Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0080 cm/cm | 0.0080 in/in | ASTM D955 |
PolyOne Nymax™ 600 A Zip 22 Natural Polyamide 6 Alloy (Nylon 6 Alloy) The Nymax® 600 Blend Series of nylon 6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materials.. |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.010 cm/cm @Thickness 3.20 mm |
0.0080 - 0.010 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics EXTEM UH1006M TPI Blend (Asia Pacific) High heat amorphous TPI Blend, Chemical Resistant |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.010 cm/cm @Thickness 3.20 mm |
0.0080 - 0.010 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics EXTEM UH1016 TPI Blend (Asia Pacific) High heat amorphous TPI Blend, Chemical Resistant, High Flow |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.010 cm/cm @Thickness 3.20 mm |
0.0080 - 0.010 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® PPC4704 PPC High heat resistant polycarbonate copolymer, provides DTUL of 300F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported wit.. |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | ASTM D955 |
PolyOne Geon™ Vinyl Flexible B5DU0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | ASTM D955 |
PolyOne Geon™ Vinyl Flexible B5D00 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.012 cm/cm @Thickness 3.17 mm |
0.0080 - 0.012 in/in @Thickness 0.125 in |
ASTM D955 |
Ravago Manufacturing Americas Hylon® N1020MHL Nylon 6/6
(discontinued **) Available in North America Filler: Mineral, 20% Filler by WeightAdditive: Heat Stabilizer and Lubricant Features: Lubricated and Heat StabilizedForm: Pellets Processing Method: Injection MoldingIn.. |
|||
Linear Mold Shrinkage, Flow | 0.0080 cm/cm | 0.0080 in/in | ISO 294-4, 2577 |
Lanxess Durethan® DP A 32 901510 Nylon 66 PA 66 standard injection molding grade, non-reinforced, very easy release |
|||
Linear Mold Shrinkage, Flow | 0.0080 cm/cm @Thickness 3.17 mm |
0.0080 in/in @Thickness 0.125 in |
1/8" Section |
Lucent Polymers GPP-110 Polypropylene Homopolymer, 10% Glass Fiber Reinforced, Chemically Coupled Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.0080 cm/cm @Thickness 3.17 mm |
0.0080 in/in @Thickness 0.125 in |
1/8" Section |
Lucent Polymers GPP-210 Polypropylene, 10% Glass Fiber Reinforced, Chemically Coupled, Impact Modified Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.010 cm/cm | 0.0080 - 0.010 in/in | |
LATI Kelon® B FR H CET/05-V2HF PA 6, Mineral Reinforced, Flame Retardant, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free.Availability: Africa & Middle East; Asia Pacific; Eur.. |
|||
Linear Mold Shrinkage, Flow | 0.0080 cm/cm | 0.0080 in/in | |
Solvay TECHNYL® C 52G3 MZ25 PA6, DRY Description: Flame retardant polyamide PA6 reinforced with mineral filler, for injection molding.Available in: Asia Pacific, Europe, Latin America and North America Product Applications: This phosph.. |
|||
Linear Mold Shrinkage, Flow | 0.0080 cm/cm @Thickness 3.17 mm |
0.0080 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Elastoblend® PA6 IM 811 HS L (Conditioned) Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedTPCI# 6109102Information provided by TP Comp.. |
|||
Linear Mold Shrinkage, Flow | 0.0080 cm/cm @Thickness 3.17 mm |
0.0080 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Electrablend® PA6/6 05012 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: ConductiveInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.010 cm/cm @Time 86400 sec |
0.0080 - 0.010 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON DX11408 PC LNP* STAT-KON* DX11408 is a compound based on Polycarbonate containing Carbon Powder. Added features of this material include: Electrically Conductive, Improved Ductility |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.010 cm/cm @Time 86400 sec |
0.0080 - 0.010 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON DX98477 PC LNP* STAT-KON* DX98477 is a compound based on Polycarbonate containing Proprietary Filler(s). Added feature of this grade is: Electrically Conductive. |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.012 cm/cm @Thickness 3.20 mm |
0.0080 - 0.012 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Xenoy® IQ1103 PBT+PC (Europe-Africa-Middle East) Xenoy iQ*1103 resin - Environmentally responsible and sustainable low carbon footprint resin. Xenoy iQ1103 is an unreinforced, impact modified alloy of PC (polycarbonate) + Valox iQ* PBT (polybuty.. |
|||
Linear Mold Shrinkage, Flow | 0.0080 cm/cm @Thickness 3.17 mm |
0.0080 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Luriblend® PA6/6 AF10 Nylon 66 Availability: North AmericaForms: PelletsFiller/Reinforcement: Aramid Fiber, 10% Filler by WeightAdditive: LubricantFeatures: Lubricated, Good Wear Resistance and Low FrictionInformation provided by.. |
|||
Linear Mold Shrinkage, Flow | 0.0080 cm/cm @Time 86400 sec |
0.0080 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Thermocomp DX93681 PC LNP* Thermocomp* DX93681 is a compound based on Polycarbonate resin containing Proprietary Filler(s).This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.010 cm/cm @Thickness 3.20 mm |
0.0080 - 0.010 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Noryl GTX GTX965 PPE+PA66 NORYL GTX965 is a mineral reinforced PPE/PA blend. It offers excellent surface appearance, processability and dimensional stability at elevated temperatures. The best molding condition for good appe.. |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.012 cm/cm @Thickness 3.20 mm |
0.0080 - 0.012 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL PPX PPX7110 PPE+PP PPE+PP blend. High Impact, Good Heat Resistance |
|||
Linear Mold Shrinkage, Flow | 0.0080 cm/cm @Thickness 3.17 mm |
0.0080 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PA12 E HS Availability: North AmericaForms: PelletsAdditive: Heat StabilizerFeatures: Heat StabilizedProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.011 cm/cm | 0.0080 - 0.011 in/in | on tensile bar; SABIC Method |
SABIC Innovative Plastics Xenoy® XL1562 PBT+PC (Europe-Africa-Middle East) XENOY XL1562 is an impact modified PBT+PC blend with outstanding chemical resistance, good UV stability and flow properties.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | ISO DIS 294-4 |
Wellman Wellamid® FRGF1827-BK1 10% Glass Fiber Reinforced Flame Retardant Nylon 66 Description: Glass Fiber Reinforced Flame Retardant Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.0080 cm/cm @Thickness 3.20 mm |
0.0080 in/in @Thickness 0.126 in |
|
Unitika M1030DH PA6, Conditioned Nano composite nylonInformation provided by Unitika Ltd. |
|||
Linear Mold Shrinkage, Flow | 0.0080 cm/cm | 0.0080 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® BS 23 PA6 Information provided by EMS Grivory |
|||
Linear Mold Shrinkage, Flow | 0.0080 cm/cm | 0.0080 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® BZ 1/2 PA6 Product description: Grilon BZ 1/2 is an unreinforced, impact modified PA6 injection molding grade with normal melt viscosity. Grilon BZ 1/2 has the following important properties: Good flow behavio.. |
|||
Linear Mold Shrinkage, Flow | 0.0080 cm/cm | 0.0080 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® L 20 HL black 9563 PA12 Product Description: Grilamid L 20 HL black 9563 is a, medium viscosity extrusion grade, based on Polyamide 12 (PA12). Grilamid L20 HL black 9563 has been especially developed for external cable she.. |
|||
Linear Mold Shrinkage, Flow | 0.0080 cm/cm | 0.0080 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® L 25 Z PA12-I Product Description: Grilamid L 25 Z is a UV- and heat stabilized high viscosity polyamide 12 grade with improved toughness. A special feature of Grilamid L25 Z is its high energy absorption capacit.. |
|||
Linear Mold Shrinkage, Flow | 0.0080 cm/cm | 0.0080 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Hytrel® RS 40F3 NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Renewably Sourced High Flow Polyester Elastomer Developed for Injection Molding Hytrel RS 40F3 NC010 is a high flow low modulus grade containing at least 50% renewably sourced ingredients.. |