Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0050 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Cycolac® MG94U ABS High flow, UV stabilized ABS molding grade |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0070 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® 4501 PPC (Asia Pacific) High heat resistant polyphthlate carbonate, provides DTUL of 290F at 264 psi. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0060 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® 925 PC (Asia Pacific) Lexan* 925 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a UL V0 rating. Lexan resin 925 is available in various opa.. |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® DMX1214 PC Copolymer (Asia Pacific) This product will be phased out per January 2015 -- Lexan* DMX1214 resin is an improved flow, transparent copolycarbonate resin with improved scratch resistance. |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® EXL1036 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1036 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high viscosity grade designed for (co-)extrusion. This resin offers extreme low temperature (-60 C) ductility and good h.. |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® EXL1132 PC Copolymer Lexan* EXL1132 polycarbonate (PC) siloxane copolymer resin is a high flow, UV stabilized injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high fl.. |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® EXL1463T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1463T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility in combination with medium flow ch.. |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® FXG1414T PC Copolymer (Europe-Africa-Middle East) PC-siloxane copolymer in special "Diamond Sparkle" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supp.. |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® FXM1414T PC Copolymer (Europe-Africa-Middle East) PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supplied by .. |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.0080 cm/cm @Thickness 4.00 mm, Temperature 23.0 °C |
0.0040 - 0.0080 in/in @Thickness 0.157 in, Temperature 73.4 °F |
Injection Molded, Bergmann Method; ASTM D955 |
PolyOne Bergamid™ B70 G/GK30 TM-Y UV NC Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® HPB3144G PC Copolymer Standard flow, transparent, high purity polycarbonate copolymer resin with reduced oxygen permeability and water vapor transmission rate. For medical devices and pharmaceutical applications. Health.. |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® HPX4 PC Copolymer (Asia Pacific) Medium flow specialty polycarbonate - improved processability & autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP.. |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® HPX8R PC Copolymer (Asia Pacific) Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o.. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0060 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® LUX9612G PC (Europe-Africa-Middle East) Lexan LUX9612G (EXRL0945) is a UV stabilized high viscosity, flame retardant polycarbonate featuring non brominated and non chlorinated FR system with diffusion effect and thin wall FR performance p.. |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.0080 cm/cm | 0.0050 - 0.0080 in/in | |
Eastman Eastalloy DA111 PC+PET Copolyester/Polycarbonate
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0060 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® 925AU PC Lexan* 925AU Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing addit.. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0060 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® DMX1132 PC Copolymer (Asia Pacific) Lexan* DMX1132 is a high flow polycarbonate copolymer resin with improved ammonia resistance over regular polycarbonate resin. |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0080 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical HIPS 410AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Office Appliances (Parts of Printer or Copier)CAS: 9003-55-8, 25713-60-4 and 1309-64-4Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.0080 cm/cm | 0.0050 - 0.0080 in/in | Test Condition: 150x105x3; acc. ISO 2577 |
Ineos ABS Lustran® Ultra 4000 PG ABS Pellets (a-methylstyrene-SAN-modified), Electroplating Grade Lustran® Ultra 4000 PG is electroplating grade with high heat resistance. It is used for the production of molded plastic articles. |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.0080 cm/cm | 0.0050 - 0.0080 in/in | |
LATI Latilub 57-30GRTS G/20 PPA, 20% Glass Fiber Reinforced Self-lubricating product based on Semi-aromatic polyamide (PPA). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu.. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0060 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL PX6120 PPE+PS (Europe-Africa-Middle East) Noryl PX6120 is an unfilled material with good flow, high Impact and chemical resistance against cleaners. Noryl PX6120 is developed for personal care appplications. |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.0080 cm/cm | 0.0050 - 0.0080 in/in | SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP GL003XXP PSU (Europe-Africa-Middle East) LNP* LUBRICOMP* GL003XXP is a compound based on Polysulfone resin containing PTFE. Added features include; Internally Lubricated. |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0080 in/in @Thickness 0.126 in |
ASTM D955 |
Samsung Cheil Industries Starex® TF-0956 HI-PMMA Information provided by Samsung Cheil Industries. |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL NH7010HF PPE+PS Noryl* NH7010HF resin is a modified PPE-PS blend that exhibits an excellent balance of non-halogenated flame retardance, high heat resistance, good flow, and low specifc gravity for light weight par.. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0060 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® VX4910 ASA+PBT (Europe-Africa-Middle East) 10% Glass reinforced nucleated PBT/ASA with excellent mechanical properties high dimensional stability, and low density. |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Xenoy® X6320 PBT+PC (Asia Pacific) X6320 is a mineral filled PBT/PC resin developed for automotive painted doorhandles. Key advantages are excellent surface finish, easy processing and paint quality. |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.0080 cm/cm | 0.0050 - 0.0080 in/in | on tensile bar; SABIC Method |
SABIC Innovative Plastics Xenoy® XL1339U PC+PET (Europe-Africa-Middle East) XENOY XL1339U is an unreinforced amorphous PC+PET blend, offering excellent impact performance over a wide temperature range. It combines very good flow characteristics with high heat resistance. XL.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0070 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics XYLEX X7519HP PC+POLYESTER (Asia Pacific) Good Chemical Resistance, XYLEX grade with good dishwasher performance, USA/Europe Food Contact Comment: While molding of thicker parts, cooling speed has an influence of transparency. Thicker parts.. |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® EXL1033C PC Copolymer Lexan*EXL1033C polycarbonate (PC) siloxane copolymer resin is a low flow, UV stabilized grade designed for (co)-extrusion. This resin offers low temperature (-30C) ductility and excellent extrusion .. |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.0080 cm/cm | 0.0040 - 0.0080 in/in | on tensile bar; SABIC Method |
SABIC Innovative Plastics Lexan® FXG1413T PC Copolymer (Europe-Africa-Middle East) PC-siloxane copolymer in special "Diamond Sparkle" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supp.. |