOne Dynaflex™ G7980-9 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7980-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.011 cm/cm | 0.0060 - 0.011 in/in | ASTM D955 |
PolyOne Dynaflex™ G7980-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7980-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen.. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.011 cm/cm | 0.0060 - 0.011 in/in | ASTM D955 |
PolyOne Dynaflex™ G7980-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylene - Rubbery Feel - Soft T.. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.011 cm/cm @Thickness 3.20 mm |
0.0060 - 0.011 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUCEL GC210 POM+GF10%, High Rigidity Feature: Injection Molding, POM+GF10%, High RigidityApplication: Casings of Pump and Pivot BearingsCAS No. 66455-31-0 and 65997-17-3Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.011 cm/cm @Thickness 3.20 mm |
0.0060 - 0.011 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUMID GP2151BF PA66+GF15%, Flame Retardant Feature: Injection Molding, PA66+GF15%, Halogen Free Flame RetardantApplication: ConnectorsCAS No. 32131-17-2, 25038-54-4, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG.. |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.011 cm/cm @Thickness 3.20 mm |
0.0050 - 0.011 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUMID LW4403A(W) PA66+GF/MF40%, Low Warpage Feature: Injection Molding, PA66+GF/MF40%, Low WarpageApplication: Automotive (Timing Belt Cover)CAS No. 25038-54-4, 13983-17-0 and 65997-17-3Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.011 cm/cm @Thickness 3.20 mm |
0.0040 - 0.011 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUMID LW4403B(W) PA66+GF/MF40%, Low Warpage Feature: Injection Molding, PA66+GF/MF40%, Low WarpageApplication: Automotive PartsCAS No. 32131-17-2, 13983-17-0 and 65997-17-3Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.011 cm/cm @Thickness 3.20 mm |
0.0090 - 0.011 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUPOL HI5205 PP+MF20%, High Impact Description: Injection Molding, PP+MF20%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 26221-73-8 and 14807-96-6Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.011 cm/cm @Thickness 3.20 mm |
0.0090 - 0.011 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUPOL HI5302RB PP+MF25%, High Impact Description: Injection Molding, PP+MF25%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 9010-79-1 and 14807-96-6Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.011 cm/cm @Thickness 3.20 mm |
0.0040 - 0.011 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical Lupox® GP2200 PBT+GF20% Description: Injection Molding, PBT+GF20%, General Purpose Application: IT/OA, E&E, Automotive (Connector)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.011 cm/cm @Time 86400 sec |
0.0090 - 0.011 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRILOY UA200A PPA LNP LUBRILOY* UA200A is a compound based on Polyphthalamide resin containing Aramid Fiber, Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.011 cm/cm @Time 86400 sec |
0.0090 - 0.011 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRILOY UA200A PPA (Asia Pacific) LNP LUBRILOY* UA200A is a compound based on Polyphthalamide resin containing Aramid Fiber, Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.011 cm/cm | 0.0070 - 0.011 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Xenoy® CL101 PBT+PC (Europe-Africa-Middle East) Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.011 cm/cm @Thickness 3.20 mm |
0.0070 - 0.011 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Xenoy® HX5600HP PBT+PC Xenoy HX5600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.011 cm/cm @Thickness 3.20 mm |
0.0070 - 0.011 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Xenoy® HX5600HP PBT+PC (Europe-Africa-Middle East) Xenoy HX5600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Linear Mold Shrinkage, Flow | 0.0095 - 0.011 cm/cm @Thickness 3.20 mm |
0.0095 - 0.011 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Xenoy® X4820 PBT+PC Xenoy X4820 is a high modulus PC/PBT Blend. This resin provides high chemical resistance, excellent impact, very low creep, low CTE, excellent fatigue and dimensional stability. |
|||
Linear Mold Shrinkage, Flow | 0.0095 - 0.011 cm/cm @Thickness 3.20 mm |
0.0095 - 0.011 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Xenoy® X4820 PBT+PC (Asia Pacific) Xenoy X4820 is a high modulus PC/PBT Blend. This resin provides high chemical resistance, excellent impact, very low creep, low CTE, excellent fatigue and dimensional stability. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.011 cm/cm @Time 86400 sec |
0.0090 - 0.011 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP 9X04488 POLYPHENYLENESULFONE (Asia Pacific) LNP* Thermocomp* 9X04488 is a compound based on POLYPHENYLENESULFONE resin containing Mineral. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.011 cm/cm @Time 86400 sec |
0.0090 - 0.011 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP 9X07435 LNP* THERMOCOMP* is a compound based on Miscellaneous resin containing Proprietary Filler(s). Added feature of this grade is: Plateable. |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.011 cm/cm @Thickness 3.20 mm |
0.0040 - 0.011 in/in @Thickness 0.126 in |
ASTM D955 |
Samsung Cheil Industries Infino® GP-5150GT PBT, 15% Glass Filled Low warpage with 15% GF reinforcement and can be used in the switches for microwave or ovensInformation provided by Samsung Cheil Industries. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.011 cm/cm @Thickness 3.20 mm |
0.0070 - 0.011 in/in @Thickness 0.126 in |
ASTM D955 |
Samsung Cheil Industries Infino® VB-3100G PBT/ABS, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.011 cm/cm @Thickness 3.20 mm |
0.0040 - 0.011 in/in @Thickness 0.126 in |
ASTM D955 |
Samsung Cheil Industries Infino® VB-5150GL PBT, 15% Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.011 cm/cm @Thickness 3.20 mm |
0.0040 - 0.011 in/in @Thickness 0.126 in |
ASTM D955 |
Samsung Cheil Industries Infino® GP-5150GT PBT, 15% Glass Filled Low warpage with 15% GF reinforcement and can be used in the switches for microwave or ovensInformation provided by Samsung Cheil Industries. |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.011 cm/cm | 0.0080 - 0.011 in/in | on tensile bar; SABIC Method |
SABIC Innovative Plastics Xenoy® XL1562 PBT+PC (Europe-Africa-Middle East) XENOY XL1562 is an impact modified PBT+PC blend with outstanding chemical resistance, good UV stability and flow properties.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.011 cm/cm | 0.0070 - 0.011 in/in | |
LATI Latimass 47/7-04 D008 PP Copolymer Specific density compound based on Polypropylene copolymer (PPc). Special filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati In.. |