Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.014 - 0.020 cm/cm | 0.014 - 0.020 in/in | ASTM D955 |
PolyOne Versalloy™ XL 9070X-9 Thermoplastic Elastomer (TPE) Versalloy™ XL 9070X-9 is a TPV alloy with exceptional flow properties and surface aesthetics for a variety of applications. - Exceptional Flow for Long, Thin Flow Paths - Overmold Adhesion to Polyp.. |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm @Thickness 3.17 mm |
0.014 in/in @Thickness 0.125 in |
ASTM D955 |
Network Polymers Softflex® 0921 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm | 0.014 in/in | Euronil |
Nilit Nilamid B3 H ZC Unfilled, Low Temperature Impact Resistant PA6 Description: Nilamid B3 H ZC has outstanding impact performance, even at minus temperatures. It is widely used for components subjected to high shock loads. Applications include bicycle components, .. |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm | 0.014 in/in | ASTM D955 |
PolyOne Elastamax™ XL 0135-33 Styrene Butadiene Block Copolymer (SBC) A thermoplastic elastomer compound formulated for use in food contact applications. The physical properties listed above are typical values obtained on laboratory prepared samples and tested in acco.. |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm | 0.014 in/in | Euronil |
Nilit Nilamid B3 H ZB Unfilled, Low Temperature Impact Resistant PA6 Description: Nilamid B3 H ZB is a high impact NYLON 6. The product has excellent impact properties, even at minus temperatures, whilst maintaining mechanical characteristics. Application areas inclu.. |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm @Thickness 2.00 mm |
0.014 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
DuPont Performance Polymers Zytel® 101 NC010 Nylon 66
(Unverified Data**) Zytel® 101 NC010 is a general purpose polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm @Thickness 2.00 mm |
0.014 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
DuPont Performance Polymers Zytel® 101F BKB009 Nylon 66
(Unverified Data**) Zytel® 101F BKB009 is an internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm @Thickness 2.00 mm |
0.014 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
DuPont Performance Polymers Zytel® FG42A NC010 Nylon 66
(Unverified Data**) Zytel® FG42A NC010 is a high viscosity polyamide 66 resin for injection molding and extrusion. It has been developed for consideration into applications such as parts for the food industry.Informat.. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.018 cm/cm @Thickness 3.20 mm |
0.014 - 0.018 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUMID HI1202A(W) PA6, High Impact Feature: Injection Molding, PA6, High ImpactApplication: Electric/Electronic PartsCAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.018 cm/cm @Thickness 3.20 mm |
0.014 - 0.018 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUPOL HG3200SK2 PP+MF20%, High Gloss Description: Injection Molding, PP+MF20%, High GlossApplication: Electrical & Electronic PartsCAS: 9003-07-0 and 7727-43-7Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm | 0.014 in/in | ISO 294 |
Inno-Comp INNOPOL® CS 2-5000 Polypropylene Block-Copolymer INNOPOL® CS 2-5000 is a polypropylene block-copolymer compound. This grade is available in nature and custom colored form.INNOPOL® CS 2-5000 is developed for producing injection molded automot.. |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm @Thickness 3.17 mm |
0.014 in/in @Thickness 0.125 in |
1/8" Section |
Lucent Polymers TPP-310 Polypropylene, 10% Talc Filled, Impact Modified Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.022 cm/cm | 0.014 - 0.022 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP KA000 Acetal Copolymer (Europe-Africa-Middle East) LNP* Lubricomp* KA000 is a compound based on Acetal Copolymer resin containing Aramid Fiber, Proprietary Lubricant. |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm | 0.014 in/in | SABIC Method |
SABIC Innovative Plastics LNP LUBRILOY UX99725 PPA LNP LUBRILOY* UX99725 is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm | 0.014 in/in | SABIC Method |
SABIC Innovative Plastics LNP Thermocomp FX05032 PE (Europe-Africa-Middle East) LNP* THERMOCOMP* FX05032 is a compound based on Polyethylene resin containing Proprietary Filler(s). Added features include : Foaming Agent for Polyolefins.This data was supplied by SABIC-IP for t.. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.016 cm/cm | 0.014 - 0.016 in/in | ASTM D955 |
Shinkong Synthetic Fibers Shinite® PP4220 PP, High Impact, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.016 cm/cm | 0.014 - 0.016 in/in | ASTM D955 |
Shinkong Synthetic Fibers Shinite® PP4410 PP, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.017 cm/cm @Thickness 3.20 mm |
0.014 - 0.017 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA (Asia Pacific) NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.018 cm/cm | 0.014 - 0.018 in/in | on tensile bar; SABIC Method |
SABIC Innovative Plastics Noryl GTX GTX976 PPE+PA (Europe-Africa-Middle East) NORYL GTX976 is a material especially designed for electrostatic painting and powder coating applications. This material combines high impact performance with conductivity in an unique way.This data.. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.016 cm/cm | 0.014 - 0.016 in/in | ASTM D955 |
Shinkong Synthetic Fibers Shinite® PP4410 PP, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm @Thickness 2.00 mm |
0.014 in/in @Thickness 0.0787 in |
TPE Method |
SCG Chemicals EL-Proâ„¢ P852J Polypropylene Injection Molding Key Characteristics:Excellent productivityHigh clarityHigh stiffnessRecommended Applications:Clear food containerClear large size containerHousehold products and other articles that require high tra.. |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm | 0.014 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Hytrel® 5553FG NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm | 0.014 in/in | DAM; ISO 294-4 2577 |
DuPont Performance Polymers Zytel® FG42A NC010 Nylon 66
(Unverified Data**) Unreinforced High Viscosity Polyamide 66 with Developed for Food Contact ApplicationsZytel FG42A NC010 is a high viscosity polyamide 66 resin for injection molding and extrusion. It has been develop.. |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm @Thickness 4.00 mm |
0.014 in/in @Thickness 0.157 in |
E2P method |
Eurostar Staramide P1000IX3 PA6, Impact Modified, Injection Molded Staramide P1000IX3 is an Impact Modified, Polyamide 6 Injection Molding Resin (also known as P1000HI020 or Star X 2020)Information provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm | 0.014 in/in | Eurotec |
Eurotec® Tecomid® NA40 MR15 NL IL PA6.6, 15% mineral filled, impact modified, natural Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm | 0.014 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Hytrel® RS R4275 BK316 Polyester Elastomer TPC-ET 55 Shore D Renewably Sourced High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm | 0.014 in/in | ISO 294-4 |
Azoty Tarnow™ Tarnamid® T-27 GB30 Polyamide 6 - Glass Beads Reinforced 30% Glass beads reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High.. |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm | 0.014 in/in | ISO 294-4 |
Azoty Tarnow™ Tarnamid® T-27 MS Polyamide 6 - Natural Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.For uncolored parts produced by injection molding, contain including and demo.. |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm @Thickness 3.17 mm |
0.014 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Luriblend® POM CO GF5 TL5 5% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 5% Filler by WeightAdditive: PTFE Lubricant(5%)Features: Lubricated and CopolymerInformation provided by TP Composites, In.. |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm @Thickness 3.17 mm |
0.014 in/in @Thickness 0.125 in |
1/8" Section |
Lucent Polymers TPP-210 Polypropylene, 10% Talc Filled, Impact Modified Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |