Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.025 - 0.028 cm/cm
0.025 - 0.028 in/in
ASTM D955
PolyOne Stat-Tech™ AT-CB2/000 CR Acetal (POM) Copolymer
Stat-Tech™ AT-CB2/000 CR XP020229R2Information provided by PolyOne
Linear Mold Shrinkage, Flow 0.025 - 0.027 cm/cm
0.025 - 0.027 in/in
ASTM D955
PolyOne Edgetek® 5209 Natural 1 Acetal (POM) Copolymer
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
Linear Mold Shrinkage, Flow 0.025 - 0.027 cm/cm
0.025 - 0.027 in/in
ASTM D955
PolyOne Edgetek® 5230 Natural 1 Acetal (POM) Copolymer
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
Linear Mold Shrinkage, Flow 0.025 cm/cm
0.025 in/in
ASTM D955
Solvay Specialty Polymers Halar® 1450LC Polyethylene, Chlorotrifluoroethylene (ECTFE)  (Unverified Data**)
Information provided by Solvay Specialty Polymers.
Linear Mold Shrinkage, Flow 0.025 cm/cm
0.025 in/in
ASTM D955
Solvay Specialty Polymers Halar® 300LC Polyethylene, Chlorotrifluoroethylene (ECTFE)  (discontinued **)
Information provided by Solvay Specialty Polymers.
Linear Mold Shrinkage, Flow 0.025 cm/cm
0.025 in/in
ASTM D955
Solvay Specialty Polymers Halar® 350LC Polyethylene, Chlorotrifluoroethylene (ECTFE)  (Unverified Data**)&
Information provided by Solvay Specialty Polymers.
Linear Mold Shrinkage, Flow 0.025 cm/cm
0.025 in/in
ASTM D955
Solvay Specialty Polymers Halar® 500LC Polyethylene, Chlorotrifluoroethylene (ECTFE)  (Unverified Data**)&
Information provided by Solvay Specialty Polymers.
Linear Mold Shrinkage, Flow 0.025 cm/cm
0.025 in/in
ASTM D955
Solvay Specialty Polymers Halar® 513LC Polyethylene, Chlorotrifluoroethylene (ECTFE)  (Unverified Data**)&
Information provided by Solvay Specialty Polymers.
Linear Mold Shrinkage, Flow 0.025 cm/cm
0.025 in/in
ASTM D955
Solvay Specialty Polymers Halar® 901 Polyethylene, Chlorotrifluoroethylene (ECTFE)  (Unverified Data**)<
Information provided by Solvay Specialty Polymers.
Linear Mold Shrinkage, Flow 0.025 cm/cm
0.025 in/in
ASTM D955
Solvay Specialty Polymers Halar® 902 Polyethylene, Chlorotrifluoroethylene (ECTFE)  (Unverified Data**)<
Information provided by Solvay Specialty Polymers.
Linear Mold Shrinkage, Flow 0.025 - 0.027 cm/cm
0.025 - 0.027 in/in
Kraton® D2104 DI-N (SBS) Compound
Description: Kraton D2104 DI-N is an easy processing, general purpose material designed for a wide variety of applications. It is supplied from North America in the physical form identified: D2104 D..
Linear Mold Shrinkage, Flow 0.025 - 0.027 cm/cm
0.025 - 0.027 in/in
Kraton® D2109 DS-W (SBS) Compound
Description: Kraton D2109 DS-W is an easy processing, general purpose 45 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form..
Linear Mold Shrinkage, Flow 0.025 cm/cm
0.025 in/in
SABIC Method
SABIC Innovative Plastics LNP LUBRICOMP KA000M POM (Europe-Africa-Middle East)
LNP* LUBRICOMP* KA000M is a compound based on Acetal Copolymer resin containg Aramide and Proprietary Lubricant. Added features include Internally Lubricated.
Linear Mold Shrinkage, Flow 0.025 - 0.030 cm/cm

@Time 86400 sec
0.025 - 0.030 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRILOY KL201 Acetal
LNP LUBRILOY* KL201 is a compound based on Acetal resin containing Proprietary Lubricant. PTFE. Added feature of this material is: Wear Resistant.
Linear Mold Shrinkage, Flow 0.025 - 0.030 cm/cm

@Time 86400 sec
0.025 - 0.030 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRILOY KL201 Acetal (Europe-Africa-Middle East)
LNP LUBRILOY* KL201 is a compound based on Acetal resin containing PTFE, Proprietary Lubricant. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Flow 0.025 cm/cm
0.025 in/in
Solvay Specialty Polymers Halar® 1400LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE)
Low ViscosityUses: FibersAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 300 °CInformation provided by Solvay Spec..
Linear Mold Shrinkage, Flow 0.025 cm/cm
0.025 in/in
Solvay Specialty Polymers Halar® 300DA Ethylene Chlorotrifluoroethylene Copolymer (ECTFE)
Halar® "DA" grades are available and meet the FDA's Condition of Use B, as described under 21 C.F.R. 176-170(c).Features: Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 ..
Linear Mold Shrinkage, Flow 0.025 cm/cm
0.025 in/in
Solvay Specialty Polymers Halar® 350LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE)
Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Pol..
Linear Mold Shrinkage, Flow 0.025 cm/cm
0.025 in/in
Solvay Specialty Polymers Halar® 5001C Ethylene Chlorotrifluoroethylene Copolymer (ECTFE)
Powder grades for masterbatches.Features: Low ViscosityUses: Masterbatch; Wire & Cable ApplicationsAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0..
Linear Mold Shrinkage, Flow 0.025 cm/cm
0.025 in/in
Solvay Specialty Polymers Halar® 500LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE)
Low ViscosityUses: Wire & Cable ApplicationsAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation prov..
Linear Mold Shrinkage, Flow 0.025 cm/cm

@Thickness 3.17 mm
0.025 in/in

@Thickness 0.125 in
ASTM D955
Techmer ES HiFill FR® PBT FR X
Availability: North AmericaForms: PelletsAdditive: Mold ReleaseFeatures: Flame RetardantProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.
Linear Mold Shrinkage, Flow 0.025 cm/cm
0.025 in/in
Solvay Specialty Polymers Halar® 901 Ethylene Chlorotrifluoroethylene Copolymer (ECTFE)
High ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Polym..
Linear Mold Shrinkage, Flow 0.025 cm/cm
0.025 in/in
Solvay Specialty Polymers Halar® 902 Ethylene Chlorotrifluoroethylene Copolymer (ECTFE)
High ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 28.0 J/g; Heat of Fusion - ASTM D3418 28.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Polym..
Linear Mold Shrinkage, Flow 0.025 - 0.030 cm/cm
0.025 - 0.030 in/in
ISO DIS 294-4
Wellman Wellamid® XT1867-BK1 High Impact Nylon 66
Description: High Impact Nylon 66Information provided by Wellman.
Linear Mold Shrinkage, Flow 0.025 cm/cm
0.025 in/in
annealed; ISO 294-4
DuPont Performance Polymers Crastin® ST820 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
Unreinforced Polybutylene Terephthalate with Excellent Impact Resistance Crastin ST820 NC010 is an unreinforced Super Tough polybutylene terephthalate resin for injection molding.Information provide..
Linear Mold Shrinkage, Flow 0.025 cm/cm
0.025 in/in
ISO 294-4
Barlog Plastics KEBAFLEX SG 55 A.01 TPE-S, Shore A55, natural
TPE-SInformation provided by BARLOG plastics GmbH.
Linear Mold Shrinkage, Flow 0.025 - 0.030 cm/cm

@Thickness 3.20 mm
0.025 - 0.030 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics NORYL FM3020V PPE+PS (Asia Pacific)
30% filled FR high modulus foam grade
Linear Mold Shrinkage, Flow 0.025 cm/cm

@Thickness 3.17 mm
0.025 in/in

@Thickness 0.125 in
ASTM D955
Techmer ES HiFill FR® PBT FR