Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.00050 - 0.0020 cm/cm | 0.00050 - 0.0020 in/in | ASTM D955 |
PolyOne Stat-Tech™ X ST6600-0041 ES NHFR Black Polyamide 66 (Nylon 66) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0020 cm/cm | 0.00050 - 0.0020 in/in | ASTM D955 |
PolyOne Trilliant™ HC HC7300-0013 ESD Black Acrylonitrile Butadiene Styrene (ABS) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.00070 cm/cm | 0.00050 - 0.00070 in/in | ASTM D955 |
LG Chemical Lupoy 1200-10 Polycarbonate Resin Description: LUPOY PC 1200-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.00070 cm/cm | 0.00050 - 0.00070 in/in | ASTM D955 |
LG Chemical Lupoy 1200-22 Polycarbonate Resin Description: LUPOY PC 1200-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.00070 cm/cm | 0.00050 - 0.00070 in/in | ASTM D955 |
LG Chemical Lupoy 1201-05 Polycarbonate Resin Description: LUPOY PC 1201-05 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.00070 cm/cm | 0.00050 - 0.00070 in/in | ASTM D955 |
LG Chemical Lupoy 1300-22 Polycarbonate Resin Description: LUPOY PC 1300-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.00070 cm/cm | 0.00050 - 0.00070 in/in | ASTM D955 |
LG Chemical Lupoy 1301V-10 Polycarbonate Resin Description: LUPOY PC 1301V-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.00070 cm/cm | 0.00050 - 0.00070 in/in | ASTM D955 |
LG Chemical Lupoy 1600-03 Polycarbonate Resin Description: LUPOY PC 1600-03 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Characteristics: .. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0020 cm/cm | 0.00050 - 0.0020 in/in | |
LATI Larpeek 10 K/40 PEEK, 40% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.00070 cm/cm | 0.00050 - 0.00070 in/in | ASTM D955 |
LG Chemical Lupoy 1200HP-15 Polycarbonate Resin Description: LUPOY PC 1200HP-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.00070 cm/cm | 0.00050 - 0.00070 in/in | ASTM D955 |
LG Chemical Lupoy 1300-03 Polycarbonate Resin Description: LUPOY PC 1300-03 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.00070 cm/cm | 0.00050 - 0.00070 in/in | ASTM D955 |
LG Chemical Lupoy 1302-10 Polycarbonate Resin Description: LUPOY PC 1302-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Linear Mold Shrinkage, Flow | 0.00050 cm/cm | 0.00050 in/in | Post-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4 |
Lanxess Durethan® BKV 35 H3.0 000000 Nylon 6, Glass Fiber Reinforced PA 6, 35% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0020 cm/cm | 0.00050 - 0.0020 in/in | |
LATI Laramid K/40 HM PPA, 40% Carbon Fiber Reinforced Semi-aromatic polyamide (PPA) based compound. Carbon fiber. High tensile modulus. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; .. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0020 cm/cm | 0.00050 - 0.0020 in/in | |
LATI Larpeek 10 K/40 HM PEEK, 40% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. High tensile modulus. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Af.. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0025 cm/cm | 0.00050 - 0.0025 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP OCL13XXP PPS - LINEAR (Europe-Africa-Middle East) LNP* Stat-kon* OCL13XXP is a compound based on PPS - LINEAR resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Linear Mold Shrinkage, Flow | 0.00050 cm/cm @Thickness 3.17 mm |
0.00050 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® ASA GF20 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: UV StabilizerFeatures: Good UV ResistanceInformation provided by TP Composites.. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0015 cm/cm @Time 86400 sec |
0.00050 - 0.0015 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON EX03319C PEI (Asia Pacific) LNP* Stat-Kon* EX03319C is a polyetherimide compound reinforced with carbon fiber for good stiffness, dimension stability and has extremely high level of cleanliness for the most demanding applicati.. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0015 cm/cm @Thickness 3.20 mm |
0.00050 - 0.0015 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP STAT-KON Lexan_LCF1506 PC LNP* Stat-kon* Lexan_LC1500N compound is a 15% carbon fiber, 6% PTFE reinforced polycarbonate. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.00070 cm/cm @Time 86400 sec |
0.00050 - 0.00070 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON OEL36A PPS - BRANCHED LNP* STAT-KON* OEL36A is a compound based on PPS - Branched resin containing 15% PTFE, 30% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive. |
|||
Linear Mold Shrinkage, Flow | 0.00050 cm/cm @Thickness 3.17 mm |
0.00050 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Luriblend® PA6/6 CF30 TL12 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE + Silicone Lubricant(15%)Features: Lubricated and Good Wear ResistanceTPCI# 6466101Inf.. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0015 cm/cm @Thickness 3.20 mm |
0.00050 - 0.0015 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP DX10313 PC (Asia Pacific) DX10313 is high modulus polycarbonate, 50% glass filled, with balanced flow and impact strength |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0015 cm/cm @Thickness 3.20 mm |
0.00050 - 0.0015 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_JK2000 PC+ABS LNP* Thermocomp* Lexan_JK2000 compound is a 22% GR, ECO-compliant FR, PC+ABS for thinwall molding applications. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0025 cm/cm @Thickness 3.20 mm |
0.00050 - 0.0025 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGK5030 PC LNP* Thermocomp* Lexan_LGN5030 compound is a glass reinforced. Flame retardant. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0015 cm/cm @Thickness 3.20 mm |
0.00050 - 0.0015 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP STAT-KON DX09303C PC (Asia Pacific) LNP* Stat-Kon* DX09303C is carbon fiber filled polycarbonate composite with high modulus, good flow ability, and high level of cleanliness for the most demanding application. A unique feature of thi.. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0020 cm/cm | 0.00050 - 0.0020 in/in | ASTM D955 |
PolyOne Stat-Tech™ NJ-20CF/000 Black Polyamide 12 (Nylon 12) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.00070 cm/cm | 0.00050 - 0.00070 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Cycoloy® CH6410 PC+ABS CH6410 is a high heat, impact modified PC resin, with nonbrominated, nonchlorinated flame retardant system. Limited colors only. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0025 cm/cm @Thickness 3.20 mm |
0.00050 - 0.0025 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGK3020 PC (Asia Pacific) Glass reinforced. Flame retardant. |
|||
Linear Mold Shrinkage, Flow | 0.00050 cm/cm @Time 86400 sec |
0.00050 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP VERTON NV008E PC/ABS (Asia Pacific) LNP* Verton* NV008E is a compound based on PC/ABS resin containing Long Glass Fiber. Added features of this material include: Easy Molding. |