Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00200 - 0.00700 cm/cm | 0.00200 - 0.00700 in/in | Average value: 0.00500 cm/cm Grade Count:3 |
Overview of materials for Polyarylsulfone (PAS), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyarylsulfone; Molded/Extruded". Each property range of values reported is minimum and maximum values .. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00700 cm/cm | 0.00100 - 0.00700 in/in | Average value: 0.00429 cm/cm Grade Count:38 |
Overview of materials for Polystyrene + Polyphenylene Ether, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Unreinforced". Each property range of values reported is minimum and .. |
|||
Linear Mold Shrinkage | 0.00500 - 0.00700 cm/cm | 0.00500 - 0.00700 in/in | Average value: 0.00600 cm/cm Grade Count:8 |
Overview of materials for Polyphenylene Ether, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Impact Grade". Each property range of values reported is minimum and maximum values.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00700 cm/cm | 0.00100 - 0.00700 in/in | Average value: 0.00505 cm/cm Grade Count:5 |
Overview of materials for Polyphenylene Ether, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Mineral Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Linear Mold Shrinkage | 0.00400 - 0.00700 cm/cm | 0.00400 - 0.00700 in/in | Average value: 0.00577 cm/cm Grade Count:11 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), PTFE Filled". Each property range of values reported is minimum a.. |
|||
Linear Mold Shrinkage | 0.000500 - 0.00700 cm/cm | 0.000500 - 0.00700 in/in | Average value: 0.00298 cm/cm Grade Count:87 |
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Glass Fiber Filled". Each property range of values reported is minimum and maxi.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00700 cm/cm | 0.00100 - 0.00700 in/in | Average value: 0.00443 cm/cm Grade Count:7 |
Overview of materials for Polycarbonate, Foam Grade, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Foam Grade, Glass Filled". Each property range of values reported is minimum and maximum .. |
|||
Linear Mold Shrinkage | 0.00300 - 0.00700 cm/cm | 0.00300 - 0.00700 in/in | Average value: 0.00490 cm/cm Grade Count:8 |
Overview of materials for Polycarbonate, Aramid Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Aramid Fiber Reinforced". Each property range of values reported is minimum and maximum v.. |
|||
Linear Mold Shrinkage | 0.000500 - 0.00700 cm/cm | 0.000500 - 0.00700 in/in | Average value: 0.00476 cm/cm Grade Count:16 |
Overview of materials for Polyetherimide (PEI), 10% Glass Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 10% Glass Fiber". Specific grades with glass content between 5% and 14% are included. Ea.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00700 cm/cm | 0.00200 - 0.00700 in/in | Average value: 0.00429 cm/cm Grade Count:14 |
Overview of materials for Polysulfone, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are incl.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00700 cm/cm | 0.00100 - 0.00700 in/in | Average value: 0.00540 cm/cm Grade Count:10 |
Overview of materials for Cyclo Olefin Polymer This property data is a summary of similar materials in the MatWeb database for the category "Cyclo Olefin Polymer". Each property range of values reported is minimum and maximum values of appropria.. |
|||
Linear Mold Shrinkage | 0.00250 - 0.00700 cm/cm | 0.00250 - 0.00700 in/in | Average value: 0.00363 cm/cm Grade Count:7 |
Overview of materials for Epoxy Encapsulant, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Encapsulant, Unreinforced". Each property range of values reported is minimum and maximum values o.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00700 cm/cm | 0.00100 - 0.00700 in/in | Average value: 0.00367 cm/cm Grade Count:12 |
Overview of materials for Epoxy, Encapsulating, Glass or Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Glass or Mineral Filled". Each property range of values reported is minimum and ma.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00700 cm/cm | 0.00100 - 0.00700 in/in | Average value: 0.00342 cm/cm Grade Count:11 |
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler". Specific grades with glass content between 15%.. |
|||
Linear Mold Shrinkage | 0.000500 - 0.00700 cm/cm | 0.000500 - 0.00700 in/in | Average value: 0.00256 cm/cm Grade Count:44 |
Overview of materials for Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled". Each property range of values reported is minimum.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00700 cm/cm | 0.00100 - 0.00700 in/in | Average value: 0.00290 cm/cm Grade Count:26 |
Overview of materials for Nylon 12, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |
|||
Linear Mold Shrinkage | 0.00300 - 0.00700 cm/cm | 0.00300 - 0.00700 in/in | Internal Method |
Topas Advanced Polymers TOPAS® IT X1 Cyclic Olefin Copolymer (COC) TOPAS® IT X1 is an injection molding grade with heat and impact resistance. It is a moderately clear resin with high moisture barrier, chemical and heat resistance, making it suitable for products .. |
|||
Linear Mold Shrinkage | 0.00300 - 0.00700 cm/cm | 0.00300 - 0.00700 in/in | Average value: 0.00518 cm/cm Grade Count:20 |
Overview of materials for Polystyrene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Extrusion Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
Linear Mold Shrinkage | 0.00300 - 0.00700 cm/cm | 0.00300 - 0.00700 in/in | Average value: 0.00479 cm/cm Grade Count:7 |
Overview of materials for Polyetherimide (PEI), Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, Aramid Fiber Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00700 cm/cm | 0.00200 - 0.00700 in/in | Average value: 0.00369 cm/cm Grade Count:24 |
Overview of materials for Polyphenylene Ether, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 20% Glass Filled". Specific grades with glass content between 15% and 24% are inclu.. |
|||
Linear Mold Shrinkage | 0.000200 - 0.00700 cm/cm | 0.000200 - 0.00700 in/in | Average value: 0.00211 cm/cm Grade Count:34 |
Overview of materials for Epoxy Molding Compound This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Molding Compound". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Linear Mold Shrinkage | 0.00400 - 0.00700 cm/cm @Temperature 80.0 - 80.0 °C |
0.00400 - 0.00700 in/in @Temperature 176 - 176 °F |
Average value: 0.00567 cm/cm Grade Count:3 |
Overview of materials for Nylon 6, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Glass Fiber Filled".Specific grades with glass content between 15% and 24% are included. Ea.. |
|||
Linear Mold Shrinkage | 0.00400 - 0.00700 cm/cm | 0.00400 - 0.00700 in/in | Average value: 0.00450 cm/cm Grade Count:4 |
Overview of materials for ABS/PVC Alloy This property data is a summary of similar materials in the MatWeb database for the category "ABS/PVC Alloy". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Linear Mold Shrinkage | 0.000300 - 0.00700 cm/cm | 0.000300 - 0.00700 in/in | Average value: 0.00163 cm/cm Grade Count:32 |
Overview of materials for Polyphthalamide (PPA), Carbon Fiber + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber + PTFE Filled". Each property range of values reported is minimum and maxi.. |