Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polykemi AB POLYelast TPE ZS706 Thermoplastic Elastomer, SEBS/SBS-based

Category Polymer , Thermoplastic , Elastomer, TPE , Styrene-Butadiene , Styrene/Butadiene/Styrene (SBS)
Manufacturer Polykemi AB
Trade Name POLYelast
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polykemi AB POLYelast TPE ZS706 Thermoplastic Elastomer, SEBS/SBS-based.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Polykemi AB
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183
Linear Mold Shrinkage 0.014 - 0.020 cm/cm
0.014 - 0.020 in/in
With Flow; ISO 2577
0.014 - 0.020 cm/cm
0.014 - 0.020 in/in
Across Flow; ISO 2577
Mechanical Properties Metric English Comments
Hardness, Shore A 70

@Time 15.0 sec
70

@Time 0.00417 hour
Polykemi
Tensile Strength at Break <= 7.00 MPa
<= 1020 psi
ISO/R527
Elongation at Break 600 %
600 %
ISO/R527
100% Modulus 0.00200 GPa
0.290 ksi
ISO/R527
300% Modulus 0.00280 GPa
0.406 ksi
ISO/R527
Processing Properties Metric English Comments
Melt Temperature 180 - 220 °C
356 - 428 °F
Mold Temperature 20.0 - 40.0 °C
68.0 - 104 °F
Back Pressure 0.500 - 1.50 MPa
72.5 - 218 psi
Descriptive Properties Value Comments
Holding Pressure () Low
% of injection pressure
Injection Pressure Low
Injection Speed () High
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved