Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0070 - 0.010 cm/cm | 0.0070 - 0.010 in/in | Compression; ISO 2577 |
Raschig Group AMPLA® 7500 melamine-modified polyester Organically and inorganically filled melamine modified Polyester molding compound. Low post-shrinkage, very good electrical values, excellent heat resistance, very good sliding behavior and wear sta.. |
|||
Linear Mold Shrinkage | 0.0050 - 0.010 cm/cm | 0.0050 - 0.010 in/in | (longitudinal) Compression; ISO 2577 |
Raschig Group MELOPLAS® 3025 MF Cellulose-reinforced and inorganically filled MF molding compound in white and colored shades. High surface hardness, good UV and heat stability, very good resistance to chemicals - also to foodstu.. |
|||
Linear Mold Shrinkage | 0.0080 - 0.010 cm/cm | 0.0080 - 0.010 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYfill PP EIP12030RF Polypropylene/EPDM, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0080 - 0.010 cm/cm | 0.0080 - 0.010 in/in | With Flow; ISO 2577 |
Polykemi AB POLYfill PPH K20040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0080 - 0.010 cm/cm | 0.0080 - 0.010 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYfill PPH K20040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0050 - 0.010 cm/cm | 0.0050 - 0.010 in/in | |
Lehmann & Voss LUVOCOM® 1500-0871 Polysulfone, with glass spheres Applications: Isotropic shrinkage characteristics.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precision parts, high continuous use temperature.Control disks, ca.. |
|||
Linear Mold Shrinkage | 0.0060 - 0.010 cm/cm | 0.0060 - 0.010 in/in | |
Lehmann & Voss LUVOCOM® 1700-8541 PPO, unreinforced Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Dynamic stressed parts.Isotropic shrinkage characteristics.Superheated steam sterilizable.Infor.. |
|||
Linear Mold Shrinkage | 0.0080 - 0.010 cm/cm | 0.0080 - 0.010 in/in | 3.2 mm; ASTM D955 |
Lavergne VYPET VNT 1021 Polyester-PC Alloy The Vypet 1021 Black is a medium viscosity Polyester and PC alloy, has an excellent balance of stiffness and impact resistance.Features: Excellent Processability; Good Impact Resistance; Good Chemic.. |
|||
Linear Mold Shrinkage | 0.0050 - 0.010 cm/cm | 0.0050 - 0.010 in/in | |
Lehmann & Voss LUVOCOM® 1105-7023/GY PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Linear Mold Shrinkage | 0.0060 - 0.010 cm/cm @Thickness 3.20 mm |
0.0060 - 0.010 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 342 Ionomer Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0060 - 0.010 cm/cm @Thickness 3.20 mm |
0.0060 - 0.010 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 396 Ionomer DescriptionFormion® FI 3936is a 3% glass fiber reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, and impact. Formion F1 396U is UV stabilized to exceed .. |
|||
Linear Mold Shrinkage | 0.0060 - 0.010 cm/cm @Thickness 3.20 mm |
0.0060 - 0.010 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 396 Ionomer DescriptionFormion® FI 3936is a 3% glass fiber reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, and impact. Formion F1 396U is UV stabilized to exceed .. |
|||
Linear Mold Shrinkage | 0.0080 - 0.010 cm/cm | 0.0080 - 0.010 in/in | |
Polyram RamLloy PVB101 ABS/NYLON alloy, Impact Modified Impact modified ABS/NYLON alloy for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.0080 - 0.010 cm/cm @Thickness 3.20 mm |
0.0080 - 0.010 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 200 Non-Reinforced, Injection Molding Grade Ionomer / Nylon Alloy DescriptionFormion® FI 200 is an injection molding grade, non-reinforce Ionomer / Nylon Alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. Applicatio.. |
|||
Linear Mold Shrinkage | 0.0060 - 0.010 cm/cm @Thickness 3.20 mm |
0.0060 - 0.010 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 342 Ionomer Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0060 - 0.010 cm/cm @Thickness 3.20 mm, Time 259000 sec |
0.0060 - 0.010 in/in @Thickness 0.126 in, Time 72.0 hour |
ISO 294 |
A. Schulman FORMION™ FI 372 Ionomer Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0060 - 0.010 cm/cm @Thickness 3.20 mm |
0.0060 - 0.010 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 396 Ionomer DescriptionFormion® FI 3936is a 3% glass fiber reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, and impact. Formion F1 396U is UV stabilized to exceed .. |
|||
Linear Mold Shrinkage | 0.0060 - 0.010 cm/cm | 0.0060 - 0.010 in/in | ASTM D955 |
Lubrizol Estane® ALR PC60D Thermoplastic Polyurethane Type: Estane® ALR PC60D is a polycarbonate diol based thermoplastic polyurethane (TPU).Features: Hydrolytically stable, very durableInformation Provided by The Lubrizol Corporation |
|||
Linear Mold Shrinkage | 0.0080 - 0.010 cm/cm @Thickness 4.00 mm |
0.0080 - 0.010 in/in @Thickness 0.157 in |
|
CP-Polymer-Technik Wellamid® 6000 GS 20 HWCP 20% Glass Sphere Filled Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Linear Mold Shrinkage | 0.0080 - 0.010 cm/cm @Thickness 4.00 mm |
0.0080 - 0.010 in/in @Thickness 0.157 in |
|
CP-Polymer-Technik Wellamid® 6000 GS 30 HWCP 30% Glass Sphere Filled Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Linear Mold Shrinkage | 0.0080 - 0.010 cm/cm | 0.0080 - 0.010 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYfill PP HJ752 UV2 Polypropylene/Elastomer, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0060 - 0.010 cm/cm @Thickness 3.20 mm |
0.0060 - 0.010 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 392 Ionomer Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0080 - 0.010 cm/cm | 0.0080 - 0.010 in/in | as molded |
A. Schulman POLYTROPE™ TPP 518 Injection Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 518 is an injection grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal expansion i.. |
|||
Linear Mold Shrinkage | 0.0060 - 0.010 cm/cm | 0.0060 - 0.010 in/in | ASTM D955 |
Beijing Chemical Industry KAIFA® MN201-G25 Nylon 66 Resin 25% glass fiber reinforced, thermal resistantInformation provided by Beijing Chemical Industry Research Institute (Group) |