Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lucent Polymers GPP-110 Polypropylene Homopolymer, 10% Glass Fiber Reinforced, Chemically Coupled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 10% Glass Fiber Filler
Manufacturer Lucent Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucent Polymers GPP-110 Polypropylene Homopolymer, 10% Glass Fiber Reinforced, Chemically Coupled.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 0.980 g/cc
0.980 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0080 cm/cm

@Thickness 3.17 mm
0.0080 in/in

@Thickness 0.125 in
1/8" Section
Mechanical Properties Metric English Comments
Tensile Strength, Yield 46.21 MPa
6702 psi
ASTM D638
Elongation at Break 7.0 %
7.0 %
ASTM D638
Flexural Strength 64.14 MPa
9303 psi
ASTM D790
Flexural Modulus 2.241 GPa
325.1 ksi
ASTM D790
Izod Impact, Notched 0.427 J/cm

@Thickness 3.17 mm
0.800 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 112.78 °C
235.00 °F
ASTM D648