Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polyram RamLloy PVB101 ABS/NYLON alloy, Impact Modified

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend , Nylon
Manufacturer Polyram
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram RamLloy PVB101 ABS/NYLON alloy, Impact Modified.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Impact modified ABS/NYLON alloy for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
DIN 53479
Linear Mold Shrinkage 0.0080 - 0.010 cm/cm
0.0080 - 0.010 in/in
Melt Flow 5.0 g/10 min

@Load 5.00 kg,
Temperature 240 °C
5.0 g/10 min

@Load 11.0 lb,
Temperature 464 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 40.0 MPa
5800 psi
ASTM-D638
Elongation at Break 200 %
200 %
ASTM-D638
Tensile Modulus 1.25 GPa
181 ksi
ASTM-D790
Flexural Strength 60.0 MPa
8700 psi
ASTM-D790
Flexural Modulus 1.40 GPa
203 ksi
ASTM-D790
Izod Impact, Notched 6.00 J/cm

@Temperature 23.0 °C
11.2 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C
203 °F
DIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
158 °F
DIN 53461