| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D792 |
| Linear Mold Shrinkage, Flow | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 48 | 48 | 15 sec; ASTM D2240 |
| 50 | 50 | ASTM D2240 | |
| Tensile Strength at Break | 17.2 MPa | 2490 psi | 510 mm/min; ASTM D638 |
| Tensile Strength | 11.7 MPa @Strain 100 % |
1700 psi @Strain 100 % |
510 mm/min; ASTM D638 |
| Elongation at Break | 300 % | 300 % | 510 mm/min; ASTM D638 |
| Tear Strength | 84.1 kN/m | 480 pli | Die C, 510 mm/min; ASTM D624 |
| Compression Set | 45 % @Temperature 23.0 °C, Time 79200 sec |
45 % @Temperature 73.4 °F, Time 22.0 hour |
ASTM D395 |
| Clash Berg Modulus | 0.634 GPa | 92.0 ksi | ASTM D1043 |
| 0.310 GPa @Temperature -20.0 °C |
45.0 ksi @Temperature -4.00 °F |
ASTM D1043 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 179 - 185 °C | 354 - 365 °F | |
| 196 - 207 °C | 385 - 405 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Additive | UV Stabilizer | |
| Appearance | Opaque | |
| Features | UV Absorbing | |
| Forms | Pellets | |
| Generic Material | PVC, Flexible | |
| Generic Name | Polyvinyl Chloride, Flexible (PVC, Flexible) | |
| Processing Method | Extrusion | |
| Injection Molding | ||
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America |