Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0070 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0070 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® 4504 PPC (Asia Pacific) High heat resistant polycarbonate copolymer, provides DTUL of 290F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported wit.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm @Thickness 3.17 mm |
0.0070 in/in @Thickness 0.125 in |
1/8" Section |
Lucent Polymers PC/PBT-1231 Polycarbonate+PBT, General Purpose, Injection Grade Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.010 cm/cm | 0.0070 - 0.010 in/in | |
LATI Latilub 73/13-15T G/15 POM, 15% Glass Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyoxymethylene (POM). PTFE. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indus.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.0090 cm/cm @Time 86400 sec |
0.0070 - 0.0090 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP UX06425 PPA LNP* LUBRICOMP* UX06425 is a compound based on Polyphthalamide (PPA) containing 10% Glass Fiber, 10% PTFE. Added features of this material include: Wear Resistant, Hot Water Moldable and Heat Stab.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.0090 cm/cm @Thickness 3.18 mm |
0.0070 - 0.0090 in/in @Thickness 0.125 in |
|
Solvay Specialty Polymers AvaSpire® AV-651 Polyaryletherketone (PAEK) AvaSpire® AV-651 is an unreinforced polyaryletherketone (PAEK) that offers more ductility and impact strength than PEEK, with higher chemical and environmental stress cracking resistance than Ava.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm | 0.0070 in/in | |
Solvay Specialty Polymers Udel® P-1750 MR Polysulfone (PSU) Udel® P-1750 MR is a lower color grade of polysulfone that contains a mold release which aids part ejection when parts with low draft are injection molded.Polysulfones have long been known for tr.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm @Thickness 3.17 mm |
0.0070 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® HDPE E GF15 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm @Thickness 3.17 mm |
0.0070 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PA6 GF40 L 40% Milled Glass Availability: North AmericaForms: PelletsFiller/Reinforcement: Milled Glass Fiber, 30% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: Natural ColorInformation provided by TP Comp.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm @Thickness 3.17 mm |
0.0070 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Luriblend® PA6/6 GF10 TL10 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 10% Filler by WeightAdditive: Heat Stabilizer and PTFE Lubricant(5%)Features: Lubricated, Good Wear Resistance, Low Fricti.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm @Time 86400 sec |
0.0070 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Thermocomp DX99721 PC LNP* Thermocomp* DX99721 is a compound based on Polycarbonate resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm | 0.0070 in/in | SABIC Method |
SABIC Innovative Plastics LNP Thermocomp FF001 PE (Europe-Africa-Middle East) LNP* THERMOCOMP* FF001 is a compound based on Polyethylene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm @Thickness 3.17 mm |
0.0070 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Plastiblend® PC/PBT IM 5727 BK Availability: North AmericaForms: PelletsAdditive: Impact Modifier and UV StabilizerFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.0090 cm/cm @Time 86400 sec |
0.0070 - 0.0090 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP MX06402H PP LNP* THERMOCOMP* MX06402H is a compound based on Polypropylene resin containing 20% Glass Fiber. Added features of this material include: Heat Stabilized, Low Extractable. |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm @Time 86400 sec |
0.0070 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP WH0450E PBT LNP* Thermocomp* WH0450E is a compound based on Polybutylene Terephalate resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm @Thickness 3.17 mm |
0.0070 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Elastoblend® PA6/6 GF33 IM HS L BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0070 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics XYLEX X7519HP PC+POLYESTER Good Chemical Resistance, XYLEX grade with good dishwasher performance, USA/Europe Food Contact Comment: While molding of thicker parts, cooling speed has an influence of transparency. Thicker parts.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm @Time 86400 sec |
0.0070 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP MF742XXH PP LNP* THERMOCOMP* MF742XXH is a compound based on Polypropylene resin containing Glass Fiber and proprietary antimicrobial additives. This product is best suited for touch surfaces in healthcare app.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm @Time 86400 sec |
0.0070 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP MFB71L PP LNP* THERMOCOMP* MFB71L is a compound based on Polypropylene resin containing 35% Glass Bead, 5% Glass Fiber. Added features of this material include: Low Extractible. |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm @Thickness 3.17 mm |
0.0070 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Luriblend® PSU TL20 Availability: North AmericaForms: PelletsAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm @Thickness 3.20 mm |
0.0070 in/in @Thickness 0.126 in |
|
Unitika CX-2500 PA6, Conditioned Transparent nylonInformation provided by Unitika Ltd. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.0090 cm/cm | 0.0070 - 0.0090 in/in | ISO DIS 294-4 |
Wellman Wellamid® MRGF3820-N 38% Mineral/Glass Reinforced Developmental Grade Nylon 66 Description: Mineral/Glass Reinforced Developmental Grade Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm | 0.0070 in/in | ISO 294-4 |
DSM Akulon® S223-G4U (Dry) 23% Glass Reinforced Nylon 66 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm | 0.0070 in/in | ISO 294-4,2577 |
Covestro Makrolon® 3103 MAS157 Polycarbonate ISO 7391-PC,EL,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minExtrusionHigh viscosityUV stabilizedAvailable in color code 550115 onlySolid sheetCorrugated sheetPreprocessingMax. Water conte.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm | 0.0070 in/in | ISO 294-4,2577 |
Covestro Makrolon® AL2447 Polycarbonate ISO 7391-PC,MLR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 19 cm3/10 minAutomotive lightingLow viscosityUV stabilizedEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in transpa.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm @Thickness 2.00 mm |
0.0070 in/in @Thickness 0.0787 in |
60x60x2 mm; 500 bar; ISO 294-4 |
Covestro Makrolon® FU4007 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Furniture applications.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm | 0.0070 in/in | ISO 294-4,2577 |
Covestro Makrolon® SF805 Polycarbonate, 5% Glass Filled MVR (300 °C/1.2 kg) 7.0 cm3/10 minStructural foam5 % Glass fiber reinforcedNormal fiberChlorine- and bromine-free flame retardantHigh viscosityEasy releaseInjection moldingAvailable in natural (opa.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm | 0.0070 in/in | DAM; ISO 294-4 2577 |
DuPont Performance Polymers Minlon® 22C NC010 Nylon 66
(Unverified Data**) 38% Mineral/Glass Reinforced Polyamide 66 Minlon 22C NC010 is a 38% mineral/glass reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polym.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm | 0.0070 in/in | DAM; ISO 294-4 2577 |
DuPont Performance Polymers Zytel® FG133F1 NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66 with Developed for Food Contact Applications Zytel FG133F1 NC010 is a nucleated PA 66. It has been developed for consideration into applications such as parts for the food .. |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm | 0.0070 in/in | ISO 294-4,2577 |
Covestro Makrolon® SF800Z Polycarbonate, 5% Glass Filled MVR (300 °C/1.2 kg) 8.0 cm3/10 minStructural foam5 % Glass fiber reinforcedMilled fiberChlorine- and bromine-free flame retardantMedium viscosityEasy releaseInjection moldingAvailable in natural (o.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 cm/cm | 0.0070 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® TS V0 PA666 Product description: Grilon TS V0 is an unreinforced, normal viscosity, self-extinguishing Polyamid 66 + Polyamide 6 injection molding grade. Grilon TS V0 is halogen free and free of red phosphorous.. |